1-4 of 4 Search Results for

isophthalic resins

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Series: ASM Handbook
Volume: 11B
Publisher: ASM International
Published: 15 May 2022
DOI: 10.31399/asm.hb.v11B.a0006929
EISBN: 978-1-62708-395-9
... in Fig. 15 include orthophthalic esters, isophthalic esters, and bisphenol A/fumarate resins. Figure 16 demonstrates the varying effect of 100 °C (212 °F) water exposure on glass laminates based on the three polyester types. Despite the orthophthalic polyester showing a dramatic loss of properties...
Series: ASM Handbook
Volume: 11B
Publisher: ASM International
Published: 15 May 2022
DOI: 10.31399/asm.hb.v11B.a0006925
EISBN: 978-1-62708-395-9
.... Engineering plastics all have, as their principal constituent, one or more synthetic polymer resins and almost universally contain additives. Additives, which have much smaller molecules than polymers, provide color, flexibility, rigidity, flame resistance, weathering resistance, and/or processibility...
Series: ASM Handbook
Volume: 11B
Publisher: ASM International
Published: 15 May 2022
DOI: 10.31399/asm.hb.v11B.a0006923
EISBN: 978-1-62708-395-9
..., and glass transition temperature. It also provides information on polyimide and bismaleimide resin systems. Representative examples of different types of engineering thermoplastics are discussed primarily in terms of structure and thermal properties. chemical composition elastomeric materials...
Series: ASM Handbook
Volume: 11B
Publisher: ASM International
Published: 15 May 2022
DOI: 10.31399/asm.hb.v11B.a0006932
EISBN: 978-1-62708-395-9
... temperature in semicrystalline polymers ( Ref 10 ). The situation is somewhat different in cross-linked or thermoset processing. In this case, solidification takes place at the cure temperature, because cross links enable the matrix to support stress ( Ref 10 ). Unsaturated polyester and epoxy resins...