Published: 15 May 2022
Fig. 17 Schematic representation of a pultrusion process More
Image
Published: 15 May 2022
Fig. 30 Master cure curve for polyurethane pultrusion resin system. The solid line is calculated from the second-order kinetic equation found to fit the master curve. Source: Ref 10 More
Image
Published: 15 May 2022
Fig. 31 Time-temperature profile for pultrusion process and development of conversion along the profile. Source: Ref 10 More
Series: ASM Handbook
Volume: 11B
Publisher: ASM International
Published: 15 May 2022
DOI: 10.31399/asm.hb.v11B.a0006935
EISBN: 978-1-62708-395-9
... for such processes as resin transfer molding and pultrusion, in which the resin must flow through preplaced glass reinforcements. For other processes, such as extra-high-strength molding compound and prepreg compression molding, the resin must be thickened by reaction to stay on the glass reinforcements. With sheet...
Series: ASM Handbook
Volume: 11B
Publisher: ASM International
Published: 15 May 2022
DOI: 10.31399/asm.hb.v11B.a0006864
EISBN: 978-1-62708-395-9
...-resistant layers to the surfaces exposed to wear Introduce wear-causing fillers downstream during extrusion Secondary feed port after the melting zone Increase length of the compression section Reduce compression ratio Reduce screw speed Special Extrusion Processes Pultrusion...
Series: ASM Handbook
Volume: 11B
Publisher: ASM International
Published: 15 May 2022
DOI: 10.31399/asm.hb.v11B.a0006924
EISBN: 978-1-62708-395-9
Series: ASM Handbook
Volume: 11B
Publisher: ASM International
Published: 15 May 2022
DOI: 10.31399/asm.hb.v11B.a0006932
EISBN: 978-1-62708-395-9
..., pultrusion, and calendering. The anisotropy of physical properties that accompanies orientation must be considered. Of paramount concern are the dimensional instabilities that arise from anisotropic CTEs. Physical aging, which is also examined, is the process by which plastics cooled below the T g...
Series: ASM Handbook
Volume: 11B
Publisher: ASM International
Published: 15 May 2022
DOI: 10.31399/asm.hb.v11B.9781627083959
EISBN: 978-1-62708-395-9
Series: ASM Handbook
Volume: 11B
Publisher: ASM International
Published: 15 May 2022
DOI: 10.31399/asm.hb.v11B.a0006925