1-14 of 14 Search Results for

probabilistic analysis

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003514
EISBN: 978-1-62708-180-1
...Abstract Abstract This article describes the historical background, uncertainties in structural parameters, classifications, and application areas of probabilistic analysis. It provides a discussion on the basic definition of random variables, some common distribution functions used...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.aero.c0090030
EISBN: 978-1-62708-217-4
... (Design Assessment of Reliability With INspection), has been developed under FAA funding that is specifically tailored to perform a probabilistic analysis of titanium rotors subject to HA ( Ref 6 ). DARWIN integrates finite-element stress analysis, fracture mechanics analysis, nondestructive inspection...
Series: ASM Handbook
Volume: 11
Publisher: ASM International
Published: 15 January 2021
DOI: 10.31399/asm.hb.v11.a0006767
EISBN: 978-1-62708-295-2
... elastic fracture mechanics analysis, with some mention of elastic-plastic fracture mechanics analysis. The article describes the probabilistic aspects of fatigue and fracture. Information on crack-growth simulation of the material is also provided. crack-growth simulation elastic-plastic fracture...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003512
EISBN: 978-1-62708-180-1
... provides information on fatigue life assessment, elevated-temperature life assessment, and fitness-for-service life assessment. elevated-temperature life assessment fabrication failure analysis fatigue life assessment fitness-for-service life assessment material defects nondestructive...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003515
EISBN: 978-1-62708-180-1
... of false alarm (PFA). The article describes the damage tolerance approach to life management of cyclic-limited engine components and lists the commonly used nondestructive evaluation methods. It concludes with an illustration on the role of NDE, as quantified by POD, in fully probabilistic life management...
Series: ASM Failure Analysis Case Histories
Volume: 1
Publisher: ASM International
Published: 01 December 1992
DOI: 10.31399/asm.fach.v01.c9001081
EISBN: 978-1-62708-214-3
... under estimated, which led to low-cycle fatigue cracking earlier than expected. Fracture mechanics analysis of the disks was carried out to assess their damage tolerance and to predict safe inspection intervals. Fatigue life Fracture mechanics Gas turbine engines Jet planes Low-cycle fatigue...
Series: ASM Handbook
Volume: 11
Publisher: ASM International
Published: 15 January 2021
DOI: 10.31399/asm.hb.v11.a0006764
EISBN: 978-1-62708-295-2
... spot/line technology Surface temperatures are imaged by point sensors, IR cameras, or coatings that change appearance with temperature. Analysis is based on absolute and change of temperature following a stimulus. Locating near-surface discontinuities that alter heat transfer through object Requires...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003505
EISBN: 978-1-62708-180-1
... of failure analysis to be included in this Volume. This article is not intended to provide legal conclusions, and the opinions are those of the author. Because every situation is different, this article should not be applied to any specific product without additional analysis. It is written from...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003545
EISBN: 978-1-62708-180-1
... of component-operating conditions with available data on creep, stress-rupture, tension, elevated-temperature fatigue, and thermal fatigue properties. Such an analysis is usually sufficient for most failure investigations, but a more thorough analysis may be required when stress, time, temperature...
Series: ASM Handbook
Volume: 11
Publisher: ASM International
Published: 15 January 2021
DOI: 10.31399/asm.hb.v11.a0006780
EISBN: 978-1-62708-295-2
.... A , Vol 84 , 1910 , p 1 – 12 10.1098/rspa.1910.0050 4. Ezrin M. , Plastics Failure Guide: Cause and Prevention , Hanser Publishers , 1996 5. Scheirs J. , Compositional and Failure Analysis of Polymers: A Practical Approach , Wiley , 2000 6. Hertzberg R.W...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003516
EISBN: 978-1-62708-180-1
... 10. Mitchell M.R. , Fundamentals of Modern Fatigue Analysis for Design , Fatigue and Fracture , Vol 19 , ASM Handbook , ASM International , 1996 , p 242 11. Irwin G.R. , Handbuch der Physik , Vol 6 , p 551 – 590 12. Broek D. , Elementary Engineering Fracture...
Series: ASM Handbook
Volume: 11
Publisher: ASM International
Published: 15 January 2021
DOI: 10.31399/asm.hb.v11.a0006775
EISBN: 978-1-62708-295-2
... compression, bending, torsion). Finally, the factors influencing the appearance of a fracture surface and various imperfections or stress raisers are described, followed by a root-cause failure analysis case history to illustrate some of these fractography concepts. brittle fracture crack nucleation...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003538
EISBN: 978-1-62708-180-1
... geometric factors and materials aspects that influence the stress-strain behavior and fracture of ductile metals. It highlights fractures arising from manufacturing imperfections and stress raisers. The article presents a root cause failure analysis case history to illustrate some of the fractography...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003503
EISBN: 978-1-62708-180-1
...FMEA analysis of the stop valve for a hot water heater Table 1 FMEA analysis of the stop valve for a hot water heater Failure mode Effect Local System 1. Fails closed Burner off No hot water 2. Fails open Burner will not shut off Overheats, release valve releases pressure...