Series: ASM Handbook
Volume: 11B
Publisher: ASM International
Published: 15 May 2022
DOI: 10.31399/asm.hb.v11B.a0006925
EISBN: 978-1-62708-395-9
... Abstract This introductory article describes the various aspects of chemical structure that are important to an understanding of polymer properties and thus their eventual effect on the end-use performance of engineering plastics. The polymers covered include hydrocarbon polymers, carbon-chain...
Series: ASM Handbook
Volume: 11B
Publisher: ASM International
Published: 15 May 2022
DOI: 10.31399/asm.hb.v11B.a0006939
EISBN: 978-1-62708-395-9
... be solved if two polymeric materials are mixed together. Currently, one-third of all plastic materials are made with a blend of two or more polymeric materials ( Ref 73 , 88 , 89 ). However, most of the polymeric alloys are thermodynamically immiscible, because polymer chains naturally have lower...