By Raymond G. Bayer
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003558
EISBN: 978-1-62708-180-1
... based on the characterization of the elements of the tribosystem at the contact. The nominal type of motion, that is rolling, sliding and impact, and in the case of sliding, lubricated or nonlubricated wear, often are considered as major subcategories of nonabrasive wear situations. Some subcategories...