... in water or seawater that is exposed to the atmosphere (a steel pier piling, for example). Corrosion occurs. The anodic reaction is: (Eq 14) Fe → Fe 2 + + 2 e − Because the medium is exposed to the atmosphere, it contains dissolved oxygen. Water and seawater are nearly neutral...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003509
EISBN: 978-1-62708-180-1
... welding processes. The article also describes failure origins in other welding processes, such as electroslag welds, electrogas welds, flash welds, upset butt welds, flash welds, electron and laser beam weld, and high-frequency induction welds. arc welding brittle fracture electrogas welds...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003549
EISBN: 978-1-62708-180-1
... or seawater that is exposed to the atmosphere (an automobile fender or a steel pier piling are examples). Corrosion occurs. The anodic reaction is: (Eq 14) Fe → Fe 2 + + 2 e Since the medium is exposed to the atmosphere, it contains dissolved oxygen. Water and seawater are nearly...
Series: ASM Handbook
Volume: 11
Publisher: ASM International
Published: 15 January 2021
DOI: 10.31399/asm.hb.v11.a0006783
EISBN: 978-1-62708-295-2
... Corrosion Failures ,” and “ High-Temperature Corrosion-Related Failures .” Additional discussion can be found in the articles “ Effect of Environment on the Performance of Plastics ” and “ Corrosion Failures of Industrial Refractories and Technical Ceramics ” in Failure Analysis and Prevention , Volume 11...
Book Chapter

Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003548
EISBN: 978-1-62708-180-1
... and prevention of several types of failure in which corrosion is a contributing factor. These articles include “Stress-Corrosion Cracking,” “Liquid-Metal and Solid-Metal Induced Embrittlement,” “Hydrogen Damage and Embrittlement,” “Corrosive Wear Failures,” “Biological Corrosion Failures,” and “High...