1-20 of 334 Search Results for

institute

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.marine.c9001164
EISBN: 978-1-62708-227-3
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.petrol.c9001167
EISBN: 978-1-62708-228-0
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.petrol.c9001247
EISBN: 978-1-62708-228-0
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.auto.c9001173
EISBN: 978-1-62708-218-1
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.auto.c9001156
EISBN: 978-1-62708-218-1
Series: ASM Failure Analysis Case Histories
Volume: 1
Publisher: ASM International
Published: 01 December 1992
DOI: 10.31399/asm.fach.v01.c9001117
EISBN: 978-1-62708-214-3
... conditions. The couplings were purchased to American Petroleum Institute (API) specifications for P-110 material. Chemical analysis and mechanical testing of the failed couplings showed that they had been manufactured to the API specification for Q-125, more stringent specification than P-110, and met all...
Series: ASM Failure Analysis Case Histories
Volume: 1
Publisher: ASM International
Published: 01 December 1992
DOI: 10.31399/asm.fach.v01.c9001084
EISBN: 978-1-62708-214-3
... with casting defects increasing stress and initiating fracture. In addition, the composition and hardness of the impeller did not meet specifications. Revision of the casting process and institution of quality assurance methods were recommended. Selected References Selected References • Failures...
Series: ASM Handbook
Volume: 11A
Publisher: ASM International
Published: 30 August 2021
DOI: 10.31399/asm.hb.v11A.a0006823
EISBN: 978-1-62708-329-4
... Abstract This article illustrates the use of the American Petroleum Institute (API) 579-1/ASME FFS-1 fitness-for-service (FFS) code (2020) to assess the serviceability and remaining life of a corroded flare knockout drum from an oil refinery, two fractionator columns affected by corrosion under...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.process.c0059924
EISBN: 978-1-62708-235-8
... Abstract The large steel ring produced for a nuclear application from a billet of 8822 steel was inspected. The large billet was first forged into a doughnut preform in a large press, and then formed into the ring by ring rolling. A straight-beam ultrasonic inspection was instituted...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.process.c0046233
EISBN: 978-1-62708-235-8
... and instituting receiving inspection of the connection castings. Castings Porosity Trailers Trucks Welded defects Welded joints Welded steel Joining-related failures Casting-related failures Fatigue fracture A drawbar connecting the two tank-type trailers of a highway gasoline rig broke while...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.process.c0049796
EISBN: 978-1-62708-235-8
... headers to eliminate the chloride contamination and a vacuum drying procedure was instituted for the pyrotechnic. Actuators Chlorine Pyrotechnics Tophet C (Other, general, or unspecified) corrosion Pyrotechnically driven devices are used in a number of ordnance applications requiring rapid...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.power.c9001594
EISBN: 978-1-62708-229-7
... Electric and Southwest Research Institute are presented regarding the frequency of failures, failure locations, and the potential causes. The topics addressed include 1) metallurgical and fractographic features of fatigue cracks at the weld toe and weld root; 2) factors that are associated with fatigue...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.aero.c0089722
EISBN: 978-1-62708-217-4
... was attached to a flexible metal hose, which provided no support and offered no resistance to vibration. The components of the elbow were made of American Iron and Steel Institute (AISI) type 321 stainless steel and were joined with ER347 stainless steel filler metal by gas tungsten arc welding. The line...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.9781627081801
EISBN: 978-1-62708-180-1
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0006548
EISBN: 978-1-62708-180-1
... temperature at which austenite begins to form on heating Ac3 temperature at which transformation of ferrite to austenite is completed on heating ABS acrylonitrile-butadiene-styrene ACI Alloy Casting Institute AES Auger electron spectroscopy AGMA American Gear Manufacturers Asso- ciation AISI American Iron...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.power.c0047621
EISBN: 978-1-62708-229-7
... editions provided substantial content used in the source article. Appreciation is expressed to: Tarsem Jutla, Caterpillar Inc.; Alan G. Glover, Welding Institute of Canada; Daniel Hauser, Edison Welding Institute; Edward A. Metzbower, Naval Research Laboratory; O.W. Blodgett, Lincoln Electric; the ASM...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.conag.c0047570
EISBN: 978-1-62708-221-1
... article. Appreciation is expressed to: Tarsem Jutla, Caterpillar Inc.; Alan G. Glover, Welding Institute of Canada; Daniel Hauser, Edison Welding Institute; Edward A. Metzbower, Naval Research Laboratory; O.W. Blodgett, Lincoln Electric; the ASM Committee on Weld Discontinuities (for Welding, Brazing...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.process.c0089738
EISBN: 978-1-62708-235-8
....; Alan G. Glover, Welding Institute of Canada; Daniel Hauser, Edison Welding Institute; Edward A. Metzbower, Naval Research Laboratory; O.W. Blodgett, Lincoln Electric; the ASM Committee on Weld Discontinuities (for Welding, Brazing, and Soldering , Volume 6 of Metals Handbook (9th ed.), 1983...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.process.c9001190
EISBN: 978-1-62708-235-8
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.process.c0089774
EISBN: 978-1-62708-235-8
... application. Acknowledgments The following authors and contributors of previous editions provided substantial content used in the source article. Appreciation is expressed to: Tarsem Jutla, Caterpillar Inc.; Alan G. Glover, Welding Institute of Canada; Daniel Hauser, Edison Welding Institute; Edward...