1-9 of 9 Search Results for

self-powered sensors

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Series: ASM Handbook
Volume: 11B
Publisher: ASM International
Published: 15 May 2022
DOI: 10.31399/asm.hb.v11B.a0006914
EISBN: 978-1-62708-395-9
...Flash-ignition and self-ignition temperatures for selected polymers from ASTM D1929 Table 1 Flash-ignition and self-ignition temperatures for selected polymers from ASTM D1929 Polymer Flash-ignition Self-ignition °C °F °C °F Polyethylene (PE) 341–357 646–674 349 660...
Series: ASM Handbook
Volume: 11
Publisher: ASM International
Published: 15 January 2021
DOI: 10.31399/asm.hb.v11.a0006829
EISBN: 978-1-62708-295-2
... fretting fatigue (i.e., crack nucleation and crack propagation) ( Ref 10 , 15 – 18 ). Fortunately, new surface treatments combining shot and laser peening with a thick self-lubricant plasma coating are now applied to prevent any critical damage process ( Ref 17 ). Fig. 3 Fretting wear damage...
Series: ASM Handbook
Volume: 11B
Publisher: ASM International
Published: 15 May 2022
DOI: 10.31399/asm.hb.v11B.a0006923
EISBN: 978-1-62708-395-9
... (0.264 ksi), °C (°F) 150 (298) 130 (266) 130–135 (266–275) Flammability rating … … 94V-0 Burning rate Self-extinguishing Self-extinguishing Self-extinguishing Specific heat (f) , kJ/kg · K (Btu/lb · °F) … … 1.68 (0.40) Coefficient of thermal expansion (f) , 10 –6 /K (in./in./°F...
Series: ASM Handbook
Volume: 11B
Publisher: ASM International
Published: 15 May 2022
DOI: 10.31399/asm.hb.v11B.9781627083959
EISBN: 978-1-62708-395-9
Series: ASM Handbook
Volume: 11
Publisher: ASM International
Published: 15 January 2021
DOI: 10.31399/asm.hb.v11.a0006753
EISBN: 978-1-62708-295-2
... are well documented. For example, the importance of investigating failures was vividly illustrated in the pioneering efforts of the Wright Brothers in developing self-propelled flight. In fact, while Wilbur was traveling in France in 1908, Orville was conducting flight tests for the U.S. Army Signal Corps...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003500
EISBN: 978-1-62708-180-1
..., the importance of investigating failures is vividly illustrated in the pioneering efforts of the Wright Brothers in developing self-propelled flight. In fact, while Wilbur was traveling in France in 1908, Orville was conducting flight tests for the U.S. Army Signal Corps and was injured when his Wright Flyer...
Series: ASM Handbook
Volume: 11
Publisher: ASM International
Published: 15 January 2021
DOI: 10.31399/asm.hb.v11.a0006791
EISBN: 978-1-62708-295-2
Series: ASM Handbook
Volume: 11B
Publisher: ASM International
Published: 15 May 2022
DOI: 10.31399/asm.hb.v11B.a0006928
EISBN: 978-1-62708-395-9
... of the mechanical energy being converted into heat within the material. Sometimes termed autogenic heating or self-heating, this gradual buildup of heat is sufficient to cause a loss in strength and rigidity and consequently affect the apparent fatigue life determined. This effect is further aggravated by the low...
Series: ASM Handbook
Volume: 11B
Publisher: ASM International
Published: 15 May 2022
DOI: 10.31399/asm.hb.v11B.a0006939
EISBN: 978-1-62708-395-9
... of braking zones; limited growth of only some colonies almost completely stopped(d) Limited efficiency 0 0 Average No braking zone; height reduced to half compared to control(e) 0 0 Powerful Lack of braking zones; absence of a reduction in growth compared to the control, or only a slight...