1-2 of 2 Search Results for

shale oil

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.bldgs.c9001702
EISBN: 978-1-62708-219-8
... concrete cast around rebar; concrete surface sealed with linseed oil; steel rocker assemblies sand blasted and painted. (Note: no details about the mix design of the patch concrete were found). July 1970 - rebar showing on column and rust streaks; small cracks on outside of all beams; transverse...
Series: ASM Handbook
Volume: 11
Publisher: ASM International
Published: 15 January 2021
DOI: 10.31399/asm.hb.v11.a0006795
EISBN: 978-1-62708-295-2
... of Steels and Elastomers , Wear , Vol 388–389 , 2017 , p 126 – 135 10.1016/j.wear.2017.06.004 90. Finnie I. , Some Observations on the Erosion of Ductile Metals , Wear , Vol 19 , 1972 , p 81 – 90 10.1016/0043-1648(72)90444-9 91. Ots A. , Oil Shale Fuel Combustion...