Fig. 31 Radial marks on tensile test specimen of Society of Automotive Engineers (SAE) 4150 steel isothermally transformed to bainite, quenched to room temperature, and then tempered. (a) Lower bainite, isothermally transformed at 300 °C (570 °F) for 1 h, tempered at 600 °C (1110 °F) for 48 h More
Image
Published: 30 August 2021
Fig. 10 American Society of Mechanical Engineers smooth-bar fatigue curve for carbon and low-alloy steels (ultimate tensile strength < 550 MPa, or 80 ksi). Adapted from Ref 16 More
Image
Published: 15 May 2022
Fig. 4 Thermal analysis of Society of Plastics Engineers (SPE) reference plastics. Identification numbers are tied to SPE resin kit (see Table 6 ) More
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003569
EISBN: 978-1-62708-180-1
..., and gearboxes. It provides information on the cavitation resistance of materials and other prevention parameters. The article describes two American Society for Testing and Materials (ASTM) standards for the evaluation of erosion and cavitation, namely, ASTM Standard G 32 and ASTM Standard G 73. It concludes...
Series: ASM Handbook
Volume: 11A
Publisher: ASM International
Published: 30 August 2021
DOI: 10.31399/asm.hb.v11A.a0006817
EISBN: 978-1-62708-329-4
... Abstract Reliability-centered maintenance (RCM) is a systematic methodology for preventing failures. This article begins by discussing the history of RCM and uses Society of Automotive Engineers (SAE) all-industry standard JA1011 as its model to describe the key characteristics of an RCM...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003505
EISBN: 978-1-62708-180-1
... someone (usually the designer) did not thoroughly think through how the product interfaced with society. Products Recall Planning It is a fact of life that mistakes are sometimes made even by highly experienced professionals exercising utmost care. When such errors occur, a products recall may...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.chem.c9001534
EISBN: 978-1-62708-220-4
.... Kartic Babu, and M. Radhika for their help during various stages of this investigation. References References 1. Metals and Alloys in the Unified Numbering System , 4th ed. , Society of Automotive Engineers , 1986 , p 127 2. Metals Handbook , Vol 1 , Properties and Selection of Irons...
Image
Published: 30 August 2021
Fig. 15 Time-temperature-transformation diagram for Inconel 718. Adapted from Ref 37 . Copyright 1991 by The Minerals, Metals & Materials Society. Used with permission More
Series: ASM Failure Analysis Case Histories
Volume: 2
Publisher: ASM International
Published: 01 December 1993
DOI: 10.31399/asm.fach.v02.c9001372
EISBN: 978-1-62708-215-0
... Society for Metals , 1964 , p 245 . 3. Parr J.G. and Hanson A. , Stainless Steel , American Society for Metals , 1965 . 4. Metals Handbook , 8th ed. , Vol. 1 , American Society for Metals , 1961 , p 421 . 5. Metals Handbook , 8th ed. , Vol. 10 , American Society...
Image
Published: 15 May 2022
Fig. 27 Schematic of the determination of critical fracture loads and relevant time-to-fracture values for the European Structural Integrity Society (ESIS; ISO) method and the peak load method More
Image
Published: 15 May 2022
Fig. 4 Brittle creep fracture surfaces in HDPE pipe; (a) continuous and (b) step-wise crack growth. Courtesy of Society of Plastics Engineers (SPE). Source: Ref 2 More
Image
Published: 30 August 2021
Fig. 9 Illustration of surface texture: roughness, waviness, lay, and flaws. Source: Ref 13 . Reprinted from ANSI/ASME B46.1-1985, by permission of The American Society of Mechanical Engineers. All rights reserved More
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.aero.c9001910
EISBN: 978-1-62708-217-4
... on Maraging Steels , American Society for Metals , Materials Park, OH , 1979 , p. 370 . 2. Vishnevsky C. : Interim Report—Contract DAAG 46–69-C-0060 , Army Materials and Mechanics Research Center , February 1970 , p. 34 . 3. Anon. : in Carburizing and Carbonitriding , Gray A.G...
Image
Published: 30 August 2021
Fig. 11 Adjustment for mean stress effects and factors of 2 and 20 applied to best-fit S - N curves for carbon and low-alloy steels to generate the American Society of Mechanical Engineers (ASME) code design fatigue curves. Adapted from Ref 43 More
Image
Published: 15 May 2022
Fig. 3 Micrographs of worn surface of (a) neat polyetheretherketone, PEEK, (b) polytetrafluoroethylene (PTFE)/ PEEK composite, (c) neat PTFE after 50-hour sliding friction and wear tests. Source: Ref 19 . This figure is reprinted from the Proceedings of the American Society for Composites More
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.usage.c9001672
EISBN: 978-1-62708-236-5
.... , Spring Designer's Handbook , Marcel Decker, Inc. , New York , pp. 177 – 197 ( 1978 ). 2. Maker J. H. , “Steel Springs,” Metals Handbook , 9th Edition , Vol. 1 , American Society for Metals , Metals Park, OH , pp. 283 – 313 ( 1978 ). 3. Swanson R. E. et al. , “Effects...
Image
Published: 30 August 2021
Fig. 5 Micrographs of cracks after heat treatment caused by seams in the steel. (a) Society of Automotive Engineers (SAE) 8630 steel as-quenched; microstructure is martensite where cracking initiated from rolling seam (b) SAE type 403 stainless steel as-quenched and tempered; microstructure More
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.med.c9001664
EISBN: 978-1-62708-226-6
... Society of America , Claitor's Publishing Division , Baton Rouge, LA , pp. 288 – 289 ( 1977 ). 6. Rostoker W. , Chao E. Y. S. and Galante J. O. , “Defects in Failed Stems of Hip Prostheses,” Journal of Biomedical Materials Research , Vol. 12 , pp. 635 – 651 ( 1978 ). 7...
Image
Published: 15 January 2021
, An Evaluation of Fretting at Small Slip Amplitudes, Materials Evaluation under Fretting Conditions , STP 780, American Society for Testing and Materials, 1982, p 30–48, copyright ASTM International, 100 Barr Harbor Drive, West Conshohocken, PA 19428 More
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.homegoods.c9001677
EISBN: 978-1-62708-222-8
... ( 1976 ). 2. Taylor J. , Superminds: An Enquiry into the Paranormal , Macmillan , London ( 1975 ). 3. “The Uri Geller Effect,” editorial review by Duckworth W.E. , Chilterns Metallurgical Society , Jan . 7 , 1977 , Metals and Materials , pp. 51 – 52 ( Oct . 1977...