Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.machtools.c9001229
EISBN: 978-1-62708-223-5
...Abstract Abstract Two slitting saw blades were delivered for the purpose of determining the cause of damage. One had cracked while the other one came from a prior sheet delivery, that had less tendency to crack formation according to the manufacturer. The blades were supposed to have been...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.bldgs.c9001261
EISBN: 978-1-62708-219-8
...Abstract Abstract A ceiling in a concrete structure was hung on flat bars with a cross section of 30 x 80 mm. The bars were borne by a slit steel plate and supported by tabs that were welded onto the flat sides. One of the bars fractured during mounting when it was dropped from a height...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.modes.c9001152
EISBN: 978-1-62708-234-1
...-alloyed steel with 39 kg/sq mm tensile strength, which had been strengthened by welding plate strips on both sides had fractured in service; an axle tube out of 40 Mn 4 after DIN 17 200 from a paper fabrication machine, which had three short longitudinal slits distributed uniformly over its surface...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003536
EISBN: 978-1-62708-180-1
... surface. The combination of the fractographs and serial sections clearly reveal the fracture segment generated due to the nucleation and growth of void(s) around the constituent particles present in the recrystallized grains. Fig. 13 Slit-island method for measuring fractal dimensions...
Series: ASM Failure Analysis Case Histories
Volume: 1
Publisher: ASM International
Published: 01 December 1992
DOI: 10.31399/asm.fach.v01.c9001045
EISBN: 978-1-62708-214-3
... to Failure Pertinent Specifications Specimen Selection The tubes were slit longitudinally to facilitate the examination of the inner wall. The longitudinal section taken from one of the received tubes is shown in Fig. 1 . The inner surface was covered by a reddish deposit, whereas the outside...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.rail.c9001175
EISBN: 978-1-62708-231-0
... in narrow slits. Hot nitrate solutions are very corrosive. Therefore this solution is used to test steels for caustic embrittlement 3 . Internal stresses, especially in cold-worked zones are also taken into account. The classic example of an intercrystalline stress corrosion is the well known rivet...
Series: ASM Failure Analysis Case Histories
Volume: 2
Publisher: ASM International
Published: 01 December 1993
DOI: 10.31399/asm.fach.v02.c9001282
EISBN: 978-1-62708-215-0
... pipe by welding. Because of stringent weld fit-up tolerances, each half was to be made from a full conical reducer by slitting it into two unequal parts and using the larger half after machining to the required size. The conical reducers from which the two halves were made were machined from two...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.bldgs.c9001576
EISBN: 978-1-62708-219-8
... casing ( Fig. 1 ). The rated rotation speed is 1, 750 rpm. Blades are of the shape as shown in Fig. 2(a) and are blanked from coldrolled steel sheet. As shown in Fig. 3 , both ends of the blade are inserted into the slits provided on the disk or the ring. Fig. 1 Multi blade Fan Fig. 2...
Series: ASM Failure Analysis Case Histories
Volume: 2
Publisher: ASM International
Published: 01 December 1993
DOI: 10.31399/asm.fach.v02.c9001304
EISBN: 978-1-62708-215-0
... the nature of the fusion-boundary cracks, a transverse section containing the crack was slit open using a precision diamond saw. Subsequent SEM examination of the opened region revealed an intergranular type of separation along columnar dendrite boundaries ( Fig. 7 ), which is typical of fusion-zone...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.conag.c9001723
EISBN: 978-1-62708-221-1
... and not slit longitudinally from sheets, the purpose of this stipulation being to ensure that the butt-weld is not made between edges where the internal segregated zone has been exposed by slitting. Steels of the rimming type may be distinguished from those of the killed variety by taking a sulphur print...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003569
EISBN: 978-1-62708-180-1
.... , Jet-in-Slit Test for Studying Erosion-Corrosion , Laboratory Corrosion Tests and Standards , STP 866, Haynes G.S. and Baboian R. , Ed., ASTM , 1985 , p 358 – 372 59. Hobbs J.M. , Report 69, National Engineering Laboratory , 1962 60. Holt J.W. and Wood...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003573
EISBN: 978-1-62708-180-1
...-rolled and slit strip because flattened wire could not be obtained in time to meet the delivery schedule. After a presetting operation, the strip springs were consistently out of tolerance; they had taken an excessive set. The Inconel strip had a hardness of 360 HV, compared to 390 HV for the wire...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003516
EISBN: 978-1-62708-180-1
... with Arbitrary Non-Linear Stress Strain Law , J. Appl. Mech. , Vol 28 , p 544 – 550 22. Dugdale D.S. , Yielding of Steel Sheets Containing Slits , J. Mech. Phys. Sol , Vol 8 , 1960 , p 100 – 108 10.1016/0022-5096(60)90013-2 23. Gallagher J.P. et al. , “A Generalized...
Series: ASM Handbook
Volume: 11
Publisher: ASM International
Published: 15 January 2021
DOI: 10.31399/asm.hb.v11.a0006797
EISBN: 978-1-62708-295-2
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003528
EISBN: 978-1-62708-180-1
... such as the dislocation density, the crystallite size in the sample, and instrumental effects such as slit size and defocusing ( Ref 1 ). In practice, that is, in most cases, XRD patterns obtained from real-life components exhibit broadening due to cold-working effects such as machining, grinding, shot peening, and so...
Series: ASM Handbook
Volume: 11
Publisher: ASM International
Published: 15 January 2021
DOI: 10.31399/asm.hb.v11.a0006768
EISBN: 978-1-62708-295-2
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003507
EISBN: 978-1-62708-180-1