1-2 of 2 Search Results for

nonequilibrium reactions

Sort by
Book Chapter

Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003548
EISBN: 978-1-62708-180-1
... denickelification desiliconification dezincification galvanic corrosion graphitic corrosion intergranular corrosion pitting corrosion selective leaching uniform corrosion velocity-affected corrosion CORROSION is the electrochemical reaction of a material and its environment. This article addresses...
Series: ASM Handbook
Volume: 11
Publisher: ASM International
Published: 15 January 2021
DOI: 10.31399/asm.hb.v11.a0006783
EISBN: 978-1-62708-295-2
... Abstract Corrosion is the electrochemical reaction of a material and its environment. This article addresses those forms of corrosion that contribute directly to the failure of metal parts or that render them susceptible to failure by some other mechanism. Various forms of corrosion covered...