Skip Nav Destination
Close Modal
Search Results for
surface-preparation
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Book Series
Date
Availability
1-20 of 450 Search Results for
surface-preparation
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
1
Sort by
Book Chapter
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.usage.c9001415
EISBN: 978-1-62708-236-5
... not been grooved but appeared to have been roughened by shot or grit-blasting prior to spraying and the deposit was more firmly adherent to these surfaces than in the case of the pins. It is doubtful, however, whether the adhesion of sprayed metal to a surface prepared even in this manner would always...
Abstract
In the course of a general overhaul, the crankpins and main journals (3 in. diam) of the crankshaft of a four-cylinder oil engine were built up by metal spraying. Four weeks later, the shaft broke through the pin remote from the flywheel (driving) end. The fracture was of the fatigue type. A creeping crack originated in the fillet at the inside surface of the pin and extended parallel to the plane of the web across practically the entire section before complete rupture occurred. The sprayed metal on the fractured pin had very poor adhesion. The surfaces of the main journals had not been grooved but appeared to have been roughened by shot or grit-blasting prior to spraying and the deposit was more firmly adherent to these surfaces than in the case of the pins. It is doubtful, however, whether the adhesion of sprayed metal to a surface prepared even in this manner would always be satisfactory under severe loading conditions, such as those to which a crankpin is subjected in service.
Image
in Effect of Strain Rate on the Failure Mode of a Rear Axle
> Handbook of Case Histories in Failure Analysis
Published: 01 December 1992
Fig. 11 Overall appearance of fracture surface of exemplar impact coupon prepared from the hardened outer perimeter of the axle. Note lack of deformation.
More
Image
in Effect of Strain Rate on the Failure Mode of a Rear Axle
> Handbook of Case Histories in Failure Analysis
Published: 01 December 1992
Fig. 12 Fracture surface of subsized impact coupon prepared from the hardened perimeter of the axle, showing cleavage rupture with river patterns. 3400×.
More
Image
in Effect of Strain Rate on the Failure Mode of a Rear Axle
> Handbook of Case Histories in Failure Analysis
Published: 01 December 1992
Fig. 13 Overall appearance of fracture surface of exemplar impact coupon prepared from the axle core. Note deformation of sides of tested coupon.
More
Image
in Effect of Strain Rate on the Failure Mode of a Rear Axle
> Handbook of Case Histories in Failure Analysis
Published: 01 December 1992
Fig. 14 Fractured surface of subsized impact coupon prepared from the axle core, exhibiting a mixed mode (brittle cleavage and ductile dimples) of rupture. 136×.
More
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.process.c9001667
EISBN: 978-1-62708-235-8
..., a procedure common to the surface preparation and machining of titanium alloys, which produced a superior surface finish. All of the grinding and polishing performed on the weldment was done with the Di-Profiler using various PSA-backed grinding papers and polishing cloths. The procedures followed...
Abstract
Nondestructive metallographic examination of materials frequently must be performed on-site when the component in question cannot be moved or destructively examined. Often, it is imperative that specific microstructural information (i.e., material type, heat treatment condition, homogeneity, etc.) be obtained either before initial use of a component, or before the use of a component can be safely resumed. In this paper, the use of standard metallurgical laboratory equipment, and the procedures required to conduct nondestructive on-site metallographic analyses of engineering materials, is presented. As an example, the materials and metallographic techniques employed in an actual on-site investigation of a gas tungsten-arc weldment joining two large diameter Ti-6Al-4V alloy cylinders are discussed in depth to illustrate what can be accomplished.
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.process.c9001641
EISBN: 978-1-62708-235-8
... for cleaning and surface preparation, as well as for the actual plating deposition. Porosity that is linked to the surface can trap liquids from the cleaning and surface preparation baths, and these liquids are usually quite acidic. The trapped acid may initiate corrosion and generate hydrogen gas as a result...
