Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.auto.c9001704
EISBN: 978-1-62708-218-1
.... The examinations revealed a classic case of microbiologically influenced corrosion (MIC), which preferentially attacked the heat affected zones of the tank welds, resulting in the leaks. Heat affected zone Leakage Water tanks Welded joints 304 UNS S30400 Biological corrosion The experienced...
Series: ASM Handbook
Volume: 11
Publisher: ASM International
Published: 15 January 2021
DOI: 10.31399/asm.hb.v11.a0006788
EISBN: 978-1-62708-295-2
...) … … Anaerobic MIC (SRB) → aerobic Elemental sulfur, iron (III) oxides plus residual anaerobic corrosion products 2–5 0.08–0.20 Source: Ref 62 Examples of microbiologically influenced corrosion (MIC) scenarios in the corrosion of stainless steel weldments Table 4 Examples of microbiologically...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.modes.c9001683
EISBN: 978-1-62708-234-1
...Abstract Abstract Corrosion in a closed-loop cooling water system constructed of austenitic stainless steel occurred during an extended lay up of the system with biologically contaminated water. The characteristics of the failure were those of microbiologically influenced corrosion (MIC...
Series: ASM Failure Analysis Case Histories
Volume: 3
Publisher: ASM International
Published: 01 December 2019
DOI: 10.31399/asm.fach.v03.c9001808
EISBN: 978-1-62708-241-9
...Abstract Abstract Six cases of failure attributed to microbiologically influenced corrosion (MIC) were analyzed to determine if any of the failures could have been avoided or at least predicted. The failures represent a diversity of applications involving typical materials, primarily stainless...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003556
EISBN: 978-1-62708-180-1
...Abstract Abstract This article focuses on the mechanisms of microbially induced or influenced corrosion (MIC) of metallic materials as an introduction to the recognition, management, and prevention of microbiological corrosion failures in piping, tanks, heat exchangers, and cooling towers...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.bldgs.c0091806
EISBN: 978-1-62708-219-8
... in Underground Brass Pipes ; Biologically Induced Corrosion , Dexter S.C. , Ed., National Association of Corrosion Engineers , 1986 , p 102 – 108 2. Yoffe P. , Microbiologically Influenced Failures of Cupronickel and Aluminum Brass Condenser Tubes: Comparison of Real Cases , Proc. 1995...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.9781627081801
EISBN: 978-1-62708-180-1
Series: ASM Handbook
Volume: 11
Publisher: ASM International
Published: 15 January 2021
DOI: 10.31399/asm.hb.v11.a0006783
EISBN: 978-1-62708-295-2
... measures. corrosion prevention crevice corrosion dealloying corrosion galvanic corrosion intergranular corrosion microbiologically influenced corrosion pitting selective leaching uniform corrosion velocity-affected corrosion CORROSION is the electrochemical reaction of a material...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.power.c0091807
EISBN: 978-1-62708-229-7
.... , Microbiologically Influenced Stress Corrosion Cracking Failure of Admiralty Brass Condenser Tubes in a Nuclear Power Plant Cooled by Freshwater , Corros. Sci. Vol 40 ( No. 11 ), 1998 , p 1821 – 1836 10.1016/S0010-938X(98)00079-1 Selected Reference Selected Reference • Warke W. R...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003549
EISBN: 978-1-62708-180-1
... from the source (incoming water supply) and from the end use (for example, a faucet). Microbiologically influenced corrosion may apply in certain cases. On-site testing or sample removal is necessary to retain the most accurate information regarding the type and number of bacteria involved. In most...
Series: ASM Failure Analysis Case Histories
Volume: 1
Publisher: ASM International
Published: 01 December 1992
DOI: 10.31399/asm.fach.v01.c9001064
EISBN: 978-1-62708-214-3
... of the material, analysis of hydrotest waters, and microbiological examination of slime that had formed in certain pipework sections. It was determined that the failure resulted from microbially induced corrosion promoted by the use of poor-quality hydrotest water and uncontrolled hydrotesting practice. Use...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003500
EISBN: 978-1-62708-180-1
..., a failure analysis incorrectly ends at the identification of the failure mechanism and perhaps causal influences. The principles of root-cause analysis (RCA) may be applied to ensure that the root cause is understood and appropriate corrective actions may be identified. An RCA exercise may simply...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.modes.c9001648
EISBN: 978-1-62708-234-1
... , 1991 , p. 778 . 5. ASM Handbook , Vol. 13, Corrosion , ASM International , Metals Park, OH , 1987 , pp. 114 – 22 , 314–5. 6. Kobrin G. : “Corrosion by Microbiological Organisms in Natural Waters,” in Corrosion Source Book , American Society for Metals , Metals Park, OH...
Series: ASM Handbook
Volume: 11
Publisher: ASM International
Published: 15 January 2021
DOI: 10.31399/asm.hb.v11.a0006753
EISBN: 978-1-62708-295-2
..., and material, which are discussed in the following sections along with examples. The tools available for failure analysis are then covered. Further, the article describes the categories of mode of failure: distortion or undesired deformation, fracture, corrosion, and wear. It provides information...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.aero.c0091809
EISBN: 978-1-62708-217-4
... a widespread potential for MIC wherever conditions permit microbial growth on aluminum or its alloys. Reference Reference 1. Hagenauer A. , Hilpert R. , and Hack T. , Microbiological Investigations of Corrosion Damage in Aircraft , Werkst. Korros. , Vol 45 , 1994 , p 355 – 360...
Series: ASM Handbook
Volume: 11
Publisher: ASM International
Published: 15 January 2021
DOI: 10.31399/asm.hb.v11.a0006782
EISBN: 978-1-62708-295-2
...: melting point, glass transition Adapted from Ref 17 Fig. 26 Impressed-current cathodic protection of a buried pipeline using graphite anodes. Source: Ref 13 Fig. 24 Examples of how design and assembly can affect localized corrosion by creating crevices and traps where corrosive...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.med.c9001690
EISBN: 978-1-62708-226-6
... of corrosion assisted fracture. Additionally, some components were found to contain fabrication/processing defects that contributed to premature failure. The implant of nonbiocompatible materials results in immeasurable damage to patients as well as losses for the public investment. It is proposed that local...
Book Chapter

Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003548
EISBN: 978-1-62708-180-1
... of galvanic potentials is only a ranking of general susceptibility; it does not address all the conditions and factors that influence galvanic corrosion. Limitations on the use of galvanic series include: No information is available on the rate of corrosion Active-passive metals may display two...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003553
EISBN: 978-1-62708-180-1
...Abstract Abstract This article commences with a discussion on the characteristics of stress-corrosion cracking (SCC) and describes crack initiation and propagation during SCC. It reviews the various mechanisms of SCC and addresses electrochemical and stress-sorption theories. The article...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.bldgs.c0091201
EISBN: 978-1-62708-219-8
... of aerobic bacteria. Chlorides Piping Sewer treatment systems 316L UNS S31603 Biological corrosion Pitting corrosion Type 316L (UNS S31603) austenitic stainless steel piping was installed as part of a collection system for a storm sewer treatment system used in a manufacturing facility...