Series: ASM Failure Analysis Case Histories
Volume: 3
Publisher: ASM International
Published: 01 December 2019
DOI: 10.31399/asm.fach.v03.c9001816
EISBN: 978-1-62708-241-9
...: The microstructure of the steel shown in Fig. 6 is formed by ferrite and pearlite bands, typical in construction steels which have suffered a peritectic reaction and solidification under non-equilibrium conditions. As the partition coefficient for carbon, alloying elements (Mn and Si), and impurities (P, S...