1-20 of 66 Search Results for

internal combustion engines

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Series: ASM Failure Analysis Case Histories
Volume: 3
Publisher: ASM International
Published: 01 December 2019
DOI: 10.31399/asm.fach.v03.c9001761
EISBN: 978-1-62708-241-9
... of the Failure Cause Conclusion Acknowledgments References References 1. Campbell A.J. : Optical alignment of reciprocating compressors . In: 12th Annual Fall Technical Conference of the ASME Internal Combustion Engine Division , New Technology in Large Bore Engines American Society...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.design.c9001424
EISBN: 978-1-62708-233-4
... service is most undesirable. Adequate rigidity is particularly important where alignment under load must be maintained, e.g., in the case of engine crankcases, and it is significant that some manufacturers of internal combustion engines, heavy gear boxes and similar plant have reverted to the use of cast...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.aero.c9001145
EISBN: 978-1-62708-217-4
... and unzipping of the chamber dome, burn-through of the dome, and shearing of bayonet locking lugs. Factors identified as significant in the failures are the pressure developed in the chamber and internal corrosion of the chamber in an environment that can produce stress-corrosion cracking. The interior...
Series: ASM Failure Analysis Case Histories
Volume: 1
Publisher: ASM International
Published: 01 December 1992
DOI: 10.31399/asm.fach.v01.c9001031
EISBN: 978-1-62708-214-3
... resulted in a higher hot-gas wall temperature and associated degradation of mechanical properties. Combustion chambers Engine components Internal oxidation Pinholes Reentry vehicles Rocket engines Transgranular fracture NARloy-Z High-temperature corrosion and oxidation Brittle fracture...
Series: ASM Failure Analysis Case Histories
Volume: 3
Publisher: ASM International
Published: 01 December 2019
DOI: 10.31399/asm.fach.v03.c9001827
EISBN: 978-1-62708-241-9
... ( 2005 ) 10.1039/b507454a 10. Koul A.K. , Immarigeon J.P. , Dainty R.V. , Patnaik P.C. : Degradation of high performance aero-engine turbine blades . In: Swaminathan V.P. , Cheruvu N.S. (eds.) Advanced Materials and Coatings for Combustion Turbines...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.power.c0047621
EISBN: 978-1-62708-229-7
..., stiffener, and flange and more skillful welding techniques to avoid undercutting and unfused interfaces. Arc welding Combustion chamber Flanges Gas turbine engines Pipe fitting Undercuts Welding defects Inconel 718 (Nickel-base superalloy) UNS N07718 Fatigue fracture Joining-related failures...
Series: ASM Failure Analysis Case Histories
Volume: 3
Publisher: ASM International
Published: 01 December 2019
DOI: 10.31399/asm.fach.v03.c9001756
EISBN: 978-1-62708-241-9
... in engine components can also be attributed to entry of foreign objects or dislodgement of any internal objects inside the engine, defects in raw material, improper material selection, inappropriate design, incorrect processing, improper maintenance, etc. Any failure in service can sometimes be catastrophic...
Series: ASM Failure Analysis Case Histories
Volume: 3
Publisher: ASM International
Published: 01 December 2019
DOI: 10.31399/asm.fach.v03.c9001760
EISBN: 978-1-62708-241-9
... the most important components in engines which are exposed to thermo-mechanical cyclic loads from the combustion chamber (thermal stresses) and bolts (mechanical stresses). Owing to these loads, the important parameter in the design of cylinder heads is known as thermo-mechanical fatigue strength. Also...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003555
EISBN: 978-1-62708-180-1
... ( No. 4 ), 1978 , p 173 18. Lai G.Y. , Nitridation of Several Combustor Alloys in a Simulated Gas Turbine Combustion Environment , Advanced Materials and Coatings for Combustion Turbines , Swaminathan V.P. and Cheruvu N.S. , Ed., ASM International , 1994 , p 113 19...
