Series: ASM Failure Analysis Case Histories
Volume: 1
Publisher: ASM International
Published: 01 December 1992
DOI: 10.31399/asm.fach.v01.c9001080
EISBN: 978-1-62708-214-3
... Abstract A steam turbine developed excessive noise and vibration during routine operation. It was found that the nut that locked the turbine disk In place had worked its way out from the threads and the disk had come of the shaft. Examination of the locking mechanism indicated that its design...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.mech.c0047105
EISBN: 978-1-62708-225-9
... Abstract The locking collar on a machine failed suddenly when the shaft it restrained was inadvertently subjected to an axial load slightly higher than the allowable working load. The locking collar fractured abruptly, producing four large fragments. This allowed the shaft to be propelled...
Series: ASM Failure Analysis Case Histories
Volume: 1
Publisher: ASM International
Published: 01 December 1992
DOI: 10.31399/asm.fach.v01.c9001023
EISBN: 978-1-62708-214-3
... and of the bevel gear had failed completely from severe fretting wear. The splines of the shaft had been plated with a silver alloy to provide fretting wear resistance. The bevel gear is normally held to the shaft by a special castellated nut, support ring, and a nut locking mechanism (which was not available...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.usage.c9001427
EISBN: 978-1-62708-236-5
... of the order of 0.3%. The failure resulted principally from the stress-raising effects of the screw holes combined with the cracks in the welds. If the screw holes had been left unfilled or if some form of mechanical locking had been used if plugged, failure would have been postponed if not averted...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.aero.c9001910
EISBN: 978-1-62708-217-4
... the M61A1 Gatling gun used on F-14 and F-18 Navy fighter jets. In addition, an individual locking block was examined. Similar components had exhibited accelerated wear during F-14 gun mount firing tests conducted at NAWCAD, Patuxent River. The Investigation A multitude of tests were performed at ARL...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.process.c9001436
EISBN: 978-1-62708-235-8
... fracture The following account relates to the failure of a shaft in a brittle manner shortly after the welding had been completed, and serves to illustrate the magnitude of the locked-up stresses which can result from such an operation. The shaft, of 3 in. diameter, was found to have suffered...
Series: ASM Failure Analysis Case Histories
Volume: 3
Publisher: ASM International
Published: 01 December 2019
DOI: 10.31399/asm.fach.v03.c9001828
EISBN: 978-1-62708-241-9
... by the pump supplier based on their past experience and meet the additional requirements imposed by the purchaser. Pump Impeller: The impeller is fitted at the bottom end of the tapered shaft and is keyed and locked in place. The impeller material is SA-487 CA-6NM. The impeller is 100...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.mech.c0089254
EISBN: 978-1-62708-225-9
... Abstract A failed tapered-ring sprocket locking device consisted of an assembly of four tapered rings that are retained by a series of cap screws. The middle wedge-shaped rings were pulled closer as the screws were tightened forcing the split inner ring to clamp tightly onto the shaft. One...
Series: ASM Failure Analysis Case Histories
Volume: 1
Publisher: ASM International
Published: 01 December 1992
DOI: 10.31399/asm.fach.v01.c9001035
EISBN: 978-1-62708-214-3
... Abstract Following an accident in which a light pickup truck left the road and overturned, one of the rear axles, made of approximately 0.30C steel, was found to be fractured adjacent to the bearing lock nut. A keyway was present in the failed area, as were threads for the lock nut. Fracture...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.chem.c9001713
EISBN: 978-1-62708-220-4
... on evaluations of the blender to determine if material or mechanical failures were the cause of the accident. The results indicate that the mixing vessel was metallurgically sound and did not contribute to the initiation of the failure. However, the vessel was not designed for mixing chemicals that must...
Series: ASM Failure Analysis Case Histories
Volume: 3
Publisher: ASM International
Published: 01 December 2019
DOI: 10.31399/asm.fach.v03.c9001819
EISBN: 978-1-62708-241-9
... to work, but after less than 3 months the shaft was broken. In the second case, the shaft was installed in the pump and after around 2 months it was broken on the edge where a nut locked the rotor in the shaft. The chemical composition of duplex stainless steel, obtained through x-ray fluorescence...
Book Chapter

Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003562
EISBN: 978-1-62708-180-1
... Abstract This article reviews the general characteristics of fretting wear in mechanical components with an emphasis on steel. It focuses on the effects of physical variables and the environment on fretting wear. The variables include the amplitude of slip, normal load, frequency of vibration...
Series: ASM Handbook
Volume: 11
Publisher: ASM International
Published: 15 January 2021
DOI: 10.31399/asm.hb.v11.a0006829
EISBN: 978-1-62708-295-2
.... This article focuses on fretting wear related to debris formation and ejection. It reviews the general characteristics of fretting wear, with an emphasis on steel. The review covers fretting wear in mechanical components, various parameters that affect fretting; quantification of wear induced by fretting...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0001812
EISBN: 978-1-62708-180-1
... Abstract This article discusses different types of mechanical fasteners, including threaded fasteners, rivets, blind fasteners, pin fasteners, special-purpose fasteners, and fasteners used with composite materials. It describes the origins and causes of fastener failures and with illustrative...
Series: ASM Failure Analysis Case Histories
Volume: 3
Publisher: ASM International
Published: 01 December 2019
DOI: 10.31399/asm.fach.v03.c9001756
EISBN: 978-1-62708-241-9
... assembly comprises of a disk, blades, rotor shaft, and stub shaft. The blades are directionally solidified, air-cooled, and are keyed to the disk by fir-tree roots. They are retained in position by locking plates which fit in circumferential grooves in the rear face of the turbine disk. The other modules...
Series: ASM Handbook
Volume: 11A
Publisher: ASM International
Published: 30 August 2021
DOI: 10.31399/asm.hb.v11A.a0006805
EISBN: 978-1-62708-329-4
... Abstract This article first provides an overview of the types of mechanical fasteners. This is followed by sections providing information on fastener quality and counterfeit fasteners, as well as fastener loads. Then, the article discusses common causes of fastener failures, namely...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003500
EISBN: 978-1-62708-180-1
... shoulders as assembled. Example 2: Sprocket Locking Device Failure ( Ref 33 ). A design deficiency involving improper materials selection was revealed through the analysis of a failed tapered-ring sprocket locking device. The device is used to attach a chain sprocket to a shaft without the use...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.mech.c9001485
EISBN: 978-1-62708-225-9
... or pitting (fatigue) Cracks or fractures Creep Smearing Wear Softening Indentation Fluting Corrosion General If it is desired to carry out a detailed examination of a defective bearing, it is essential that, when it is removed from a shaft or a housing or is dismantled...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0001810
EISBN: 978-1-62708-180-1
... mechanisms fabrication practices fretting corrosion hardness heat treatment lubrication plastic flow rolling-contact fatigue rolling-element bearings failures ROLLING-ELEMENT BEARINGS use rolling elements (either balls or rollers) interposed between two raceways, and relative motion is permitted...
Series: ASM Handbook
Volume: 11
Publisher: ASM International
Published: 15 January 2021
DOI: 10.31399/asm.hb.v11.a0006753
EISBN: 978-1-62708-295-2
.... The device is used to attach a chain sprocket to a shaft without the use of a locking key, enabling the shaft to either drive or be driven anywhere on the shaft ( Fig. 8 ). The configuration consists of an assembly of four tapered rings ( Fig. 9 ) that are retained by a series of cap screws. As shown in Fig...