Abstract
Near-surface porosity in zinc die castings that were subsequently plated with copper, nickel, and bright chromium was causing blemishes in the plating. Identifying die casting turbulence and hot spots were keys to process modifications that subsequently allowed porosity to be greatly minimized.
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.process.c9001520
EISBN: 978-1-62708-235-8
... with the quality of surface preparation. Cracks were prevalent in areas where the surface was smeared rather than properly machined. The area of cracking (for the cylinder that failed during pressure testing) was found by metallography to contain a distinct cold-worked layer with several shallow surface laps...
Abstract
Two types of chromium-plated hydraulic cylinders failed by cracking on their outer surfaces. In one case, the parts had a history of cracking in the nominally unstressed, as-fabricated condition. In another, cracks were detected after the cylinders were subjected to a pressure impulse test. Both part types were made of 15-5 PH (UNS S15500) precipitation hardening stainless steel. Hydrogen embrittlement cracking was the likely cause of failure for both part types. Cracking of the as-fabricated parts was ultimately prevented by changing the manufacturing procedure to allow for a reheat treatment. For parts that cracked after pressure testing, excessive dimensional changes precluded the inclusion of a reheat treatment as a manufacturing step, and further failure was averted by carefully employing proper machining practices, avoiding abusive machining.
Book Chapter
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.aero.c0006402
EISBN: 978-1-62708-217-4
... of the panels was endorsed. Most importantly, surveillance of the anodizing process itself was emphasized. Alkaline cleaning Anodizing Auger electron spectroscopy Energy dispersive x ray analysis Fuel tanks Panels Scanning electron microscopy Sealing Surface preparation Vapor degreasing Wings...
Abstract
New aircraft wing panels extruded from 7075-T6 aluminum exhibited an unusual pattern of circular black interrupted lines, which could not be removed by scouring or light sanding. The panels, subsequent to profiling and machining, were required to be penetrated inspected, shot peened, H2SO4 anodized, and coated with MIL-C-27725 integral fuel tank coating on the rib side. Scanning electron microscopy and microprobe analysis (both conventional energy-dispersive and Auger analyzers) showed that the anodic coating was applied over an improperly cleaned and contaminated surface. The expanding corrosion product had cracked and, in some places, had flaked away the anodized coating. The corrodent had penetrated the base aluminum in the form of subsurface intergranular attack to a depth of 0.035 mm (0.0014 in.). It was recommended that a vapor degreaser be used during cleaning prior to anodizing. A hot inhibited alkaline cleaner was also recommended during cleaning prior to anodizing. The panels should be dichromate sealed after anodizing. The use of deionized water was also recommended during the dichromate sealing operation. In addition, the use of an epoxy primer prior to shipment of the panels was endorsed. Most importantly, surveillance of the anodizing process itself was emphasized.
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.modes.c9001628
EISBN: 978-1-62708-234-1
... or energy levels characteristic of that element, identifying the approximate concentration of each major element in the sample. The portable instrumentation is designed for rapid direct analysis without extensive surface preparation. The purpose of performing these analyses was to detect any metallic...
Abstract
A nickel alloy cylinder plated with chromium along its inner liner, installed in a commercial ice cream freezer, showed gray discoloration along its OD surface. The discolored parts exhibited significantly reduced cooling efficiency as compared with new cylinders. During operation, the OD of the cylinder was exposed to liquid ammonia refrigerant containing lubricant from the compressor. The lubricant (mineral oil) was intended to separate from the ammonia and be recirculated through the compressor. Nondestructive portable optical microscopy, XRF, EDS, and XPS analyses showed that the discoloration on the cylinder was associated with metal oxidation products coated with a thin oil film. One of the recommendations was to plate the OD of the cylinder with hard chromium to increase its resistance to erosion. Another recommendation was to reduce the amounts of water contamination in the refrigerant.
Book Chapter
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.usage.c9001722
EISBN: 978-1-62708-236-5
.... 2 . It will be noted that, as is to be expected, the fatigue cracks followed the line of the pre-existing crack network. In order to investigate the foregoing features microscopically, a specimen was cut from the V-shaped region between the cracks and the oil-hole, the surface prepared lying...