Series: ASM Failure Analysis Case Histories
Volume: 3
Publisher: ASM International
Published: 01 December 2019
DOI: 10.31399/asm.fach.v03.c9001767
EISBN: 978-1-62708-241-9
... Selected References Selected References • Fracture of Plastics , Failure Analysis and Prevention , Vol 11 , ASM Handbook , Becker W.T. and Shipley R.J. , Ed., ASM International , 2002 , p 650 – 661 . 10.31399/asm.hb.v11.a0003541 • Engineering Thermoplastics , Engineered...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.aero.c9001560
EISBN: 978-1-62708-217-4
... both combustion products from the cartridges and corrosion products from the chamber, were analyzed using elemental analysis and x-ray diffraction techniques. Electrochemical polarization techniques were also utilized to estimate corrosion rates. Aerospace engines Aircraft components Breech...
Series: ASM Handbook
Volume: 11
Publisher: ASM International
Published: 15 January 2021
DOI: 10.31399/asm.hb.v11.a0006787
EISBN: 978-1-62708-295-2
... in a Simulated Gas Turbine Combustion Environment , Advanced Materials and Coatings for Combustion Turbines , Swaminathan V.P. and Cheruvu N.S. , Ed., ASM International , 1994 , p 113 22. Swaminathan V.P. and Lukezich S.J. , Degradation of Transition Duct Alloys in Gas...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.power.c9001609
EISBN: 978-1-62708-229-7
... International , Materials Park, OH , 1987 , pp. 355 and 1265 . 6. Espy R.H. , “ How Composition and Welding Conditions Affect Corrosion Resistance of Type 430 Stainless Steel ,” Preprint 22, National Association of Corrosion Engineers , Cleveland, OH , 1968 . 7. Anon. : ASME SA-268...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0001816
EISBN: 978-1-62708-180-1
... in steam demand, composition of fuel, amount of excess combustion air, type and amount of water-conditioning chemicals added, type and amount of contaminants in condensate and make-up feedwater, frequency and methods of cleaning fire-side and water-side surfaces of steam generators, materials specified...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003565
EISBN: 978-1-62708-180-1
... on automotive engine inlet valves and seat inserts. References References 1. Engel P.A. , Impact Wear , Friction, Lubrication and Wear Technology , Vol 18 , ASM Handbook , ASM International , 1992 , p 263 – 270 2. De Gee A.W.L. , Commissaris C.P.L. , and Zaat J.H...
Series: ASM Failure Analysis Case Histories
Volume: 2
Publisher: ASM International
Published: 01 December 1993
DOI: 10.31399/asm.fach.v02.c9001281
EISBN: 978-1-62708-215-0
... Conclusion and Recommendations Selected References Selected References • Benac D.J. and Swaminathan V.P. , Elevated-Temperature Life Assessment for Turbine Components, Piping, and Tubing , Failure Analysis and Prevention , Vol. 11 , ASM Handbook , ASM International , 2002 , p...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.usage.c9001488
EISBN: 978-1-62708-236-5
...Abstract Abstract While an attempt was being made to start the diesel engine of a dragline type excavator, a severe explosion took place, the operator unfortunately being killed. The engine was normally started by compressed air from an air bottle or receiver charged to a pressure of 350 psi...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003529
EISBN: 978-1-62708-180-1
...) produced from 5 keV electrons. The carbon peak is also higher in Fig. 4(b), suggesting a trace of carbon, probably from oil, on the surface of the part. The unlabeled peak at the far left is the internal calibration peak for the EDS unit. Fig. 5 Schematic diagram of the components of a wavelength...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.usage.c9001508
EISBN: 978-1-62708-236-5
...-P-408 gas turbine (turbojet) engines, involves the rework and/or replacement of many components including the fuel nozzle heat shields. These heat shields, which are fabricated by press forming from annealed type 321 corrosion resistant steel (CRES) sheet, are utilized to keep hot combustion gases...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.modes.c9001681
EISBN: 978-1-62708-234-1