... properties. At the present time, stainless steels are not used in permanent implants, such as hip or knee joint prostheses, because their corrosion resistance is inadequate; the cobalt-chromium-molybdenum alloys of ASTM F 75 are used instead. Selected References Selected References • Pohler...