1-8 of 8 Search Results for

nickel-tungsten composite electroplating

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Series: ASM Handbook
Volume: 11
Publisher: ASM International
Published: 15 January 2021
DOI: 10.31399/asm.hb.v11.a0006778
EISBN: 978-1-62708-295-2
... in Fig. 4 . Face-centered-cubic (fcc) metals (for example, copper, aluminum, nickel, and austenitic steels) exhibit the greatest ductility during rapid fracture and, in benign environments, do not normally fracture via cleavage. However, brittle cracking of fcc metals can occur under conditions...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003543
EISBN: 978-1-62708-180-1
..., specifically oriented grains tend to crack, leaving a shiny, faceted appearance easily differentiated from dull and fibrous, dimple-rupture features. Cleavage in a steel sample is shown in Fig. 4 . Face-centered-cubic (fcc) metals (for example, copper, aluminum, nickel, and austenitic steels) exhibit...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003555
EISBN: 978-1-62708-180-1
...-base superalloy 1040 1900 1 S-816 cobalt-base superalloy 980 1800 1 Hastelloy X nickel-base superalloy 1205 2200 1 HX (17Cr-66Ni-bal Fe) 1150 2100 1 (a) Seamless tube. (b) Electric resistance welded tube Melting points of common refractories Table 2...
Book Chapter

Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003548
EISBN: 978-1-62708-180-1
... can be obtained by using polarization curves, critical potentials, and the mixed potential of the galvanic couple. In chloride-bearing environments, galvanically induced localized corrosion of many stainless steels occurs in couples with copper or nickel and their alloys and with other more noble...
Series: ASM Handbook
Volume: 11
Publisher: ASM International
Published: 15 January 2021
DOI: 10.31399/asm.hb.v11.a0006783
EISBN: 978-1-62708-295-2
... steels can be obtained by using polarization curves, critical potentials, and the mixed potential of the galvanic couple. In chloride-bearing environments, galvanically induced localized corrosion of many stainless steels occurs in couples with copper or nickel and their alloys and with other more noble...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003553
EISBN: 978-1-62708-180-1
... mm (0.050 in.) thick; both were made of 19-9 DL heat-resisting alloy with the following composition: Element Composition, % Carbon 0.3 Manganese 1.1 Silicon 0.6 Chromium 19 Nickel 9 Molybdenum 1.25 Tungsten 1.2 Niobium 0.4 Titanium 0.3 Iron Bal...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003524
EISBN: 978-1-62708-180-1
... as a study tool for the investigation of fracture mechanisms and of behavior of materials Periodic inspection of tanks and aerial-device booms made of composite materials This type of data may be useful background information in a failure analysis, or the technique might be used in evaluation...
Series: ASM Handbook
Volume: 11A
Publisher: ASM International
Published: 30 August 2021
DOI: 10.31399/asm.hb.v11A.9781627083294
EISBN: 978-1-62708-329-4