1-20 of 136 Search Results for

precipitation hardenability

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Image
Published: 15 January 2021
Fig. 7 Precipitate in a precipitation-hardened (PH) steel fracture surface, labeled as Spectrum 1, and energy-dispersive spectroscopy spectrum from the corresponding point showing nearby steel constituents (iron, chromium, nickel, and copper) that are detected. According to the quantitative More
Image
Published: 15 January 2021
Fig. 6 Scanning electron microscope image of 15-5 precipitation-hardened (PH) steel debris with gold plating that had transferred onto the metal surface during the failure event. In secondary electron imaging, topographical differences in the gold plating such as wrinkling are more evident More
Series: ASM Failure Analysis Case Histories
Volume: 2
Publisher: ASM International
Published: 01 December 1993
DOI: 10.31399/asm.fach.v02.c9001361
EISBN: 978-1-62708-215-0
...) Macrograph of the sectioned failed rod-end body. The cracks in the swaged ring should be attributed to both the high inclusion content in the material and the abnormal loads shown in (a). Pertinent Specifications The rod end body was manufactured of 17-4PH steel hardened to 36 to 38 HRc, whereas...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.process.c9001520
EISBN: 978-1-62708-235-8
... test. Both part types were made of 15-5 PH (UNS S15500) precipitation hardening stainless steel. Hydrogen embrittlement cracking was the likely cause of failure for both part types. Cracking of the as-fabricated parts was ultimately prevented by changing the manufacturing procedure to allow...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.aero.c9001707
EISBN: 978-1-62708-217-4
... Abstract The failures of two aircraft components, one from a landing gear and the other from an ejector rack mechanism, were investigated. Both were made from PH 13-8 Mo (UNS S13800) precipitation-hardening stainless steel which had been heat treated to the H1000 and H950 tempers respectively...
Series: ASM Failure Analysis Case Histories
Volume: 2
Publisher: ASM International
Published: 01 December 1993
DOI: 10.31399/asm.fach.v02.c9001294
EISBN: 978-1-62708-215-0
... Abstract A precipitation-hardened stainless steel poppet valve assembly used to shut off the flow of hydrazine fuel to an auxiliary power unit was found to leak. SEM and optical micrographs revealed that the final heat treatment designed for the AM-350 bellows material rendered the AM-355...
Series: ASM Failure Analysis Case Histories
Volume: 1
Publisher: ASM International
Published: 01 December 1992
DOI: 10.31399/asm.fach.v01.c9001081
EISBN: 978-1-62708-214-3
... Abstract Several compressor disks in military fighter and trainer aircraft gas turbine engines cracked prematurely in the bolt hole regions. The disks were made of precipitation-hardened AM355 martensitic stainless steel. Experimental and analytical work was performed on specimens from...
Series: ASM Failure Analysis Case Histories
Volume: 2
Publisher: ASM International
Published: 01 December 1993
DOI: 10.31399/asm.fach.v02.c9001357
EISBN: 978-1-62708-215-0
... Abstract Two 20 MW turbines suffered damage to second-stage blades prematurely. The alloy was determined to be a precipitation-hardening nickel-base superalloy comparable to Udimet 500, Udimet 710, or Rene 77. Typical protective coatings were not found. Test results further showed that the fuel...
