Series: ASM Handbook
Volume: 11B
Publisher: ASM International
Published: 15 May 2022
DOI: 10.31399/asm.hb.v11B.a0006932
EISBN: 978-1-62708-395-9
... ), 1971 , p 4622 10.1063/1.1659831 61. Li J.C.M. and Wu J.B.C. , Pressure and Normal Stress Effects in Shear Yielding , J. Mater. Sci. , Vol 11 , 1976 , p 445 10.1007/BF00540925 62. Li J.C.M. , Behavior and Properties of Shear Bands , Polym. Eng. Sci. , Vol 24...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003508
EISBN: 978-1-62708-180-1
... Abstract This article focuses on the general root causes of failure attributed to the casting process, casting material, and design with examples. The casting processes discussed include gravity die casting, pressure die casting, semisolid casting, squeeze casting, and centrifugal casting. Cast...
Series: ASM Handbook
Volume: 11
Publisher: ASM International
Published: 15 January 2021
DOI: 10.31399/asm.hb.v11.a0006787
EISBN: 978-1-62708-295-2
... changes in the alloy mechanical properties and thus possible alloy embrittlement. Variables that affect the carburization rate are temperature, exposure time, alloy composition, and partial pressures of H 2 , CH 4 , and H 2 S. Hydrogen sulfide tends to slow alloy decarburization rates. Carbon dioxide...
Series: ASM Handbook
Volume: 11A
Publisher: ASM International
Published: 30 August 2021
DOI: 10.31399/asm.hb.v11A.a0006831
EISBN: 978-1-62708-329-4
... that of the dimensions of the sand grains Rough casting surface D 122 Depth of surface roughness is greater than that of the sand grain dimensions Severe roughness, high pressure molding defect D 130 Grooves on the casting surface D 131 Grooves of various lengths, often branched, with smooth...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003543
EISBN: 978-1-62708-180-1
Series: ASM Handbook
Volume: 11
Publisher: ASM International
Published: 15 January 2021
DOI: 10.31399/asm.hb.v11.a0006778
EISBN: 978-1-62708-295-2
Series: ASM Handbook
Volume: 11B
Publisher: ASM International
Published: 15 May 2022
DOI: 10.31399/asm.hb.v11B.a0006940
EISBN: 978-1-62708-395-9
... structure includes lamellar crystals in an entangled network of amorphous polymer chains that are held together by tie molecules. The lamellae thickness (usually between 3 and 20 nm) is affected by interfacial energies, glass transition temperature and melting temperature, undercooling, and segmental...
Series: ASM Handbook
Volume: 11A
Publisher: ASM International
Published: 30 August 2021
DOI: 10.31399/asm.hb.v11A.9781627083294
EISBN: 978-1-62708-329-4