1-10 of 10 Search Results for

induction heater

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.power.c9001143
EISBN: 978-1-62708-229-7
... cause liquid droplet erosion in the HP or IP turbines is the failure of the water level control mechanism on one of these heaters. This will allow water to drain back into the turbine. Liquid droplet erosion pits on the HP or IP turbine blades are evidence of water induction since condensation does...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003503
EISBN: 978-1-62708-180-1
... Hot Water Heater Role of FMEA in the Design Process System Design Reliability System Safety Maintainability Logistics Support Manufacturing Systems Testability and Quality Assurance Project Management The FMEA methodology is based on a hierarchical, inductive...
Series: ASM Failure Analysis Case Histories
Volume: 3
Publisher: ASM International
Published: 01 December 2019
DOI: 10.31399/asm.fach.v03.c9001826
EISBN: 978-1-62708-241-9
..., nondestructive testing, energy dispersive x-ray analysis, and inductively coupled plasma mass spectrometry. The tube was made from SA 210A1 carbon steel that had been compromised by wall thinning and the accumulation of fire and water-side scale deposits. Investigators determined that the tube failed due...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0001818
EISBN: 978-1-62708-180-1
.... Example 2: Rupture of a Ferritic Steel Return Bend Because of Inclusions After 2 years of service, a return bend from a triolefin-unit heater ruptured ( Fig. 3a ). The bend was made from 115-mm (4 1 2 -in.) schedule 40 (6.0 mm, or 0.237-in., wall thickness) pipe of ASTM A213, grade T11...
Series: ASM Handbook
Volume: 11A
Publisher: ASM International
Published: 30 August 2021
DOI: 10.31399/asm.hb.v11A.a0006834
EISBN: 978-1-62708-329-4
...–0.25 3.25–3.75 Rolling-element bearing material families, group III or induction-hardening group Table 4 Rolling-element bearing material families, group III or induction-hardening group Steel name WN material number Composition, wt% C Si Mn P S Cr Mo...
Series: ASM Handbook
Volume: 11A
Publisher: ASM International
Published: 30 August 2021
DOI: 10.31399/asm.hb.v11A.a0006812
EISBN: 978-1-62708-329-4
...—Nondestructive Examination ASME B31.3—Process Piping ASME B31.1—Power Piping API 650—Welded Steel Tanks for Oil Storage API 620—Design and Construction of Large, Welded, Low-Pressure Storage Tanks API 530—Calculation of Heater Tube Thickness in Petroleum Refineries Inspection codes: API...
Series: ASM Handbook
Volume: 11
Publisher: ASM International
Published: 15 January 2021
DOI: 10.31399/asm.hb.v11.a0006782
EISBN: 978-1-62708-295-2
... to identify the material and to compare it with the specification requirements on the drawing. Otherwise, the alloy is identified using available standards. For metallic components, destructive analysis is performed using inductively coupled plasma/atomic or optical emission spectroscopy, an analytical...
Book Chapter

Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003548
EISBN: 978-1-62708-180-1
... in galvanic attack of less noble metals. In the example shown at left, copper ions from the copper heater coil could deposit on the aluminum stirrer. A nonmetallic stirrer would be better. At right, the distance from a metal container to a heater coil should be increased to minimize ion transfer. (f) Wood...
Series: ASM Handbook
Volume: 11
Publisher: ASM International
Published: 15 January 2021
DOI: 10.31399/asm.hb.v11.a0006783
EISBN: 978-1-62708-295-2
... metals. In the example shown at left, copper ions from the copper heater coil could deposit on the aluminum stirrer. A nonmetallic stirrer would be better. At right, the distance from a metal container to a heater coil should be increased to minimize ion transfer. (f) Wood treated with copper...
Series: ASM Handbook
Volume: 11A
Publisher: ASM International
Published: 30 August 2021
DOI: 10.31399/asm.hb.v11A.a0006808
EISBN: 978-1-62708-329-4
... Recommendations Creep Example 13: Creep Damage of a Weld Reformer Tube <xref rid="a0006808-ref54" ref-type="bibr">(Ref 54)</xref> A reformer heater in a section of an ammonia-urea fertilizer complex having a capacity to produce 1100 metric tons of ammonia and 1650 metric tons of urea per day...