Published: 15 May 2022
DOI: 10.31399/asm.hb.v11B.a0006849
EISBN: 978-1-62708-395-9
... Abstract This article addresses some established protocols for characterizing thermoplastics and whether they are homogeneous resins, alloyed, or blended compositions or highly modified thermoplastic composites. It begins with a discussion on characterizing mechanical, rheological, and thermal...
Series: ASM Handbook
Volume: 11B
Publisher: ASM International
Published: 15 May 2022
DOI: 10.31399/asm.hb.v11B.a0006924
EISBN: 978-1-62708-395-9
... Abstract This article discusses the most common thermal analysis methods for thermosetting resins. These include differential scanning calorimetry, thermomechanical analysis, thermogravimetric analysis, and dynamic mechanical analysis. The article also discusses the characterization of uncured...
Image
Published: 15 May 2022
Fig. 15 Structure of unsaturated polyester resins. (a) Phthalate esters, (b) Bisphenol A/fumarate resins More
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.design.c0090436
EISBN: 978-1-62708-233-4
... Abstract Molded plastic couplings used in an industrial application exhibited abnormally brittle properties, as compared to previously produced components. The couplings were specified to be molded from a custom-compounded glass-filled nylon 6/12 resin. An inspection of the molding resin used...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.homegoods.c0090448
EISBN: 978-1-62708-222-8
... Abstract Housings (being tested as part of a material conversion) from an electrical appliance failed during an engineering evaluation. They had been injection molded from a commercial polycarbonate/PET blend. Parts produced from the previous material, a nylon 6/6 resin, had consistently passed...
Series: ASM Failure Analysis Case Histories
Volume: 3
Publisher: ASM International
Published: 01 December 2019
DOI: 10.31399/asm.fach.v03.c9001798
EISBN: 978-1-62708-241-9
... Abstract The crosslinked epoxy resin encapsulant protecting an electromagnetic valve coil failed during long-term storage and was examined to determine the cause. The investigation included fault-tree analysis, FTIR and EDX spectroscopy, and differential scanning calorimetry...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.chem.c0090439
EISBN: 978-1-62708-220-4
...) resin plasticized with trioctyl trimellitate. Investigation included visual inspection, micro-FTIR in the ATR mode, and thermogravimetric analysis. The spectrum on the failed tubing exhibited absorption bands indicative of a PVC resin containing an adipate-based plasticizer. Thermograms of the failed...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.chem.c0090454
EISBN: 978-1-62708-220-4
... Abstract A chemical storage vessel failed while in service. The failure occurred as cracking through the vessel wall, resulting in leakage of the fluid. The tank had been molded from a high-density polyethylene (HDPE) resin. The material held within the vessel was an aromatic hydrocarbon-based...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.homegoods.c0090430
EISBN: 978-1-62708-222-8
... Abstract The handle from a consumer product exhibited an apparent surface defect. The handle had been injection molded from a medium viscosity grade ABS resin. The anomalous appearance was objectionable to the assembler of the final product and resulted in a production lot being placed...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.auto.c0090433
EISBN: 978-1-62708-218-1
... representing an older lot, which exhibited satisfactory performance properties, were also available for reference purposes. The clips were specified to be injection molded from an impact-modified grade of nylon 6/6. However, the part drawing did not indicate a specific resin. Investigation included visual...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.homegoods.c0090445
EISBN: 978-1-62708-222-8
... had been injection molded from an ABS resin to which regrind was routinely added. Inspection of both the failed covers and retained parts, which exhibited normal behavior during assembly, included visual inspection, micro-FTIR in the ATR mode, and analysis using DSC. The FTIR results indicated...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.auto.c0090451
EISBN: 978-1-62708-218-1
... Abstract Cracking occurred within the plastic jacket (injection molded from an impact-modified, 15% glass-fiber-reinforced PET resin.) of several assemblies used in a transportation application during an engineering testing regimen which involved cyclic thermal shock (exposing the parts...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.homegoods.c0090427
EISBN: 978-1-62708-222-8
... Abstract A set of plastic grips from an electric consumer product failed while in service. The grips had been injection molded from a general-purpose grade of ABS resin. The parts had cracked while in use after apparent embrittlement of the material. Investigation (visual inspection, SEM...
Image
Published: 01 June 2019
Fig. 1 The DSC thermogram representing a molding resin pellet that had produced brittle parts. The thermogram shows a major melting transition associated with nylon 6/12 and a weaker transition attributed to polypropylene. More
Image
Published: 01 June 2019
Fig. 2 The DSC thermogram representing a second molding resin pellet that had produced brittle parts. The thermogram shows a major melting transition associated with nylon 6/12 and a weaker transition attributed to nylon 6/6. More
Image
Published: 01 June 2019
Fig. 3 Resin anomaly in the fiber tow of an exterior ply. (MAG 80×) More
Image
Published: 01 June 2019
Fig. 4 FTIR analysis of resin extracted from the exterior ply (top curve) and from the interior ply (bottom curve). More
Image
Published: 01 June 2019
Fig. 5 Higher magnification of the resin anomaly (long, black arrow) in the tow of an exterior ply. Short, black arrow indicates cracking in the coating materials. (MAG 200×) More
Image
Published: 01 June 2019
Fig. 6 SEM photomicrograph of suspected resin anomaly within the fiber tows in an exterior ply. More
Image
Published: 01 June 2019
Fig. 7 Microcracking (arrows) in the resin rich regions of the component. (MAG 50×) More