1-1 of 1 Search Results for

physiochemical test

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Book Chapter

Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003541
EISBN: 978-1-62708-180-1
...-density polyethylene pipe. Arrows indicate the direction of crack propagation. Fig. 28 Fracture band width as a function of crack length for the polyethylene pipe shown in Fig. 27 Fig. 15 Typical load-displacement curve for a ductile polymer tested in uniaxial tension Fig. 16...