... Abstract Leakage was detected in a malleable iron elbow (ASTM A 47, grade 35018) after only three months in service. Life expectancy for the elbow was 12 to 24 months. The piping alternately supplied steam and cooling water to a tire-curing press. The supply line and elbow were subjected to 14...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.bldgs.c0046505
EISBN: 978-1-62708-219-8
... by a pivoted malleable iron latch. The latch and top surface of the clapper plate were usually in a sanitary-water environment (stabilized, chlorinated well water with a pH of 7.3) under stagnant conditions. Process make-up water that had been clarified, filtered, softened, and chlorinated and had a pH of 9.8...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.process.c0089651
EISBN: 978-1-62708-235-8
... Abstract Several diesel-engine rocker levers (malleable iron similar to ASTM A 602, grade M7002) failed at low hours in overspeed, over-fuel, highly loaded developmental engine tests. Identical rocker levers had performed acceptably in normal engine tests. The rocker levers were failing through...
Image
Published: 01 June 2019
Fig. 1 Sprinkler system in which a malleable iron deluge clapper latch failed from galvanic attack caused by contact with a copper alloy clapper in stagnant water. (a) Schematic illustration of sprinkler system showing deluge clapper latch that failed. (b) Photograph of clapper latch showing More
Image
Published: 01 June 2019
Fig. 1 Malleable iron elbow in which impingement corrosion caused leakage and failure at the bend. (a) Section through the elbow showing extent of corrosion and point of leakage. Regions A and B are locations of specimens shown in micrographs (b) and (c), respectively. (b) Micrograph More
Image
Published: 01 June 2019
Fig. 1 Failed malleable iron rocker lever. (a) Illustration showing failure location (arrow). (b) Typical appearance of fracture face with dark overload fracture at top, light-gray fatigue fracture, and black casting defect (arrow). 1.5x More
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003508
EISBN: 978-1-62708-180-1
... iron, gray cast iron, malleable irons, ductile iron, low-alloy steel castings, austenitic steels, corrosion-resistant castings, and cast aluminum alloys are the materials discussed. The article describes the general types of discontinuities or imperfections for traditional casting with sand molds...
Series: ASM Failure Analysis Case Histories
Volume: 2
Publisher: ASM International
Published: 01 December 1993
DOI: 10.31399/asm.fach.v02.c9001307
EISBN: 978-1-62708-215-0
.... The hanger was made from malleable cast iron that had been heat treated to produce a decarburized surface layer and a pearlitic transition layer. It had been repair welded after breaking into two pieces longitudinally in a prior incident, using cast iron as weld metal. The repair weld bead on both surfaces...
Book Chapter

Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003548
EISBN: 978-1-62708-180-1
.... For example, aluminum is anodic to zinc in an aqueous 1 M sodium chromate (Na 2 CrO 4 ) solution and cathodic to iron in an aqueous 1 M sodium sulfate (Na 2 SO 4 ) solution ( Ref 4 ). Emf Series The emf series is a table that lists in order the standard electrode potentials of specified...
Series: ASM Handbook
Volume: 11
Publisher: ASM International
Published: 15 January 2021
DOI: 10.31399/asm.hb.v11.a0006783
EISBN: 978-1-62708-295-2
... for seawater is not necessarily valid in nonsaline solutions. For example, aluminum is anodic to zinc in an aqueous 1 M sodium chromate (Na 2 CrO 4 ) solution and cathodic to iron in an aqueous 1 M sodium sulfate (Na 2 SO 4 ) solution ( Ref 4 ). Electromotive Force Series The electromotive force...
Series: ASM Handbook
Volume: 11A
Publisher: ASM International
Published: 30 August 2021
DOI: 10.31399/asm.hb.v11A.a0006831
EISBN: 978-1-62708-329-4
... some of the common defects in each category. The following sections reference the terminology introduced in Table 1 . Failures Related to Gray Iron Castings The cast iron family consists of several different alloys, including gray iron, ductile iron, malleable iron, white iron, compacted...
Series: ASM Handbook
Volume: 11A
Publisher: ASM International
Published: 30 August 2021
DOI: 10.31399/asm.hb.v11A.9781627083294
EISBN: 978-1-62708-329-4
Series: ASM Handbook
Volume: 11
Publisher: ASM International
Published: 15 January 2021
DOI: 10.31399/asm.hb.v11.a0006778
EISBN: 978-1-62708-295-2
... depending on the component geometry. Mechanical conditions and metallurgical features can influence the appearance of MVC. Examples are shown for a ferritic steel ( Fig. 1a ), ductile iron ( Fig. 1b ), and cast titanium alloy ( Fig. 1c ). The dimple features are evident in equiaxed form for tensile loading...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0001812
EISBN: 978-1-62708-180-1
... fasteners are one-piece fasteners, either solid or tubular, that are used in assemblies in which the load is primarily shear. A malleable collar is sometimes swaged or formed on the pin to secure the joint. Special-Purpose Fasteners Special-purpose fasteners, many of which are proprietary...
Series: ASM Handbook
Volume: 11A
Publisher: ASM International
Published: 30 August 2021
DOI: 10.31399/asm.hb.v11A.a0006805
EISBN: 978-1-62708-329-4
... mechanism, an explosive, or other device forms an upset on the inaccessible side. Pin fasteners are one-piece fasteners, either solid or tubular, that are used in assemblies in which the load is primarily shear. A malleable collar is sometimes swaged or formed on the pin to secure the joint. Special-purpose...