Published: 01 June 2019
Fig. 13 Photomicrograph of specimen (a) in figure 12 . (× 80). More
Image
Published: 01 June 2019
Fig. 14 Photomicrograph of specimen (b) in figure 12 . (× 160). More
Image
Published: 01 June 2019
Fig. 7 Photomicrograph showing microstructure of cross section parallel to preexisting crack in bent bar. Equiaxed grain structure is indicated. More
Image
Published: 01 June 2019
Fig. 3 (a) SEI photomicrograph of an inclusion embedded within a crack and X-ray analysis of (b) Fe, (c) Si, (d) Ca, and (e) O More
Image
Published: 01 June 2019
Fig. 6 Photomicrograph showing a cross section of a corrosion pit. (50×) More
Image
Published: 01 June 2019
Fig. 4 Photomicrograph of an ANSI 5 8 -11 failed bolt cross section showing the crack path and morphology. More
Image
Published: 01 June 2019
Fig. 5 Photomicrograph of a secondary SCC crack at the thread root of an ASTM A574 ANSI 5 8 -11 failed bonnet screw. More
Image
Published: 01 June 2019
Fig. 6 Photomicrograph of a secondary SCC crack at the thread root of an ASTM A574 ANSI 5 8 -11 failed bonnet screw. More
Image
Published: 01 June 2019
Fig. 7 Photomicrograph of a secondary SCC crack at the thread root of an ASTM A574 ANSI 5 8 -11 failed bonnet screw. More
Image
Published: 01 June 2019
Fig. 8 SEM photomicrograph of an ASTM 574 ANSI 1 2 -13 bonnet screw fracture surface showing intergranular fracture. More
Image
Published: 01 June 2019
Fig. 9 SEM photomicrograph of an ASTM 574 ANSI 1 2 -13 bonnet screw fracture surface showing intergranular fracture. More
Image
Published: 01 June 2019
Fig. 10 SEM photomicrograph of an ASTM 574 ANSI 1 2 -13 bonnet screw fracture surface showing ductile overload. More
Image
Published: 01 June 2019
Fig. 11 SEM photomicrograph of an ASTM 574 ANSI 5 8 -11 bonnet screw fracture surface showing intergranular fracture. More
Image
Published: 01 June 2019
Fig. 12 SEM photomicrograph of an ASTM 574 ANSI 5 8 -11 bonnet screw fracture surface showing intergranular fracture. More
Image
Published: 01 June 2019
Fig. 13 SEM photomicrograph of an ASTM 574 ANSI 5 8 -11 bonnet screw fracture surface showing ductile overload. More
Image
Published: 01 June 2019
Fig. 9 SEM photomicrograph of pit (crater) morphology More
Image
Published: 01 June 2019
Fig. 2 Composite photomicrograph showing fissures adjacent to fracture. (×50). More
Image
Published: 01 June 2019
Fig. 2 Photomicrograph of a type 301 half-hard stainless steel band clamp loop field failure by hydrogen-stress cracking. 250x More
Image
Published: 01 June 2019
Fig. 4 a. Low magnification photomicrograph showing the weld, base metal and HAZ. b. Higher magnification photomicrograph depicting a typical ferrite + pearlite base material. c. Photomicrograph of the weld metal having a typical dendritic structure. d. The HAZ for the weld composed of fine More
Image
Published: 01 June 2019
Fig. 5 Photomicrograph of a fractured socket-weld. Arrow indicates lack of weld penetration at the weld root More