Abstract
The crankshaft of a 37.5-hp, 3-cylinder oil engine was examined. The engine had been dismantled for the purpose of a general overhaul and in the course of this work the crankpins were chromium-plated before regrinding. The engine was returned to service and after running for 290 h the crankshaft broke at the junction of the No. 3 crankpin and the crankweb nearest to the flywheel. A typical fatigue crack had originated at a number of points in the root of the fillet to the web. In its early stages it ran slightly into the web but turned back to the pin when it encountered the oil hole. The shaft had been made from a heat-treated alloy steel. The thickness of the plating was approximately 0.025 in. and numerous cracks were visible in it, several of which had given rise to cracks in the steel below. The primary cause of the crankshaft failure was the plating of the crankpins. The presence of the grooves alone would result in considerable intensification of stress in zones which are normally highly stressed, while the crazy cracking introduced a multiplicity of stress-raisers of a type almost ideal from the point of view of initiating fatigue cracks.
Series: ASM Failure Analysis Case Histories
Volume: 2
Publisher: ASM International
Published: 01 December 1993
DOI: 10.31399/asm.fach.v02.c9001319
EISBN: 978-1-62708-215-0
... of the crown areas would also be tensile. Metallographic inspection of the cracked regions was carried out in situ by using a fixture to position a portable microscope vertically over the cracked region ( Fig. 1 ). Surface preparation was performed using standard commercial equipment. Figure 2 shows...
Abstract
Several type 304L stainless steel dished ends used in the fabrication of cylindrical vessels developed extensive cracking during storage. All of the dished ends had been procured from a single manufacturer and belonged to the same batch. When examined visually, several rust marks were observed, indicating contamination by rusted carbon steel particles. Liquid penetrant testing was used to determine the extent of the cracks, and in situ metallographic analysis was performed over the cracked region. The morphology of the cracks was indicative of transgranular stress-corrosion cracking (TGSCC). Conditions promoting the occurrence of the TGSCC included significant tensile stresses on the inside of the dished ends, the presence of surface contamination by iron due to poor handling practice using carbon steel implements, and storage in a coastal environment with an average temperature of 25 to 32 deg C (77 to 90 deg F), an average humidity ranging from 70 to 80%, and an atmospheric NaCl content ranging from 8 to 45 mg/m2 /day. Recommendations preventing further occurrence of the situation were strict avoidance of the use of carbon steel handling implements, strict avoidance of cleaning practices that cause long-term exposure to chlorine-containing cleaning fluid, and solution annealing of the dished ends at 1050 deg C (1920 deg F) for 1 h followed by water quenching to relieve residual stresses.
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003532
EISBN: 978-1-62708-180-1
... grinding scratches must be removed; even very fine polishing scratches may not be tolerable in examining failed parts. Pullout, pitting, cracking of hard particles, smear, and other preparation artifacts must be avoided. Relief (i.e., excessive surface-height variations between structural features...
Abstract
This article provides a discussion on the metallographic techniques used for failure analysis, and on fracture examination in materials, with illustrations. It discusses various metallographic specimen preparation techniques, namely, sectioning, mounting, grinding, polishing, and electrolytic polishing. The article also describes the microstructure examination of various materials, with emphasis on failure analysis, and concludes with information on the examination of replicas with light microscopy.
Series: ASM Handbook
Volume: 11
Publisher: ASM International
Published: 15 January 2021
DOI: 10.31399/asm.hb.v11.a0006765
EISBN: 978-1-62708-295-2
... by the etchant. Coarse grinding scratches must be removed; even very fine polishing scratches may not be tolerable in examining failed parts. Pullout, pitting, cracking of hard particles, smear, and other preparation artifacts must be avoided. Relief (i.e., excessive surface-height variations between...
