Series: ASM Handbook
Volume: 11B
Publisher: ASM International
Published: 15 May 2022
DOI: 10.31399/asm.hb.v11B.a0006850
EISBN: 978-1-62708-395-9
... as a tribological material and failure examples, explaining wear resistance of polyurethane elastomeric coatings and failure of an acetal gear wheel. References References 1. Briscoe B.J. and Sinha S.K. , “ Wear of Polymers ,” Proc. Inst. Mech. Eng. J., J. Eng. Tribol. , Vol 216 , 2002...
Series: ASM Handbook
Volume: 11B
Publisher: ASM International
Published: 15 May 2022
DOI: 10.31399/asm.hb.v11B.a0006866
EISBN: 978-1-62708-395-9
...‑monooxygenase (AHs), styrene monooxygenase (StyA), NADH-dependent flavin reductase (StyB), styrene-oxide isomerase (StyC), phenylacetaldehyde dehydrogenase (StyD) Polyurethane, PUR 27 × 10 6 Hydrolases (polyurethanases) Hydrolases (Alkyl carbamate hydrolase) Polyethylene terephthalate, PET 33 × 10 6...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.modes.c9001696
EISBN: 978-1-62708-234-1
..., and is similar to the tubing used in LC-39B's GO 2 System and B/A Line. The tubing was specified to be coated with either a nitrile-rubber-base, aluminum pigmented coating or a polyamide epoxy coating with an aliphatic polyurethane topcoat. The coatings are required for corrosion protection of 300-series...
Series: ASM Handbook
Volume: 11B
Publisher: ASM International
Published: 15 May 2022
DOI: 10.31399/asm.hb.v11B.a0006920
EISBN: 978-1-62708-395-9
.... Gardette J.-L. et al. , in Service Life Prediction: Challenging the Status Quo , Martin J.W. , Ryntz R.A. , and Dickie R.A. , Ed., Federation of Societies for Coatings Technology , Philadelphia, PA , 2005 , p 286 6. “ Recommended Reference Solar Spectra for Industrial...
Series: ASM Handbook
Volume: 11B
Publisher: ASM International
Published: 15 May 2022
DOI: 10.31399/asm.hb.v11B.a0006939
EISBN: 978-1-62708-395-9
... (Clariant Plastics and Coatings Ltd.) Low smoke density Nonhalogenated Higher thermal stability Polyurethane rigid foam Polyolefin system Hot-melt adhesive Phosphate ester Resorcinol diphosphate (RDP) Monophosphate bisphenol A diphosphate (BAPP) Not very hydrolytically stable Monophosphate may...
Series: ASM Handbook
Volume: 11B
Publisher: ASM International
Published: 15 May 2022
DOI: 10.31399/asm.hb.v11B.a0006924
EISBN: 978-1-62708-395-9
... curve for polyurethane pultrusion resin system. The solid line is calculated from the second-order kinetic equation found to fit the master curve. Source: Ref 10 Fig. 1 Schematic comparing the processing of (a) thermoplastics and (b) thermosets Fig. 2 Epoxy reaction with primary...
Series: ASM Handbook
Volume: 11B
Publisher: ASM International
Published: 15 May 2022
DOI: 10.31399/asm.hb.v11B.a0006926
EISBN: 978-1-62708-395-9
.... , Wyzogoski M.G. , and Myers M.E. Jr. , Polyurethane Aging in Water and Methanol Environments , The Effects of Hostile Environments on Coatings and Plastics , Garner D.P. & Stahl G.P. , Ed., American Chemical Society Symposium Series , Vol 229 , 1983 , p 173 10.1021/bk-1983...
Series: ASM Handbook
Volume: 11B
Publisher: ASM International
Published: 15 May 2022
DOI: 10.31399/asm.hb.v11B.a0006849
EISBN: 978-1-62708-395-9
... Universal Extensional Rheometer for Polymer Melts , Proc. Society of Rheology , Oct 1978 , Google Scholar 21. “ Recommended Practices for Testing Polymeric Powders and Powder Coatings ,” D 3451-92, Vol 6.02 , Annual Book of ASTM Standards , ASTM International 22. “ Standard Practice...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003570
EISBN: 978-1-62708-180-1
... have confirmed that commercially available powder (e.g., Ni-15.5Cr-4Fe-4Si-3B, in weight percent), plasma sprayed on a variety of substrates and then flame remelted, form adherent, hard, erosion-resistant coatings ( Ref 25 ). Performance in vibratory cavitation of as-sprayed and flame remelted Ni-Cr-Fe...
