Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.aero.c9001517
EISBN: 978-1-62708-217-4
... patterns, were evident in these areas. Fractographs of these anomalous areas were then compared to previous fractographic data obtained on epoxy composite specimens. The fracture characteristics on humidity aged epoxy specimens and on epoxy specimens in which the prepreg had been exposed to humidity prior...