Abstract
Metallographic examination is one of the most important procedures used by metallurgists in failure analysis. Typically, the light microscope (LM) is used to assess the nature of the material microstructure and its influence on the failure mechanism. Microstructural examination can be performed with the scanning electron microscope (SEM) over the same magnification range as the LM, but examination with the latter is more efficient. This article describes the major operations in the preparation of metallographic specimens, namely sectioning, mounting, grinding, polishing, and etching. The influence of microstructures on the failure of a material is discussed and examples of such work are given to illustrate the value of light microscopy. In addition, information on heat-treatment-related failures, fabrication-/machining-related failures, and service failures is provided, with examples created using light microscopy.
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.chem.c9001162
EISBN: 978-1-62708-220-4
... Abstract Some 99.90 pure tin tubes (0.15 mm thick) used for packaging a chemical compound cracked on bending and underwent brittle fracture prior to filling, while others remained ductile and showed no sign of failure. Examination showed that specimens prepared by mechanical methods...
Abstract
Some 99.90 pure tin tubes (0.15 mm thick) used for packaging a chemical compound cracked on bending and underwent brittle fracture prior to filling, while others remained ductile and showed no sign of failure. Examination showed that specimens prepared by mechanical methods such as electrolytic and hand polishing and the vibration method resulted in poor edge and crack edge definition due to material thickness. Etching experiments involved a grain surface attack and hence produced a rather strong surface relief from which the grain boundary cracks could again not clearly be differentiated. The sections were therefore examined unetched in polarized light. The microstructure of the cracked tubes was shown to have much smaller grains than the ductile and showed cracks from the surface down along the grain boundaries. Material hardness also differed between the unusable tubes and the ductile, and chemical analysis showed a higher level of aluminum in the brittle specimens. Failure obviously occurred due to the high material aluminum content that increased hardness which then caused embrittlement at the surface which led to cracks or fracture on bending. Since no explanation of how the aluminum entered the tin was available, no recommendations could be made.
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.homegoods.c9001610
EISBN: 978-1-62708-222-8
... conditions (passivation and surface roughness). Review of ASTM medical device standards, 8 however, does not provide any quantitative data concerning surface roughness and finish of surgical implants. One standard, 9 concerning the practice for surface preparation of metallic surgical implants, states...
Abstract
This investigation characterizes five surgical stainless steel piercings and one niobium piercing that caused adverse reactions during use, culminating with the removal of the jewelry. Chemical composition shows that none of the materials are in accordance with ISO standards for surgical implant materials. Additionally, none of the stainless steel piercings passed the pitting-resistance criterion of ISO 5832-1, which implies that [%Cr + 3.3(%Mo)] > 26. Under microscopic examination, most of the jewelry revealed the intense presence of linear irregularities on the surface. The lack of resistance to pitting corrosion associated with the poor surface finishing of the stainless steel jewelry may induce localized corrosion, promoting the release of cytotoxic metallic ions (such as Cr, Ni, and Mo) in the local tissue, which can promote several types of adverse effects in the human body, including allergic reactions. The adverse reaction to the niobium jewelry could not be directly associated with the liberation of niobium ions or the residual presence of cytotoxic elements such as Co, Ni, Mo, and Cr. The poor surface finish of the niobium jewelry seems to be the only variable of the material that may promote adverse reactions.
Series: ASM Failure Analysis Case Histories
Volume: 1
Publisher: ASM International
Published: 01 December 1992
DOI: 10.31399/asm.fach.v01.c9001035
EISBN: 978-1-62708-214-3
... retainer nut, adjacent to the keyway. Fig. 6 SEM micrograph of flat fracture characterstics in the area shown in Fig. 5 , composed of cleavage with river patterns. 4000×. Fig. 11 Overall appearance of fracture surface of exemplar impact coupon prepared from the hardened outer perimeter...