Series: ASM Handbook
Volume: 11B
Publisher: ASM International
Published: 15 May 2022
DOI: 10.31399/asm.hb.v11B.a0006925
EISBN: 978-1-62708-395-9
... (PS) Polysulfone PTFE Polytetrafluoroethylene PUR Polyurethane (urethane) PVA Polyvinyl acetal PVAC Polyvinyl acetate PVAL (PVA) Polyvinyl alcohol PVB Polyvinyl butyral PVC Polyvinyl chloride PVDC Polyvinylidene chloride PVDF Polyvinylidene fluoride PVF...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003549
EISBN: 978-1-62708-180-1
... in the environment; change in the alloy or heat treatment; change in design; use of galvanic protection; use of inhibitors; use of nonmetallic coatings and liners; application of metallic coatings; use of surface treatments, thermal spray, or other surface modifications; corrosion monitoring; and preventive...
Series: ASM Handbook
Volume: 11B
Publisher: ASM International
Published: 15 May 2022
DOI: 10.31399/asm.hb.v11B.a0006915
EISBN: 978-1-62708-395-9
.... , Electrical Properties of Polymers: Chemical Principles , Hanser Publishers , 1987 , p 181 , 182 29. Strong A.B. , Plastics: Materials and Processing , Prentice-Hall , 1996 , p 144 30. Austin M.J. , Inorganic Anti-Corrosive Pigments , Paint and Coating Testing Manual...
Series: ASM Handbook
Volume: 11B
Publisher: ASM International
Published: 15 May 2022
DOI: 10.31399/asm.hb.v11B.9781627083959
EISBN: 978-1-62708-395-9
Series: ASM Handbook
Volume: 11
Publisher: ASM International
Published: 15 January 2021
DOI: 10.31399/asm.hb.v11.a0006782
EISBN: 978-1-62708-295-2
... been dissolved. Iron is nearly inert in air-free water and seawater, because there is limited cathodic reaction possible. If the surface of the metal is coated with paint or other nonconducting film, the rates of both anodic and cathodic reactions are greatly reduced, and corrosion will be retarded...
Series: ASM Handbook
Volume: 11B
Publisher: ASM International
Published: 15 May 2022
DOI: 10.31399/asm.hb.v11B.a0006871
EISBN: 978-1-62708-395-9
...) >380 Fading 370–385 Increasing ultraviolet sensitivity (extended exposure) Polyacrylate 385 Yellowing Polyamide (aromatic) 360–370, 415 Yellowing Polypropylene 340–380 Creation of carbonyl groups 360–380 Decreasing tensile strength Polyurethane (aromatic) 350–415 Yellowing...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0001812
EISBN: 978-1-62708-180-1
...-corrosion cracking, hydrogen embrittlement, and liquid-metal embrittlement of bolts and nuts. The article explains the most commonly used protective metal coatings for ferrous metal fasteners. Zinc, cadmium, and aluminum are commonly used for such coatings. The article also illustrates the performance...
Series: ASM Handbook
Volume: 11A
Publisher: ASM International
Published: 30 August 2021
DOI: 10.31399/asm.hb.v11A.a0006805
EISBN: 978-1-62708-329-4
... composites Fastener type Fastener material Surface coating Suggested application Epoxy/graphite composite Kevlar (DuPont) Fiberglass Honeycomb Blind rivets (a) 5056 aluminum None Not recommended (b) Excellent (b) Excellent (b) (c) Monel None Good (b...
Series: ASM Handbook
Volume: 11B
Publisher: ASM International
Published: 15 May 2022
DOI: 10.31399/asm.hb.v11B.a0006923
EISBN: 978-1-62708-395-9
... 50–205 120–400 120–150 250–300 0.17–0.22 0.10–0.13 55–100 Polyimide 305–360 580–680 260–315 500–600 0.10–0.34 0.058–0.20 25–80 Polyurethane (cast) 50–205 120–400 90–120 190–250 0.17–0.21 0.10–0.12 70–100 Silicone … … 260 500 0.22 0.13 80–300 Urethane elastomer...
Series: ASM Handbook
Volume: 11B
Publisher: ASM International
Published: 15 May 2022
DOI: 10.31399/asm.hb.v11B.a0006864
EISBN: 978-1-62708-395-9
... land temperature ○ Open die gap wider ○ Reduce extrusion rate ○ Coat die wall with low-friction ceramic finish Process above the upper critical shear rate for melt fracture Use a processing aid (fluoroelastomers are common for polyolefins) Draw resonance Excessive drawdown...
Series: ASM Handbook
Volume: 11B
Publisher: ASM International
Published: 15 May 2022
DOI: 10.31399/asm.hb.v11B.a0006922
EISBN: 978-1-62708-395-9
... polyurethane elastomer TPU Styrene ethene butene styrene SEBS Ethylene propylene diene monomer rubber EPDM Styrene butadiene rubber SBR Acrylonitrile butadiene rubber NBR Silicone rubber SI Isoprene rubber IR Chloroprene rubber CR Thermosets Epoxy EP Melamine ME...