Series: ASM Failure Analysis Case Histories
Volume: 3
Publisher: ASM International
Published: 01 December 2019
DOI: 10.31399/asm.fach.v03.c9001811
EISBN: 978-1-62708-241-9
..., the uniformity in hardness along the circumference of the tube also did not indicate the inhomogenity in material. However, XRD revealed the presence of 1–6% retained austenite at various locations. Since the austenite is the softer phase compared with bainite, it will be expected that the transformation of rest...
Series: ASM Handbook
Volume: 11B
Publisher: ASM International
Published: 15 May 2022
DOI: 10.31399/asm.hb.v11B.a0006931
EISBN: 978-1-62708-395-9
... crystal phases and structures in solid materials. failure analysis infrared spectroscopy nuclear magnetic resonance spectroscopy polymer structure thermal analysis X-ray diffraction FAILURE OF POLYMERIC materials is the result of a very complex process. This article introduces procedures...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003570
EISBN: 978-1-62708-180-1
... that are far more erosion resistant than the standard constructional materials described earlier are well known. The best of these, exemplified by cobalt-base alloys and NiTi alloys, are characterized by energy-absorbing deformation modes: fine twinning, stress- or strain-induced phase transformation...
Series: ASM Handbook
Volume: 11B
Publisher: ASM International
Published: 15 May 2022
DOI: 10.31399/asm.hb.v11B.a0006941
EISBN: 978-1-62708-395-9
... Abstract This article describes the viscoelastic behavior of plastics in their solid state only, from the standpoint of the material deforming without fracturing. The consequences of viscoelasticity on the mechanical properties of plastics are described, especially in terms of time-dependencies...
Series: ASM Handbook
Volume: 11A
Publisher: ASM International
Published: 30 August 2021
DOI: 10.31399/asm.hb.v11A.a0006826
EISBN: 978-1-62708-329-4
... (macroscopic and microscopic) Residual-tension stress distribution in surface layer Processing inclusions introduced Plastically deformed debris as a result of grinding Voids, pits, burrs, or foreign material inclusions in surface Physical Transformation of phases Grain size and distribution...
Series: ASM Handbook
Volume: 11B
Publisher: ASM International
Published: 15 May 2022
DOI: 10.31399/asm.hb.v11B.a0006930
EISBN: 978-1-62708-395-9
... that are predominantly in the solid state and the methods employed for solids testing. Examples of unidirectional and dynamic oscillatory testing are provided for different mechanical behaviors. deformation flow behavior polymers rheological testing Rheology Fundamentals Rheology is defined as the study...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003526
EISBN: 978-1-62708-180-1
... design software. It is now possible to quickly create 3-D solid models with automatic mesh generation rather than having to input each individual node location. It is common for desktop computer and workstations to be able to handle complex 3-D FEA linear and steady-state models and simpler nonlinear...
Series: ASM Handbook
Volume: 11
Publisher: ASM International
Published: 15 January 2021
DOI: 10.31399/asm.hb.v11.a0006773
EISBN: 978-1-62708-295-2
..., linearity, and steady-state conditions. As computing power increased, so did the complexity of finite-element modeling and analysis techniques. The first analyses and elements available were limited to 2D beams and spars. The progression was then toward three-dimensional (3D) spars and beams, 2D solid...
Series: ASM Handbook
Volume: 11B
Publisher: ASM International
Published: 15 May 2022
DOI: 10.31399/asm.hb.v11B.a0006933
EISBN: 978-1-62708-395-9
... limited quantitative, information regarding the composition and state of the material evaluated. Fourier transform infrared spectroscopy uses infrared energy to produce vibrations within the molecular bonds that constitute the material being evaluated. Vibrational states of varying energy levels exist...
Series: ASM Handbook
Volume: 11
Publisher: ASM International
Published: 15 January 2021
DOI: 10.31399/asm.hb.v11.a0006778
EISBN: 978-1-62708-295-2
... • Little distortion evident • Intergranular or transgranular • May relate to notches at surface or brittle phases internally • Progressive zone: usually transgranular with little apparent distortion • Overload zone: may be either ductile or brittle • Microstructural change typical of overheating...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003543
EISBN: 978-1-62708-180-1
... at surface or brittle phases internally • Progressive zone: usually transgranular with little apparent distortion• Overload zone: may be either ductile or brittle • Microstructural change typical of overheating• Multiple intergranular cracks• Voids formed on grain boundaries or wedge shaped cracks at grain...
Series: ASM Handbook
Volume: 11
Publisher: ASM International
Published: 15 January 2021
DOI: 10.31399/asm.hb.v11.a0006787
EISBN: 978-1-62708-295-2
... surface in different orientations Growth of graphite into the metal phase by carbon atoms from the solid solution, attaching to graphite planes growing vertical to the metal surface Destruction of the metal phase by the inward-growing graphite under transfer of metal particles into the “coke” layer...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003545
EISBN: 978-1-62708-180-1
... instabilities, such as transgranular-intergranular fracture transition, recrystallization, aging or overaging (phase precipitation or decomposition of carbides, borides, or nitrides), intermetallic-phase precipitation, delayed transformation to equilibrium phases, order-disorder transition, general oxidation...
Series: ASM Handbook
Volume: 11
Publisher: ASM International
Published: 15 January 2021
DOI: 10.31399/asm.hb.v11.a0006780
EISBN: 978-1-62708-295-2
... change of slope in a rupture life curve can occur from metallurgical instabilities, such as TG-IG fracture transition, recrystallization, aging or overaging (phase precipitation or decomposition of carbides, borides, and nitrides), intermetallic-phase precipitation, delayed transformation to equilibrium...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003510
EISBN: 978-1-62708-180-1
... Abstract This article provides an overview of the effects of various material- and process-related parameters on residual stress, distortion control, cracking, and microstructure/property relationships as they relate to various types of failure. It discusses phase transformations that occur...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003538
EISBN: 978-1-62708-180-1
...), and the activation of a given mechanism depends on the temperature, loading rate, and degree of constraint. In an ideal material containing neither inclusions nor second phases, ductile fracture would be expected to occur by slip and possibly twinning and result in complete reduction in area ( Fig. 1 ). Ref 1...
Series: ASM Handbook
Volume: 11A
Publisher: ASM International
Published: 30 August 2021
DOI: 10.31399/asm.hb.v11A.a0006816
EISBN: 978-1-62708-329-4
... Abstract This article introduces some of the general sources of heat treating problems with particular emphasis on problems caused by the actual heat treating process and the significant thermal and transformation stresses within a heat treated part. It addresses the design and material factors...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003530
EISBN: 978-1-62708-180-1
... of stress transformations are discussed first, and then the determination of stress maxima is discussed. To define stress transformation, it is easier to start with a two-dimensional case. One common way to define a two-dimensional (2-D) stress state is with a plane stress assumption. Plane stress...
Series: ASM Handbook
Volume: 11
Publisher: ASM International
Published: 15 January 2021
DOI: 10.31399/asm.hb.v11.a0006767
EISBN: 978-1-62708-295-2
..., and a procedure to deal with stress by determining maximum values through stress transformation is described. The article provides the stress analysis equations of typical component geometries and discusses some of the implications of the stress analysis relative to failure in components. It focuses on linear...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003555
EISBN: 978-1-62708-180-1
... in the nickel-iron matrix Deposition of graphite on the alloy surface in different orientations Growth of graphite into the metal phase by carbon atoms from the solid solution, attaching to graphite planes growing vertical to the metal surface Destruction of the metal phase by the inward-growing...