Series: ASM Failure Analysis Case Histories
Volume: 1
Publisher: ASM International
Published: 01 December 1992
DOI: 10.31399/asm.fach.v01.c9001036
EISBN: 978-1-62708-214-3
... ) was distended in a horizontal plane, indicating that it was incandescent at the time of the collision. The high-beam filament (lower coil in Fig. 2 ) exhibited some sag in a vertical plane. This filament was not incandescent when the collision occurred. Neither filament exhibited marked oxidation, suggesting...