1-11 of 11 Search Results for

microchemical analysis

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003529
EISBN: 978-1-62708-180-1
... Abstract This article describes some of the common elemental composition analysis methods and explains the concept of referee and economy test methods in failure analysis. It discusses different types of microchemical analyses, including backscattered electron imaging, energy-dispersive...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003518
EISBN: 978-1-62708-180-1
... Abstract Failure analysis is a process that is performed to determine the causes or factors that have led to an undesired loss of functionality. This article describes some of the factors and conditions that might be considered when approaching a failure analysis problem. It focuses on the key...
Series: ASM Handbook
Volume: 11
Publisher: ASM International
Published: 15 January 2021
DOI: 10.31399/asm.hb.v11.a0006754
EISBN: 978-1-62708-295-2
... Abstract Failure analysis is a process that is performed in order to determine the causes or factors that have led to an undesired loss of functionality. This article is intended to demonstrate proper approaches to failure analysis work. The goal of the proper approach is to allow the most...
Series: ASM Handbook
Volume: 11
Publisher: ASM International
Published: 15 January 2021
DOI: 10.31399/asm.hb.v11.a0006782
EISBN: 978-1-62708-295-2
... is not contaminated during the collection process. The most common types of analysis performed on the corrosion debris are discussed later. Energy-dispersive x-ray spectroscopy (EDS) is a semiquantitative microchemical analysis technique performed using equipment attached to the scanning electron...
Series: ASM Failure Analysis Case Histories
Volume: 3
Publisher: ASM International
Published: 01 December 2019
DOI: 10.31399/asm.fach.v03.c9001771
EISBN: 978-1-62708-241-9
..., coke readily accumulates on the surface of the tubes, fueling carbon diffusion into the metal and a corresponding degradation in microstructure and loss of ductility at high temperatures. radiant tube stress rupture thermal shock heat resistant steel carbide precipitates SEM-EDS analysis...
Series: ASM Handbook
Volume: 11
Publisher: ASM International
Published: 15 January 2021
DOI: 10.31399/asm.hb.v11.a0006757
EISBN: 978-1-62708-295-2
.... ceramic materials corrosion damage macroscopic examination metallic components metallographic specimens microchemical analysis microfractography microstructure polymers visual examination wear EXAMINATION of a damaged component involves a chain of activities that, first and foremost...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003522
EISBN: 978-1-62708-180-1
..., Auger electron spectroscopy, secondary ion mass spectroscopy, and X-ray powder diffraction. The article discusses the analysis and interpretation of base material composition and microstructures. Preparation and examination of metallographic specimens in failure analysis are also discussed. The article...
Series: ASM Handbook
Volume: 11
Publisher: ASM International
Published: 15 January 2021
DOI: 10.31399/asm.hb.v11.a0006784
EISBN: 978-1-62708-295-2
... hydrogen damage in all the major commercial alloy systems. It covers the broader topic of hydrogen damage, which can be quite complex and technical in nature. The article focuses on failure analysis where hydrogen embrittlement of a steel component is suspected. It provides practical advice for the failure...
Series: ASM Failure Analysis Case Histories
Volume: 3
Publisher: ASM International
Published: 01 December 2019
DOI: 10.31399/asm.fach.v03.c9001757
EISBN: 978-1-62708-241-9
... through the 17th compressor stages, as were stator vanes and casing sections. The fractured surface of the 17th blade showed multiple origins along with secondary cracking and extensive propagation that preceded separation. The metallographic analysis of the microstructure suggested work hardening. Based...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.modes.c9001681
EISBN: 978-1-62708-234-1
... this procedure, a microstructural analysis was made of the cast components. This involved optical microscopy (OM), scanning electron microscopy (SEM), transmission electron microscopy (TEM) and scanning transmission electron microscopy (STEM). IN SEM and STEM, microchemical analyses were obtained of...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003552
EISBN: 978-1-62708-180-1
... is an overview of the different types of hydrogen damage in all the major commercial alloy systems. These two sections cover the broader topic of hydrogen damage, which can be quite complex and technical in nature. The third part of this article focuses on failure analysis where hydrogen...