Abstract
Following an accident in which a light pickup truck left the road and overturned, one of the rear axles, made of approximately 0.30C steel, was found to be fractured adjacent to the bearing lock nut. A keyway was present in the failed area, as were threads for the lock nut. Fracture surfaces of the failed axle and exemplar fractures obtained from simulation tests were studied using scanning electron microscope. The examination showed that the outer perimeter fracture in the axle was very flat and composed of cleavage and that the interior portion was composed of both cleavage and dimples. No evidence of prior cracking was found. The exemplar specimens from the simulation impact testing failed in a manner consistent with that observed in the axle. The examination confirmed that the failure was a one-time impact overload fracture and not the result of any prior crack in the material, indicating that the axle failure did not initiate the accident.
Book Chapter
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.modes.c0090460
EISBN: 978-1-62708-234-1
... image showing features characteristic of severe degradation of the filter material. 118× To allow further assessment of the failure, a mounted cross section was prepared through one of the cracks. The cross section, as presented in Fig. 2 , showed a clear zone of degradation along the surface...
Abstract
A component of a water filtration unit failed while being used in service for approximately eight months. The filter system had been installed in a commercial laboratory, where it was stated to have been used exclusively in conjunction with deionized water. The failed part had been injection molded from a 30% glass-fiber and mineral-reinforced nylon 12 resin. Investigation, including visual inspection, 118x SEM images, 9x micrographs, energy-dispersive x-ray spectroscopy, micro-FTIR in the ATR mode, and TGA, supported the conclusion that the filter component failed as a result of molecular degradation caused by the service conditions. Specifically, the part material had undergone severe chemical attack, including oxidation and hydrolysis, through contact with silver chloride. The source of the silver chloride was not established, but one potential source was photographic silver recovery.
Series: ASM Failure Analysis Case Histories
Volume: 2
Publisher: ASM International
Published: 01 December 1993
DOI: 10.31399/asm.fach.v02.c9001273
EISBN: 978-1-62708-215-0
... Fig. 1 An example of the fracture surface observed on the hanger rods. Fig. 2 A macrograph of the prepared section. The arrow points to an area of cracking. Fig. 3 Examples of the cracking observed in the hanger rods. Abstract One-quarter inch diameter 304...
Abstract
One-quarter inch diameter 304 stainless steel cooling tower hanger rods failed by chloride-induced stress-corrosion cracking (SCC). The rods were located in an area of the cooling tower where the air contains drop lets of water below the mist eliminators and above the flow of water The most extensive cracking was observed in the rod nuts and in the portions of the rod which were covered by the nuts. Cracking was transgranular with extensive branching, and some corrosion occurred along the crack paths. The clamping force from the nuts used on both sides of the supported member and residual stresses from thread rolling likely contributed to the stresses for the cracking mechanism, along with the stresses induced by the supported load. The external surfaces of the hanger rods were reportedly exposed to a chloride-containing atmosphere, likely due to the biocide. Type 304 stainless steel is not a suitable material for this application, and materials that resist SCC, such as Inconel, should be considered.
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.aero.c9001216
EISBN: 978-1-62708-217-4
... Abstract Countersunk riveted joints in aluminum sheet are widely employed in the aircraft industry. The preparation of the sheet for the riveting process consists either of countersinking where the sheet is sufficiently thick or of dimpling. Metallographic assessment of dimple defects...
Abstract
Countersunk riveted joints in aluminum sheet are widely employed in the aircraft industry. The preparation of the sheet for the riveting process consists either of countersinking where the sheet is sufficiently thick or of dimpling. Metallographic assessment of dimple defects is described in specimens made of clad aluminum sheet of alloy type AlZnMgCu1.5. Addressed are a dimple with partially missing stamped surface (bell-mouth), a cylindrical prominence because the dimpling force was too great and the stamping cylinder force too low, and a dimple with flashes at the top surfaces of the sheet as a result of play between the stamping cylinder and the anvil head (ringed dimple). Frequently, overlapping of several defects occurs, especially with steel or titanium sheet, with the result that it is difficult to identify the defects.
1