... Abstract The article commences with an overview of short-term and long-term mechanical properties of polymeric materials. It discusses plasticization, solvation, and swelling in rubber products. The article further describes environmental stress cracking and degradation of polymers...
Series: ASM Handbook
Volume: 11B
Publisher: ASM International
Published: 15 May 2022
DOI: 10.31399/asm.hb.v11B.a0006917
EISBN: 978-1-62708-395-9
... parameters are commonly used when evaluating interactions of solvents with polymers ( Ref 2 ). The general idea is that materials with similar solubility parameters will show interaction with each other, resulting in solvation, miscibility, or swelling. The concept of ESC involves similar types...
Series: ASM Handbook
Volume: 11B
Publisher: ASM International
Published: 15 May 2022
DOI: 10.31399/asm.hb.v11B.a0006867
EISBN: 978-1-62708-395-9
... degradation of the polymer, breaking the macromolecular chains, reducing molecular weight, and diminishing polymer properties as a result. Each of these effects is examined in subsequent paragraphs. Plasticization, Solvation, and Swelling Certain interactions between liquid chemicals and polymers can...
Series: ASM Handbook
Volume: 11B
Publisher: ASM International
Published: 15 May 2022
DOI: 10.31399/asm.hb.v11B.a0006933
EISBN: 978-1-62708-395-9
... in addressing polymeric degradation, the technique is also useful in evaluating the failed sample material for chemical contact. Plastic materials can be affected in several ways through contact with chemical agents. Depending on the polymer/chemical combination, solvation, plasticization, additive abstraction...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003525
EISBN: 978-1-62708-180-1
..., solvation, plasticization, chemical attack, or environmental stress cracking can occur. In the case of property alteration through solvation or plasticization, FTIR can be helpful in identifying the absorbed chemicals. Because these chemicals are present within the failed plastic material, the likelihood...
Series: ASM Handbook
Volume: 11B
Publisher: ASM International
Published: 15 May 2022
DOI: 10.31399/asm.hb.v11B.a0006942
EISBN: 978-1-62708-395-9
..., such as fibrils caused by ductile deformation, shear yielding, and tearing, can be found, but higher magnifications may be needed to see microfibrils. Others features such as crack growth directionality caused by creep and fatigue may also be seen, as well as evidence of solvation, environmental stress cracking...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003555
EISBN: 978-1-62708-180-1
... conditions. Reducing conditions tend to lower the melting temperature of any deposited slag, which also increases the solvation of the normal oxide scales. A stable gaseous sulfur compound under reducing conditions is H 2 S. Under the reducing environment, iron sulfide is the expected corrosion product...
Series: ASM Handbook
Volume: 11B
Publisher: ASM International
Published: 15 May 2022
DOI: 10.31399/asm.hb.v11B.a0006939