1-20 of 54 Search Results for

laser processing

Sort by
Series: ASM Handbook
Volume: 11A
Publisher: ASM International
Published: 30 August 2021
DOI: 10.31399/asm.hb.v11A.a0006838
EISBN: 978-1-62708-329-4
... at specific locations on a build platform or part. The materials in the AM jetting processes involved controlled deposition of curable polymers or atomized melt (material jetting) or powder deposition with binder resins (binder jetting). Other AM technologies emerged with the development of selective laser...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.power.c9001580
EISBN: 978-1-62708-229-7
... details the laser surface mapping activity and demonstrates the potential utility of this technology in failure investigations. Discussion Normal Canister Production A brief description of the canister welding process is given here in an effort to clarify later descriptions and conclusions...
Image
Published: 30 August 2021
Fig. 1 Power ( P ) and velocity ( V ) in metal additive manufacturing processes by powder-bed fusion, wire-feed electron beam, and directed-energy (laser) deposition processes. Source: Ref 5 More
Image
Published: 15 May 2022
Fig. 51 Schematic drawing of the selective laser sintering additive manufacturing process More
Series: ASM Handbook
Volume: 11B
Publisher: ASM International
Published: 15 May 2022
DOI: 10.31399/asm.hb.v11B.a0006936
EISBN: 978-1-62708-395-9
... in accordance with a predetermined scanning regime. The robot control program can then be autogenerated and downline loaded into the robot controller, thus eliminating the need for human programming. Fig. 16 Laser scanner system Image Processing Acquiring the C-scan in digital form makes image...
Series: ASM Handbook
Volume: 11
Publisher: ASM International
Published: 15 January 2021
DOI: 10.31399/asm.hb.v11.a0006772
EISBN: 978-1-62708-295-2
... in compiling the dataset. Data acquisition is critical in creating virtual point clouds. Three-dimensional data cannot be compiled properly without enough data overlap between photographs or laser scans. Figure 4 shows the final image of one-tenth mile of rural roadway imaged by an sUAS and processed...
Series: ASM Handbook
Volume: 11B
Publisher: ASM International
Published: 15 May 2022
DOI: 10.31399/asm.hb.v11B.a0006864
EISBN: 978-1-62708-395-9
... Abstract This article discusses technologies focused on processing plastic materials or producing direct tools used in plastics processing. The article focuses on extrusion and injection molding, covering applications, materials and their properties, equipment, processing details, part design...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003509
EISBN: 978-1-62708-180-1
... welding processes. The article also describes failure origins in other welding processes, such as electroslag welds, electrogas welds, flash welds, upset butt welds, flash welds, electron and laser beam weld, and high-frequency induction welds. arc welding brittle fracture electrogas welds...
Series: ASM Handbook
Volume: 11A
Publisher: ASM International
Published: 30 August 2021
DOI: 10.31399/asm.hb.v11A.a0006828
EISBN: 978-1-62708-329-4
... Abstract The various methods of furnace, torch, induction, resistance, dip, and laser brazing are used to produce a wide range of highly reliable brazed assemblies. However, imperfections that can lead to braze failure may result if proper attention is not paid to the physical properties...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003569
EISBN: 978-1-62708-180-1
... and Laser-Processed Hardfaced Coatings , Wear , Vol 117 ( No. 1 ), 1987 , p 103 – 107 40. Tomlinson W.J. , Megaw J.H.P.C. , Brandsden A.S. , and Girardi M. , The Effect of Laser Melting on the Cavitation Wear of Grey Cast Iron in Distilled and 3% Salt Water , Wear , Vol...
Series: ASM Handbook
Volume: 11
Publisher: ASM International
Published: 15 January 2021
DOI: 10.31399/asm.hb.v11.a0006764
EISBN: 978-1-62708-295-2
... and resolution at least equivalent to that obtained with direct visual inspection. The final image can be very high quality by using a contemporary camera plus appropriate software for further image processing. Optical Laser Scanning One important extension of “visual” inspection is the use of optical...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003549
EISBN: 978-1-62708-180-1
... electrically charged, which is clearly impossible. The corrosion of zinc in hydrochloric acid is an electrochemical process. That is, any reaction that can be divided into two or more partial reactions of oxidation and reduction due to the transfer of electrical charge is termed electrochemical. Dividing...
Series: ASM Failure Analysis Case Histories
Volume: 3
Publisher: ASM International
Published: 01 December 2019
DOI: 10.31399/asm.fach.v03.c9001840
EISBN: 978-1-62708-241-9
...-5 2. Sexton L. , Lavin S. , Byrne G. , Kennedy A. : Laser cladding of aerospace materials . J. Mater. Process . 122 , 63 – 68 ( 2002 ) 10.1016/S0924-0136(01)01121-9 3. Dinda G.P. , Dasgupta A.K. , Mazumder J. : Laser aided direct deposition...
Series: ASM Handbook
Volume: 11
Publisher: ASM International
Published: 15 January 2021
DOI: 10.31399/asm.hb.v11.a0006782
EISBN: 978-1-62708-295-2
... the electrochemical nature of corrosion and provides the typical analysis of environmental- and corrosion-related failures. It presents common methods of testing of laboratory corrosion and discusses the processes involved in the prevention of environmental- and corrosion-related failures of metals and nonmetals...
Series: ASM Handbook
Volume: 11
Publisher: ASM International
Published: 15 January 2021
DOI: 10.31399/asm.hb.v11.a0006768
EISBN: 978-1-62708-295-2
... be used in (but are not necessarily limited to) situations where failures result from overloading, stress corrosion, fatigue, stress concentrations, or inappropriate manufacturing processes. X-ray diffraction residual-stress analysis methods can also be applied to the evaluation of corrective measures...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003536
EISBN: 978-1-62708-180-1
..., and practical examples are provided. fracture profilometry quantitative fractography scanning electron microscope three-dimensional fracture surface reconstruction A FRACTURE SURFACE is generated by the deformation and fracture processes operative at numerous length scales ranging from nanometers...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.power.c9001682
EISBN: 978-1-62708-229-7
..., the fatigue life of these expansion joints could be improved by using a high energy density welding process such as laser beam welding to further reduce heat input . These steps would reduce the number and size of potential microcracks to act as fatigue crack initiation sites. References References 1...
Series: ASM Handbook
Volume: 11A
Publisher: ASM International
Published: 30 August 2021
DOI: 10.31399/asm.hb.v11A.a0006801
EISBN: 978-1-62708-329-4
... in quantifying the relationship with processing quality parameters in production. Factors known to influence the ability to expand a cut edge include: Sheet metal Sheet metal strength Edge-creation method (punching, laser, waterjet, etc.) Edge quality of the hole Hole diameter Punch/die...
Series: ASM Handbook
Volume: 11B
Publisher: ASM International
Published: 15 May 2022
DOI: 10.31399/asm.hb.v11B.9781627083959
EISBN: 978-1-62708-395-9
Series: ASM Handbook
Volume: 11
Publisher: ASM International
Published: 15 January 2021
DOI: 10.31399/asm.hb.v11.a0006759
EISBN: 978-1-62708-295-2
... failure analysis. It describes the general considerations for bulk and microscale chemical analysis in failure analysis, the most effective techniques to use for organic or inorganic materials, and examples of using these techniques. The article discusses the processes involved in the chemical analysis...