Series: ASM Failure Analysis Case Histories
Volume: 3
Publisher: ASM International
Published: 01 December 2019
DOI: 10.31399/asm.fach.v03.c9001816
EISBN: 978-1-62708-241-9
... (where the deformation is accumulated in the austenite in order to obtain the finest ferrite possible after the allotropic transformation), in the same fashion as described in previous work [ 10 ]. In order to achieve this small grain size microstructure, the composition of the steels is very...