Published: 01 January 2002
Fig. 6 Device used by Velez and Powell to investigate the spalling of 1060 steel. Source: Ref 5 More
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003519
EISBN: 978-1-62708-180-1
... Abstract This article reviews the most common reasons for failures and the purpose of a failure investigation. It discusses the nine steps for the organization of a good failure investigation. The three basic tools that are helpful in any failure investigation, namely, a fault tree, a failure...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.aero.c9001729
EISBN: 978-1-62708-217-4
... (Other, miscellaneous, or unspecified) failure In July 1965, a plane crashed in central British Columbia, killing 52 passengers and crew members. Since eyewitness accounts and other evidence indicated that an explosion might be responsible, Dept. of Transport investigators undertook to establish...
Image
Published: 01 January 2002
Fig. 3 General sequence of failure investigation from design point of view More
Image
Published: 01 June 2019
Fig. 1 A drawing showing a compression hip screw device of the type investigated here, used for fracture fixation in the vicinity of the femur. More
Image
Published: 01 January 2002
Fig. 19 Investigation of cracking of a box-girder web. (a) Hole resulting from removal of the core. (b) Polished-and-etched surface showing crack, slag, and lack of fusion More
Image
Published: 01 January 2002
Fig. 1 Carrying case with contents of field investigation kit (Table 1) without camera, cell phone, and laptop or hand-held computer device More
Image
Published: 01 June 2019
Fig. 1 Schematic representation of the parts investigated with fracture sites and crack propagation. Shrunk connectors 4 1 2 ″. More
Image
Published: 01 June 2019
Fig. 1 Investigation sequence. More
Image
Published: 01 June 2019
Fig. 1 Photomacrograph of the fastener combination investigated in this paper (a). During normal installation, the collar separates (b). For a number of fasteners, the pin fractured instead of the collar separating (c). More
Image
Published: 15 January 2021
Fig. 10 Application of fracture mechanics in failure investigation More
Image
Published: 15 January 2021
Fig. 27 (a) Investigation of crack length extension under a partial slip condition as a function of the tangential force amplitude. Compressive residual stresses limit the crack propagation. (b) Investigation of wear volume extension under a gross slip condition as a function of the friction More
Image
Published: 15 January 2021
Fig. 3 Hard plastic carrying case with contents of field investigation kit ( Table 1 ) More
Image
Published: 01 December 2019
Fig. 3 Specimens cut for investigation from ( a ) splint A and ( b ) splint B More
Image
Published: 01 December 2019
Fig. 1 As-received photographs of the primary hardware of interest in the investigation: ( a ) beveled gear, ( b ) sleeve, ( c ) outer race, ( d ) inner race, ( e ) rolling elements, ( f ) generic schematic of assembly More
Image
Published: 01 December 2019
Fig. 10 The zone below cracked surface: ( a ) for microstructure investigation; and ( b ) for measuring the porosity More
Image
Published: 01 December 2019
Fig. 12 Results of SEM investigations near the cracked surface More
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.matlhand.c9001209
EISBN: 978-1-62708-224-2
... Abstract Three links of a chain showing unusually strong wear were examined. Corresponding to the stress, the wear was strongest in the bends of the links, but it was especially pronounced in the bend in which the butt weld seam was located. Investigation showed the links were manufactured from...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.aero.c9001708
EISBN: 978-1-62708-217-4
... blade by approximately 40%. Casting defects Icebreakers Propeller blades Superston 70 C95700 UNS C95700 Brittle fracture Casting-related failures Introduction In the past Fleet Technology Ltd. has carried out a number of investigations on damaged propellor blades from ice breaking...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.aero.c9001587
EISBN: 978-1-62708-217-4
.... This investigation is continuing. Aircraft components Commercial planes Crashes Passenger airline materials (Other, miscellaneous, or unspecified) failure The National Transportation Safety Board simultaneously investigates major accidents in different modes of transportation at any time. The services...