Series: ASM Handbook
Volume: 11A
Publisher: ASM International
Published: 30 August 2021
DOI: 10.31399/asm.hb.v11A.a0006817
EISBN: 978-1-62708-329-4
... the failure. In the vocabulary of RCM, those investigators are looking at deeper levels of causation. Various RCM processes may have different methods of identifying the appropriate level of causation, with each method promising to do so more efficiently and more effectively than the others, but SAE...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003504
EISBN: 978-1-62708-180-1
.... Various RCM processes may have different methods of identifying the appropriate level of causation, with each method promising to do so more efficiently and more effectively than the others, but SAE JA1011-compliant processes will all be looking for the level of causation at which the most appropriate...
Series: ASM Failure Analysis Case Histories
Volume: 3
Publisher: ASM International
Published: 01 December 2019
DOI: 10.31399/asm.fach.v03.c9001832
EISBN: 978-1-62708-241-9
... the processing of nuclear materials are kept in large underground storage tanks made of low-carbon steel. The wastes consist primarily of concentrated solutions of sodium nitrate and sodium hydroxide. Each of the tanks is equipped with a purge ventilation system designed to continuously remove hydrogen gas...
Series: ASM Handbook
Volume: 11
Publisher: ASM International
Published: 15 January 2021
DOI: 10.31399/asm.hb.v11.a0006791
EISBN: 978-1-62708-295-2
... Abstract Friction and wear are important when considering the operation and efficiency of components and mechanical systems. Among the different types and mechanisms of wear, adhesive wear is very serious. Adhesion results in a high coefficient of friction as well as in serious damage...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.process.c9001258
EISBN: 978-1-62708-235-8
... Abstract A drawing plant which processed steel wire of designation 105 Cr 2 for ball bearings had losses due to crack formation and wire breakage during drawing. To establish the reason for the breakage, seven fractures were submitted for investigation with contiguous wire segments on both...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003567
EISBN: 978-1-62708-180-1
... of energy consumed annually by U.S. industry for crushing and grinding purposes, whereas contributions from minerals account for 50%; cement, 25%; coal, 13%; and agricultural products, 12% ( Ref 5 ). The development of more efficient mining, transportation, and processing systems has allowed exploitation...
Series: ASM Failure Analysis Case Histories
Volume: 3
Publisher: ASM International
Published: 01 December 2019
DOI: 10.31399/asm.fach.v03.c9001788
EISBN: 978-1-62708-241-9
... the final extrusion section may need more finishing operations or may not be accurate in final dimensions. The current investigation has shown that finite element simulation of extrusion process integrated with fatigue theory yield an efficient tool for the identification of critical process parameters...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.modes.c9001628
EISBN: 978-1-62708-234-1
... Abstract A nickel alloy cylinder plated with chromium along its inner liner, installed in a commercial ice cream freezer, showed gray discoloration along its OD surface. The discolored parts exhibited significantly reduced cooling efficiency as compared with new cylinders. During operation...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.modes.c0046378
EISBN: 978-1-62708-234-1
... Sleeves Hardfaced stainless steel Corrosive wear Abrasive wear Whenever river water is used in a manufacturing process, the presence of abrasive silt in the water can be expected to result in wear problems. A typical wear problem was encountered in a brine plant when river water was pumped...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003514
EISBN: 978-1-62708-180-1
... components to design for appropriate levels of safety. Computational resources are becoming less of an impediment through enhancements in computational algorithms and computer efficiency. Factor of safety approaches may not give the desired reliability or may lead to overdesigned structures...
Series: ASM Handbook
Volume: 11A
Publisher: ASM International
Published: 30 August 2021
DOI: 10.31399/asm.hb.v11A.a0006800
EISBN: 978-1-62708-329-4
... in design and processing was required. However, with the heightened awareness of efficient design, optimized performance, economic competition, environmental impacts, safety concerns, and legal liability, current methods of materials selection are viewed more and more as a simultaneous and integral part...
Series: ASM Handbook
Volume: 11A
Publisher: ASM International
Published: 30 August 2021
DOI: 10.31399/asm.hb.v11A.a0006809
EISBN: 978-1-62708-329-4
... Abstract A detailed fracture mechanics evaluation is the most accurate and reliable prediction of process equipment susceptibility to brittle fracture. This article provides an overview and discussion on brittle fracture. The discussion covers the reasons to evaluate brittle fracture, provides...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.steel.c9001714
EISBN: 978-1-62708-232-7
... ratio. Metallographic investigations revealed that the surface of the attacked pipes consisted of (Cr, Fe) carbide. The metal dusting was the result of a decomposition process (CO to CO2 + C) that deposited C on the pipe surface. Because of the high temperature, the C subsequently diffused through...
Series: ASM Handbook
Volume: 11A
Publisher: ASM International
Published: 30 August 2021
DOI: 10.31399/asm.hb.v11A.a0006838
EISBN: 978-1-62708-329-4
... in the range of 400 to 1200 °C (750 to 2190 °F). The advantages of EBM, including the ability to produce complex shapes, the efficient use of materials, and the fast processing cycle, make it a good alternative for manufacturing titanium products. Electron beam PBF is an excellent choice for high-reflectivity...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003503
EISBN: 978-1-62708-180-1
... Careful planning for the FMEA tailors the scope of the analysis to the needs of the program and provides a process that efficiently identifies design deficiencies so that corrective actions or compensating provisions can be made in a timely manner. Proper planning requires that the system requirements...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003501
EISBN: 978-1-62708-180-1
... and processing was required. However, with the heightened awareness of efficient design, optimized performance, economic competition, environmental impacts, safety concerns, and legal liability, current methods of materials selection are viewed more and more as a simultaneous and integral procedure of the entire...
Series: ASM Handbook
Volume: 11A
Publisher: ASM International
Published: 30 August 2021
DOI: 10.31399/asm.hb.v11A.a0006815
EISBN: 978-1-62708-329-4
... Abstract The intent of this article is to assist the failure analyst in understanding the underlying engineering design process embodied in a failed component or system. It begins with a description of the mode of failure. This is followed by a section providing information on the root cause...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.pulp.c0090276
EISBN: 978-1-62708-230-3
... is placed on the rotating face of the dryer, which is located toward the back end of a crepe papermaking machine. As the dryer rotates, contact with the high-temperature face removes considerable moisture from the paper by the time it is removed from the dryer. The drying process only occurs while the paper...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.machtools.c0091853
EISBN: 978-1-62708-223-5
.... The process continued until approximately 4.5 kg (10 lb) of the 75 μm product was deposited in the collection tray. The product was removed from the collection tray and the process repeated. Eventually, the machine failed due to grinding plate wear. Fig. 2 Macrographs of new (left) and worn (right...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003519
EISBN: 978-1-62708-180-1
... is that time spent in preparation and planning can save a lot of time and money and even help achieve a successful conclusion of the failure investigation. What Is a Failure? A good definition of a failure is “the inability of a component, machine, or process to function properly.” Failures come in all...