Published: 30 August 2021
Fig. 3 Silver Bridge between West Virginia and Ohio over the Ohio River. (a) Before collapse. Source: Ref 10 . Courtesy of The Herald-Dispatch , Huntington, WV. (b) After collapse. Source: Ref 11 . Courtesy: © The Blade , Toledo, OH, Dec 1967 More
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.petrol.c9001693
EISBN: 978-1-62708-228-0
... up and down from the defect when the stress induced by filling reached a critical value for the steel, which had poor toughness properties. This steel had been used in the original construction of a tank in Ohio more than 40 years previously. The defect at which brittle fracture originated...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.mech.c9001733
EISBN: 978-1-62708-225-9
... , ASTM STP 436, pp. 3 – 16 , ASTM , Philadelphia , 1968 . 3. Warke W. R. and McCall J. L. : Fractography Using the Electron Microscope , Tech. Rpt. No. W3-2-65, ASM , Metals Park, Ohio . 4. Pelloux R. M. N. : Metals Eng. Quart. , 1965 , vol. 5 , p. 26 . 5...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.marine.c9001673
EISBN: 978-1-62708-227-3
...,” Proceedings of the 3rd International Congress on Marine Corrosion and Fouling , National Bureau of Standards , Gaithersburg, MD , pp. 241 – 263 ( 1972 ). 4. Powell G. W. , “Effect of Sulfides on the Corrosion of Cupro-nickels,” The Ohio State University, private communication ( 1985 ). 5...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.usage.c9001672
EISBN: 978-1-62708-236-5
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003566
EISBN: 978-1-62708-180-1
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.mech.c9001684
EISBN: 978-1-62708-225-9
... , Battelle, Columbus, Ohio , 1970 . 4. Leidheiser H. , The Corrosion of Copper, Tin, and Their Alloys , Wiley , New York , 1971 . 5. Metals Handbook , 10th ed. , Vol. 2 . Properties and Selection:Nonferrous Alloys and Special-Purpose Materials , ASM International , Materials Park...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.petrol.c9001148
EISBN: 978-1-62708-228-0
... V. , Rowe R. A. and Whiteson B. V. , Electron Fractography Handbook , Battelle Laboratories , Columbus, Ohio , 1976 , pp. 3 – 35 . 4. Metals Handbook , Vol. 10 , American Society for Metals , Metals Park, Ohio , 1975 , pp. 216 . 5. Russo M. , “Analysis...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.med.c0089543
EISBN: 978-1-62708-226-6
.... Chaudhari, Columbus Metallurgical Services, Inc., Columbus, Ohio. Selected Reference Selected Reference • Pohler O.E.M. , Failures of Metallic Orthopedic Implants , Failure Analysis and Prevention , Vol 11 , ASM Handbook , ASM International , 1986 , p 670 – 694 10.31399/asm.hb.v11...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.pulp.c0089682
EISBN: 978-1-62708-230-3
.... Worzala, University of Wisconsin; Carl J. Czajkowski, Department of Nuclear Energy, Brookhaven National Laboratory, Upton, New York; and Mohan D. Chaudhari, Columbus Metallurgical Services, Inc., Columbus, Ohio. Selected Reference Selected Reference • Forms of Corrosion , Failure Analysis...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.aero.c0089563
EISBN: 978-1-62708-217-4
...; Frank J. Worzala, University of Wisconsin; Carl J. Czajkowski, Department of Nuclear Energy, Brookhaven National Laboratory, Upton, New York; and Mohan D. Chaudhari, Columbus Metallurgical Services, Inc., Columbus, Ohio. Selected Reference Selected Reference • Miller B.A. , Overload...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.bldgs.c0089530
EISBN: 978-1-62708-219-8
... Services, Inc., Columbus, Ohio. Selected Reference Selected Reference • Miller B.A. , Overload Failures , Failure Analysis and Prevention , Vol 11 , ASM Handbook , ASM International , 2002 , p 671 – 699 10.31399/asm.hb.v11.a0003543 ...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.auto.c0089551
EISBN: 978-1-62708-218-1
..., Ohio. Selected Reference Selected Reference • Fatigue Failures , Failure Analysis and Prevention , Vol 11 , ASM Handbook , ASM International , 2002 , p 700 – 727 10.31399/asm.hb.v11.a0003544 ...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.process.c9001522
EISBN: 978-1-62708-235-8
... Laboratory Materials and Manufacturing Directorate entered into a collaborative research effort with H.R. Textron Inc., of Valencia, Calif.; Crown Pattern and Foundry of Alahambra, Calif.; Universal Energy Systems Inc., of Dayton, Ohio; and Boeing, to examine the problem. Researchers systematically...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.chem.c0089633
EISBN: 978-1-62708-220-4
..., Columbus Metallurgical Services, Inc., Columbus, Ohio. Selected Reference Selected Reference • Fatigue Failures , Failure Analysis and Prevention , Vol 11 , ASM Handbook , ASM International , 2002 , p 700 – 727 10.31399/asm.hb.v11.a0003544 ...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.machtools.c0089534
EISBN: 978-1-62708-223-5
... of Wisconsin; Carl J. Czajkowski, Department of Nuclear Energy, Brookhaven National Laboratory, Upton, New York; and Mohan D. Chaudhari, Columbus Metallurgical Services, Inc., Columbus, Ohio. Selected Reference Selected Reference • Becker W.T. and McGarry D. , Mechanisms and Appearances...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.aero.c9001555
EISBN: 978-1-62708-217-4
... Vol.9 p. 186 , American Society for Metals , Ohio ( 1974 ) 2. Lothar Engle and Hermann Klesigele “An Atlas of Metal Damage” (English version), p. 121 , 122 & 123 , Wolfe Publishing Ltd. , Conway Street, London ( 1981 ) Selected References Selected References • Fatigue...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.power.c0089663
EISBN: 978-1-62708-229-7
..., Case Western Reserve University; Frank J. Worzala, University of Wisconsin; Carl J. Czajkowski, Department of Nuclear Energy, Brookhaven National Laboratory, Upton, New York; and Mohan D. Chaudhari, Columbus Metallurgical Services, Inc., Columbus, Ohio. Selected References Selected References...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.process.c0089651
EISBN: 978-1-62708-235-8
..., Columbus Metallurgical Services, Inc., Columbus, Ohio. Selected Reference Selected Reference • Fatigue Failures , Failure Analysis and Prevention , Vol 11 , ASM Handbook , ASM International , 2002 , p 700 – 727 10.31399/asm.hb.v11.a0003544 ...
Series: ASM Handbook
Volume: 11A
Publisher: ASM International
Published: 30 August 2021
DOI: 10.31399/asm.hb.v11A.a0006833
EISBN: 978-1-62708-329-4
... manufacturing, design, regulation, and/or maintenance. Point Pleasant, West Virginia, Silver Bridge over the Ohio River In December 1967, the Silver Bridge between West Virginia and Ohio over the Ohio River collapsed, killing 46 people ( Fig. 3 ). The collapse was due to preexisting cracks that resulted...