EISBN: 978-1-62708-395-9
... to gain an understanding of the nature of the cracking. In a way, it is a roadmap to understanding the failure. Much of the information regarding the failure mechanism can be obtained by interpreting the features found on the fracture surface. The fracture-surface characteristics are created based...