.... The weldments were finally secured to the bases of the turbine blades by a brazing operation. One of the laser beam attachment welds broke after a 28-h engine test run. Exposure of the fracture surface for study under the electron microscope revealed the joint had broken in stress rupture. Failure was caused...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.modes.c0006440
EISBN: 978-1-62708-234-1
...Abstract Abstract A failed laser mirror and another complete mirror of the same construction were analyzed. The laser mirror consisted of three layers of material brazed together to form channels through which the cooling water flows. Samples were analyzed with light optical and scanning...
Series: ASM Failure Analysis Case Histories
Volume: 3
Publisher: ASM International
Published: 01 December 2019
DOI: 10.31399/asm.fach.v03.c9001840
EISBN: 978-1-62708-241-9
.../0022-3115(81)90166-5 2. Sexton L. , Lavin S. , Byrne G. , Kennedy A. : Laser cladding of aerospace materials . J. Mater. Process . 122 , 63 – 68 ( 2002 ) 10.1016/S0924-0136(01)01121-9 3. Dinda G.P. , Dasgupta A.K. , Mazumder J. : Laser aided...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003509
EISBN: 978-1-62708-180-1
... welding processes. The article also describes failure origins in other welding processes, such as electroslag welds, electrogas welds, flash welds, upset butt welds, flash welds, electron and laser beam weld, and high-frequency induction welds. arc welding brittle fracture electrogas welds...
Series: ASM Handbook
Volume: 11
Publisher: ASM International
Published: 15 January 2021
DOI: 10.31399/asm.hb.v11.a0006764
EISBN: 978-1-62708-295-2
... for dimensional anomalies, color variation, cracks, pits, etc. Only sensitive to surface flaws Low cost, intuitive. May be enhanced with PT, MT, IR, UV, laser reference lines, video, and magnifying lenses All Thermal/infrared (IR)—includes passive thermal inspections, flash thermography, and laser flying...