1-19 of 19 Search Results for

shape memory alloys

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Series: ASM Handbook
Volume: 11A
Publisher: ASM International
Published: 30 August 2021
DOI: 10.31399/asm.hb.v11A.a0006836
EISBN: 978-1-62708-329-4
... failure. It also covers failures of shape memory alloy springs and failures caused by corrosion and operating conditions. corrosion failure analysis fatigue failures material defects mechanical springs shape memory alloys MECHANICAL SPRINGS are used in mechanical components to exert force...
Series: ASM Failure Analysis Case Histories
Volume: 3
Publisher: ASM International
Published: 01 December 2019
DOI: 10.31399/asm.fach.v03.c9001802
EISBN: 978-1-62708-241-9
... microscopy strain nitinol (nickel-titanium shape memory alloy) UNS N01555 Introduction Experimental Tensile Overload Torsional Overload Fatigue Hydrogen Embrittlement Compressive Damage Kinking Failures Conclusions Acknowledgments References References 1. Gall K...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.med.c9001690
EISBN: 978-1-62708-226-6
.... Orthod. Dentofac. , Foster B.E. , ed., 1982 , vol. 81 ( 1 ), pp. 45 – 49 . 33. Rondelli G. , Vicentini B. , and Cigada A. : Corrosion Properties of NiTi Shape Memory Alloys , vol. 9 , MRS , Tokyo , 1989 , pp. 237 – 242 . 34. Anon : in Standard Specification...
Series: ASM Failure Analysis Case Histories
Volume: 3
Publisher: ASM International
Published: 01 December 2019
DOI: 10.31399/asm.fach.v03.c9001841
EISBN: 978-1-62708-241-9
... stents fracture ultrasonic vibration damage stainless steel nitinol striations beach marks SEM analysis natural frequency 316L (austenitic wrought stainless steel) UNS S31603 nitinol (nickel-titanium shape memory alloy) UNS N01555 Background Case Study 1: 316L Stainless Steel Stent...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003570
EISBN: 978-1-62708-180-1
... of NiTi and CuZnAl Shape Memory Alloys , Proc. Fifth Int. Conf. on the Strength of Metals and Alloys , Haasen P. , Gerold V. , and Kostorz G. , Ed., Pergamon , 1979 , p 1243 – 1248 14. Richman R.H. , Maasberg J.A. , and Rao A.S. , Comparison of Actual...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003566
EISBN: 978-1-62708-180-1
... hammer: 50–60 Ball-peen hammer: 50–57 <60 cm (25 in.) handle: 92–105 HRB >60 cm (25 in.) handle: 40–45 HRC ANSI B209.3-1990 Wood splitting wedges Carbon steel (ASTM A29, A576, A681) 35 max Drop-weight test, 4.5 kg (10 lb) from 1.5 m (5 ft) ANSI B209.1-1991 Chisels Carbon or alloy steel...
Series: ASM Handbook
Volume: 11A
Publisher: ASM International
Published: 30 August 2021
DOI: 10.31399/asm.hb.v11A.a0006811
EISBN: 978-1-62708-329-4
... , SMST-2003 Proceedings of the International Conference on Shape Memory and Superelastic Technologies , 2004 , p 321 – 324 56. James B.A. , McVeigh C. , Rosenbloom S.N. , Guyer E.P. , and Lieberman S.I. , Ultrasonic Cleaning-Induced Failures in Medical Devices , J...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003510
EISBN: 978-1-62708-180-1
.... The formation of these products and the proportions of each are dependent on the time and temperature cooling history of the particular alloy and the elemental composition of that alloy. The transformation products formed are typically illustrated with the use of transformation diagrams, which show...
Series: ASM Handbook
Volume: 11
Publisher: ASM International
Published: 15 January 2021
DOI: 10.31399/asm.hb.v11.a0006773
EISBN: 978-1-62708-295-2
..., with emphasis on structural analysis. However, the ongoing advances in computing power and speed have continued to reduce computational costs, where personal computers (PCs) with very efficient and strong computing-powered central processing units and enormous amounts of dedicated memory are quite readily...
Series: ASM Handbook
Volume: 11
Publisher: ASM International
Published: 15 January 2021
DOI: 10.31399/asm.hb.v11.9781627082952
EISBN: 978-1-62708-295-2
Series: ASM Failure Analysis Case Histories
Volume: 3
Publisher: ASM International
Published: 01 December 2019
DOI: 10.31399/asm.fach.v03.c9001762
EISBN: 978-1-62708-241-9
.... Other documented axles with photographs were also re-inspected at this time with the same results, no dents. These dents are present in a fully martensitic structure which appears to have a shape memory effect [ 5 ] over a period of at least 5 years. Button dents were still present when the end...
Series: ASM Handbook
Volume: 11A
Publisher: ASM International
Published: 30 August 2021
DOI: 10.31399/asm.hb.v11A.9781627083294
EISBN: 978-1-62708-329-4
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003536
EISBN: 978-1-62708-180-1
... In a random plane through bulk microstructure Voids 15.5 1.6 Inclusions 7.5 1.9 Source: Ref 14 , 30 Fig. 15 Systematic random sampling of fields of view Fig. 17 Scanning electron microscope fractograph of fracture surface of a wrought aluminum alloy. Observe...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003526
EISBN: 978-1-62708-180-1
... (a) thread contact and (b) distortion and stress state Fig. 6 Example of an elastic/plastic finite element analysis. (a) Photograph showing distorted transformer housing from internal overpressurization. (b) Finite element results showing permanently distorted shape and stress contours Fig...
Series: ASM Handbook
Volume: 11
Publisher: ASM International
Published: 15 January 2021
DOI: 10.31399/asm.hb.v11.a0006753
EISBN: 978-1-62708-295-2
... or systems. In a broad sense, form, fit, function, and service life represent the technically relevant properties of a product. The form, or physical characteristics of components or products, includes the size and shape of a product as well as the materials of construction and the manufacturing techniques...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003555
EISBN: 978-1-62708-180-1
...Suggested maximum temperatures for various alloys in continuous, isothermal oxidizing atmospheres without excessive scaling Table 1 Suggested maximum temperatures for various alloys in continuous, isothermal oxidizing atmospheres without excessive scaling Alloy designation Temperature...
Series: ASM Handbook
Volume: 11
Publisher: ASM International
Published: 15 January 2021
DOI: 10.31399/asm.hb.v11.a0006755
EISBN: 978-1-62708-295-2
... A good definition of a failure is “the inability of a component, machine, process, or culture/thinking to function properly.” It is not just things that break. Failures come in all shapes and sizes. They can be individual parts, entire machines, an assembly, a system, or a process. Broken down...
Series: ASM Handbook
Volume: 11A
Publisher: ASM International
Published: 30 August 2021
DOI: 10.31399/asm.hb.v11A.a0006819
EISBN: 978-1-62708-329-4
... Including Non-Proportional Hardening and Variable Amplitude Loading Effects ,” Dissertation for Doctor of Philosophy Degree in Engineering, The University of Toledo , 2010 37. Price J. , Weld Cracking in Ferrous Alloys , Singh R. , Ed., Woodhead Publishing , United Kingdom , 2008...
Series: ASM Handbook
Volume: 11A
Publisher: ASM International
Published: 30 August 2021
DOI: 10.31399/asm.hb.v11A.a0006834
EISBN: 978-1-62708-329-4
... 1 , 2 Fig. 34 Low-alloy steel roller bearing from an improperly grounded electric motor that was pitted and etched by electrolytic action of stray electric currents in the presence of moisture Fig. 35 Different wearing patterns observed in rolling-element bearings. (a) Smearing...