1-20 of 32 Search Results for

orthopedic implants

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0001819
EISBN: 978-1-62708-180-1
...Abstract Abstract This article commences with a description of the prosthetic devices and implants used for internal fixation. It describes the complications related to implants and provides a list of major standards for orthopedic implant materials. The article illustrates the body environment...
Series: ASM Failure Analysis Case Histories
Volume: 3
Publisher: ASM International
Published: 01 December 2019
DOI: 10.31399/asm.fach.v03.c9001804
EISBN: 978-1-62708-241-9
...Abstract Abstract A stainless steel screw securing an orthopedic implant fractured and was analyzed to determine the cause. Investigators used optical and scanning electron microscopy to examine the fracture surfaces and the microstructure of the austenitic stainless steel from which the screw...
Series: ASM Failure Analysis Case Histories
Volume: 3
Publisher: ASM International
Published: 01 December 2019
DOI: 10.31399/asm.fach.v03.c9001803
EISBN: 978-1-62708-241-9
... discussed. orthopedic implant devices fracture corrosion inclusions and stress gaps medical materials cracking fretting pitting fractography fracture toughness Ti6Al4V (titanium-aluminum-vanadium alloy) UNS R56406 316L stainless steel (austenitic wrought stainless steel) UNS S31603...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.med.c9001690
EISBN: 978-1-62708-226-6
... J. : Proc. Symp. on Retrieval and Analysis of Orthopedic Implants , NBS Special Publication 472 , Maryland , 1976 , pp. 23 – 30 . 2. Pohler O.E.M. : Failure Analysis and Prevention , 9th ed. , vol. 11 , ASM International , 1986 , pp. 668 – 694 . 3. Dumblenton J.H...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.med.c9001606
EISBN: 978-1-62708-226-6
..., or plates, these orthopedic devices are surgically implanted and affixed to bones, usually with screws of the same alloy composition. Fixation implants usually remain in the human body until the broken bone has healed sufficiently to sustain normal loading without the additional support provided...
Series: ASM Failure Analysis Case Histories
Volume: 1
Publisher: ASM International
Published: 01 December 1992
DOI: 10.31399/asm.fach.v01.c9001097
EISBN: 978-1-62708-214-3
...Abstract Abstract Two type 316L stainless steel orthopedic screws broke approximately 6 weeks after surgical implant. The screws had been used to fasten a seven-hole narrow dynamic compression plate to a patient's spine. The broken screws and screws of the same vintage and source were examined...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.med.c9001664
EISBN: 978-1-62708-226-6
... Orthopedic Implants,” Journal of Biomedical Materials Research , Vol. 3 , pp. 247 – 265 ( 1969 ). 2. Hughes A. N. and Jordan B. A. , “Metallurgical Observations on Some Metallic Surgical Implants Which Failed in Vivo,” Journal of Biomedical Materials Research , Vol. 6 , pp. 33...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.med.c9001573
EISBN: 978-1-62708-226-6
... Reference • Pohler O.E.M. , Failures of Metallic Orthopedic Implants , Failure Analysis and Prevention , Vol 11 , ASM Handbook , ASM International , 1986 , p 670 – 694 10.31399/asm.hb.v11.a0001819 The TiN coated back surgery wires were made of Ti6A14V. The reported failure...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.med.c0089543
EISBN: 978-1-62708-226-6
... oxides. 155× Acknowledgments Selected Reference Selected Reference • Pohler O.E.M. , Failures of Metallic Orthopedic Implants , Failure Analysis and Prevention , Vol 11 , ASM Handbook , ASM International , 1986 , p 670 – 694 10.31399/asm.hb.v11.a0001819 The following...
Series: ASM Failure Analysis Case Histories
Volume: 2
Publisher: ASM International
Published: 01 December 1993
DOI: 10.31399/asm.fach.v02.c9001264
EISBN: 978-1-62708-215-0
... • Pohler O.E.M. , Failures of Metallic Orthopedic Implants , Failure Analysis and Prevention , Vol 11 , ASM Handbook , ASM International , 1986 , p 670 – 694 10.31399/asm.hb.v11.a0001819 ...
Series: ASM Failure Analysis Case Histories
Volume: 3
Publisher: ASM International
Published: 01 December 2019
DOI: 10.31399/asm.fach.v03.c9001801
EISBN: 978-1-62708-241-9
... ), 28 – 30 ( 1999 ) 10.1007/s11837-999-0090-y 15. Hertzberg R.W. , Deformation and Fracture Mechanics of Engineering Materials ( Wiley , New York , 1976 ) Selected references Selected references • Pohler O.E.M. , Failures of Metallic Orthopedic Implants , Failure...
Series: ASM Failure Analysis Case Histories
Volume: 2
Publisher: ASM International
Published: 01 December 1993
DOI: 10.31399/asm.fach.v02.c9001266
EISBN: 978-1-62708-215-0
... Reference Selected Reference • Pohler O.E.M. , Failures of Metallic Orthopedic Implants , Failure Analysis and Prevention , Vol 11 , ASM Handbook , ASM International , 1986 , p 670 – 694 10.31399/asm.hb.v11.a0001819 ...
Series: ASM Failure Analysis Case Histories
Volume: 1
Publisher: ASM International
Published: 01 December 1992
DOI: 10.31399/asm.fach.v01.c9001133
EISBN: 978-1-62708-214-3
... of Metallic Orthopedic Implants , Failure Analysis and Prevention , Vol 11 , ASM Handbook , ASM International , 1986 , p 670 – 694 10.31399/asm.hb.v11.a0001819 ...
Series: ASM Failure Analysis Case Histories
Volume: 2
Publisher: ASM International
Published: 01 December 1993
DOI: 10.31399/asm.fach.v02.c9001265
EISBN: 978-1-62708-215-0
... implants for this analysis. Selected Reference Selected Reference • Pohler O.E.M. , Failures of Metallic Orthopedic Implants , Failure Analysis and Prevention , Vol 11 , ASM Handbook , ASM International , 1986 , p 670 – 694 10.31399/asm.hb.v11.a0001819 ...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.homegoods.c9001610
EISBN: 978-1-62708-222-8
.... The usual types of surface finish available in stainless steel bar and wire products, which are delivered to the implant manufacturer, are cold-draw, pickled, ground, and polished. For example, ISO 5839 10 requires that the surfaces of orthopedic prostheses present satin and/or mirror polished finishing...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.med.c9001579
EISBN: 978-1-62708-226-6
.... Styles C.M. , Evans S.L. , and Gregson P.J. : Biomaterials , 1998 , vol. 19 ( 11–12 ), pp. 1057 – 65 . Selected References Selected References • Pohler O.E.M. , Failures of Metallic Orthopedic Implants , Failure Analysis and Prevention , Vol 11 , ASM Handbook , ASM...
Book Chapter

Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003562
EISBN: 978-1-62708-180-1
..., splines, couplings, clutches, spindles, and seals; in press fits on shafts; and in universal joints, base plates, shackles, and orthopedic implants. Generally, fretting occurs at contacting surfaces that are intended to be fixed in relation to each other but that actually undergo minute alternating...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.med.c0048400
EISBN: 978-1-62708-226-6
... to intercrystalline corrosion and implant separation. The wire came from a source different from that of the screws and washers and did not meet current standards for orthopedic wire. Reference Reference 1. Müller M.E. , Allgöwer M. , Schneider R. , and Willenegger H. , Manual...
Series: ASM Handbook
Volume: 11
Publisher: ASM International
Published: 15 January 2021
DOI: 10.31399/asm.hb.v11.a0006829
EISBN: 978-1-62708-295-2
.... , Vol 44 ( No. 5 ), 2011 , p 532 – 549 10.1016/j.triboint.2010.06.010 36. Geringer J. , Forest B. , and Combrade P. , Fretting-Corrosion of Materials Used as Orthopaedic Implants , Wear , Vol 259 , 2005 , p 943 – 951 10.1016/j.wear.2004.11.027 37. Bacroix B...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003522
EISBN: 978-1-62708-180-1
...). Oxalic acid etch Fig. 39 Stress-corrosion cracking in a 316 stainless steel orthopedic implant Fig. 40 Hydrogen-induced cracking in pipeline steel Fig. 41 Voids formed by methane in a carbon steel exposed to a hydrogen atmosphere at high temperature. The carbides...