...Abstract Abstract A return bend (made from ASTM A213, grade T11, ferritic steel) from a triolefin-unit heater ruptured after two years in service. The unit operated at 2410 kPa, with a hydrocarbon feed stream (85% propylene) entering at 260 to 290 deg C and leaving at 425 to 480 deg C...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0001818
EISBN: 978-1-62708-180-1
..., ferritic steel. The unit operated at 2410 kPa (350 psi), with a hydrocarbon feed stream (85% propylene) entering at 260 to 290 °C (500 to 550 °F) and leaving at 425 to 480 °C (800 to 900 °F). The temperature of the combustion gas was 900 °C (1650 °F). Fig. 3 Return bend made of ASTM A213, grade T11...