Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003570
EISBN: 978-1-62708-180-1
... benefits notwithstanding, as-sprayed deposits have not been very successful in resisting liquid impact, owing to the presence of brittle phases or porosity in the deposits or inadequate adhesion between deposits and substrates ( Ref 22 , 23 ). In contrast, Ni-Cr-Si-B alloys, plasma sprayed and then flame...
Series: ASM Handbook
Volume: 11
Publisher: ASM International
Published: 15 January 2021
DOI: 10.31399/asm.hb.v11.a0006787
EISBN: 978-1-62708-295-2
.... , Salinas-Bravo V.M. , Arrieta-Gonzalez C.D. , Ramos-Hernandez J.J. , and Cuevas-Arteaga C. , Electrochemical Performance of Ni20Cr Coatings Applied by Combustion Powder Spray in ZnCl 2 -KCl Molten Salts , Int. J. Electrochem. Sci. , Vol 7 , 2012 , p 1134 – 1148 82. Lai G.Y...