1-20 of 70 Search Results for

special-purpose bearing steels

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0001812
EISBN: 978-1-62708-180-1
... Abstract This article discusses different types of mechanical fasteners, including threaded fasteners, rivets, blind fasteners, pin fasteners, special-purpose fasteners, and fasteners used with composite materials. It describes the origins and causes of fastener failures and with illustrative...
Series: ASM Failure Analysis Case Histories
Volume: 3
Publisher: ASM International
Published: 01 December 2019
DOI: 10.31399/asm.fach.v03.c9001755
EISBN: 978-1-62708-241-9
... Steels, Tool Materials, and Special-Purpose Metals , vol. 3 , Metals Handbook , 9th ed. , American Society for Metals , 1980 , pp. 425 – 426 . 4. Failure Analysis and Prevention , vol. 11 , Metals Handbook , 9th ed. , American Society for Metals , 1986 , pp. 490 – 495 , 506 – 507 . 5...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003520
EISBN: 978-1-62708-180-1
..., detailed failure examination. With many types of “routine” failures, the procedure can be simple and still be effective. Most suppliers are receptive to constructive criticism regarding their products. Individual background, including the area of specialization and professional experience, still has...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003522
EISBN: 978-1-62708-180-1
... in such circumstances. A special case of wear is fretting, in which contacting surfaces are involved in vibration or very small relative motion at high frequency. Generally, corrosion is also involved, because the small particles of material that are removed expose fresh material during the small-amplitude motion...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0001819
EISBN: 978-1-62708-180-1
... and Special-Purpose Materials, Volume 2 of the of ASM Handbook. Fatigue resistance is another general requirement for implants, but the critical loading is different for the various types of implants and applications. The required mechanical strength of orthopedic implants also varies and depends...
Series: ASM Handbook
Volume: 11
Publisher: ASM International
Published: 15 January 2021
DOI: 10.31399/asm.hb.v11.a0006757
EISBN: 978-1-62708-295-2
... and bearings under high contact (Hertzian) loading. Figures 42 and 43 illustrate the subsurface nature of cracking in the carburized surface layer of a tooth in gears manufactured from Deutsche Industrie-Normen (DIN) 17CrNiMo6 steel (0.18 C, 0.38 Mn, 0.008 P, 0.020 S, 0.20 Si, 1.73 Cr, 1.58 Ni, and 0.25 Mo...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.process.c9001647
EISBN: 978-1-62708-235-8
... Matrix of Initial Test Welds Test ID Special Conditions (a) Purpose Results AP-1 CS/Al inner Internal gas and pressure analysis No porosity AP-2 SS inner Internal gas and pressure analysis No porosity AP-3 SS inner, max interference fit Internal gas and pressure analysis...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0001809
EISBN: 978-1-62708-180-1
... is to be transmitted from one part to the other. Mechanical bearings are usually made of selected material and in special geometries in order to effect easy and reliable motion for a specific task. The major types are rolling-element (ball or roller) bearings and sliding bearings. This article will discuss sliding...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003502
EISBN: 978-1-62708-180-1
... facilities, but for each particular facility there was also a detailed set of special requirements. Within these documents were embedded the requirements for the conveying systems in general, and within those the requirements for the vertical lift units in particular. Prototype vertical lift units that used...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003524
EISBN: 978-1-62708-180-1
... of a complete service history depends on how detailed and thorough the record keeping was prior to the failure. A complete service record greatly simplifies the assignment of the failure analyst. In collecting service histories, special attention should be given to environmental details such as normal...
Series: ASM Handbook
Volume: 11
Publisher: ASM International
Published: 15 January 2021
DOI: 10.31399/asm.hb.v11.a0006792
EISBN: 978-1-62708-295-2
... 51. Voskamp A.P. , Fatigue and Material Response in Rolling Contact , ASTM Special Technical Publication , American Society for Testing and Materials , 1998 , p 152 – 166 52. Voskamp A.P. and Mittemeijer E.J. , The Effect of the Changing Microstructure on the Fatigue...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.design.c9001578
EISBN: 978-1-62708-233-4
... , Failure Analysis and Prevention , Vol 11 , ASM Handbook , ASM International , 2002 , p 559 – 586 10.31399/asm.hb.v11.a0003537 Part I—Special Cases Part II—Turbines, Pumps, and Compressors Part III—Fans and Motors Case #1: Vibration in Hydroelectric Dam Case #2: Vibration of Steel...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0001815
EISBN: 978-1-62708-180-1
... are carburized. Some special-purpose steel gears are case hardened by either carbonitriding or nitriding. Other special-purpose gears, such as those used in chemical or food-processing equipment, are made of stainless steels or nickel-base alloys because of their corrosion resistance, their ability to satisfy...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003554
EISBN: 978-1-62708-180-1
... to U.S. Department of Transportation , 1988 9. Roberts A.I. , Safety Advisory; High Pressure Aluminum Composite Hoop-Wrapped Cylinders, Research and Special Programs Administration, Department of Transportation , Fed. Reg. , Vol 59 , ( No. 142 ), 1994 , p 38028 10. Sperling...
Series: ASM Handbook
Volume: 11
Publisher: ASM International
Published: 15 January 2021
DOI: 10.31399/asm.hb.v11.a0006765
EISBN: 978-1-62708-295-2
... and are very effective. Besides these papers, there are several other options available. One option is to planar grind the specimens with a conventional alumina grinding stone. This requires a special-purpose machine, because the stone must rotate at a high speed, ≥1500 rpm, to cut effectively. The stone must...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003500
EISBN: 978-1-62708-180-1
.... The discipline of failure analysis has evolved and matured, as it has been employed and formalized as a means for failure prevention. Consistent with the recent trend toward increased accountability and responsibility, its purpose has been extended to include determining which party may be liable for losses...
Series: ASM Failure Analysis Case Histories
Volume: 1
Publisher: ASM International
Published: 01 December 1992
DOI: 10.31399/asm.fach.v01.c9001099
EISBN: 978-1-62708-214-3
... compressor installation and during disassembly for repair, no special precautions were taken to exclude moisture or ambient atmospheres from the compressor chamber or its components. Microhardness measurements (Knoop scale) were made on the polished metallographic samples. Several readings were taken...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003529
EISBN: 978-1-62708-180-1
... the analyst is not very familiar with the alloy system in question. For example, the potential consequences of exceeding impurity limits for zinc and aluminum casting alloys are discussed in various articles in Properties and Selection: Nonferrous Alloys and Special-Purpose Materials, Volume 2 of ASM...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003501
EISBN: 978-1-62708-180-1
... requirements involving corrosion resistance and elevated-temperature service. Many other engineering disciplines also have unique and special requirements for design and materials selection. In electrical engineering design, for example, the physical property requirements (e.g., magnetic, electrical...
Series: ASM Handbook
Volume: 11
Publisher: ASM International
Published: 15 January 2021
DOI: 10.31399/asm.hb.v11.9781627082952
EISBN: 978-1-62708-295-2