Image
Published: 15 January 2021
Fig. 21 (a) Correlation of particle spacing with dimple size. Data are from several aluminum alloys. Ellipse size indicates scatter. Source: Ref 45 . (b) Change in dimple size and onset of intergranular cracking as a function of aging time for a precipitation-hardened titanium alloy (B-1208CA More
Image
Published: 01 January 2002
Fig. 21 (a) The correlation of particle spacing with dimple size. Data are from several aluminum alloys, as indicated. Ellipse size indicates scatter. Source: Ref 44 . (b) Change in dimple size and onset of intergranular cracking as a function of aging time for a precipitation-hardened More
Image
Published: 01 January 2002
Fig. 7 Comparison of light microscope (top row) and scanning electron microscope (bottom row) fractographs showing the intergranular fracture appearance of an experimental nickel-base precipitation-hardenable alloy rising-load test specimen that was tested in pure water at 95 °C (200 °F). All More
Series: ASM Failure Analysis Case Histories
Volume: 1
Publisher: ASM International
Published: 01 December 1992
DOI: 10.31399/asm.fach.v01.c9001031
EISBN: 978-1-62708-214-3
... as a precipitation hardener, and zirconium acts as a getter for soluble oxygen. The NARloy-Z goes through a fabrication process that includes casting, forging, and heat treatment. Chemical analysis is performed at various stages in the fabrication process to ensure that impurity levels are minimal. Cooling channels...
Series: ASM Handbook
Volume: 11
Publisher: ASM International
Published: 15 January 2021
DOI: 10.31399/asm.hb.v11.a0006777
EISBN: 978-1-62708-295-2
...) Improperly precipitation-hardened alloys, resulting in coarse grain-boundary precipitates and a denuded region (precipitation-free zone) Embrittlement of molybdenum by interstitials (carbon, nitrogen, oxygen) Embrittlement of copper by antimony Reduction of Cu 2 O in tough pitch copper by hydrogen...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003540
EISBN: 978-1-62708-180-1
... Cu alloy with (a) IG facets at low magnification (10×) and (b) uniform dimples on one facet at higher magnification Dimpled IG fracture is also observed in other precipitation-hardening alloys (such Al-Mg-Zn alloys) with large precipitates on grain boundaries and wide precipitation-free zones...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.design.c0047109
EISBN: 978-1-62708-233-4
... stem was compared with that of a new part. There was no significant difference between microstructures in the new and in the used stems. The microstructures were found to be typical of a martensitic precipitation-hardening stainless steel in the H900 condition. Because of the small size...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.power.c0046966
EISBN: 978-1-62708-229-7
... to age hardening, subsurface oxidation related to intragranular carbides, and high residual tensile macrostresses. No further conclusions could be drawn because of the lack of detailed service history, and no recommendations were made. Airfoils Carbides Precipitation Turbines Vanes AMS 5382...
Series: ASM Failure Analysis Case Histories
Volume: 1
Publisher: ASM International
Published: 01 December 1992
DOI: 10.31399/asm.fach.v01.c9001025
EISBN: 978-1-62708-214-3
..., a precipitation-hardened aluminum alloy containing 4.4% Cu, 0.8% Si, 0.8% Mn, and 0.4% Mg. Tensile property specifications for this material are as follows: ultimate tensile strength, 480 MPa (70 ksi); yield strength, 410 MPa (60 ksi); and elongation, 10%. Wheels are required to be inspected during each tire...
Series: ASM Handbook
Volume: 11
Publisher: ASM International
Published: 15 January 2021
DOI: 10.31399/asm.hb.v11.a0006759
EISBN: 978-1-62708-295-2
... the interaction volume of the electrons, and the lower the voltage, the more surface features are being analyzed, as shown in Fig. 6 . Fig. 6 Scanning electron microscope image of 15-5 precipitation-hardened (PH) steel debris with gold plating that had transferred onto the metal surface during the failure...
Series: ASM Handbook
Volume: 11
Publisher: ASM International
Published: 15 January 2021
DOI: 10.31399/asm.hb.v11.a0006778
EISBN: 978-1-62708-295-2
... • Multiple intergranular cracks • Voids formed on grain boundaries or wedge-shaped cracks at grain triple points • Reaction scales or internal precipitation • Some cold flow in last stages of failure Contributing factors • Load exceeded the strength of the part • Check for proper alloy and processing...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.process.c9001207
EISBN: 978-1-62708-235-8
... examination showed welding conditions were such that a carburizing atmosphere developed, which led to an increase in carbon content and hardening at certain locations such as terminal bells and lap joints. This explained the processing difficulties during the threading operation. Hardening Pipe Weld...