Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.modes.c0048498
EISBN: 978-1-62708-234-1
... Abstract A graphite-epoxy tapered-box structure, which consisted of two honeycomb skin panels fastened to a spanwise spar with intermediate chordwise ribs, fractured during testing. Hinge-line deflection of the front spar was revealed. Through-thickness cracks in the forward and trailing edges...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.modes.c9001486
EISBN: 978-1-62708-234-1
... to this cause takes the form of deep pitting of a honeycomb nature. It is restricted to certain specific locations on the waterside surface and is found principally on the thrust side of the cylinder liner, i.e., that subjected to the thrust from the piston on the firing stroke, and occasionally...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.chem.c9001687
EISBN: 978-1-62708-220-4
.... To counteract the increase in local deformation at the inner section, higher stresses are induced in the outer regions, accelerating the formation and coalescence of microcracks; leading to the premature failure of the tube. References References 1. Wen-Tai Hou and Honeycombe R.W.K...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.bldgs.c9001171
EISBN: 978-1-62708-219-8
... ( 1966 ) 418 . 14. Doshi C. P. , Austin W. W. , Corrosion 21 ( 1965 ) 332 . 10.5006/0010-9312-21.10.332 15. Gooch T. G. , Honeycombe J. , Walker P. , Br. Corros. J. 6 ( 1971 ) 148 . 10.1179/000705971798323838 16. Goncharevsky M. S. , Schesno L...
Series: ASM Failure Analysis Case Histories
Volume: 3
Publisher: ASM International
Published: 01 December 2019
DOI: 10.31399/asm.fach.v03.c9001837
EISBN: 978-1-62708-241-9
.... Bhadeshia H.K.D.H. , Honeycomb R. : Steels: Microstructure and Properties , 3rd edn. , pp. 296 – 297 . Elsevier ( 2006 ) 9. Andrews K.W. : Empirical formulae for the calculation of some transformation temperatures . J. Iron Steel Inst . 203 , 721 – 727 ( 1965 ) 10...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0001812
EISBN: 978-1-62708-180-1
... Honeycomb Blind rivets (a) 5056 aluminum None Not recommended (h) Excellent (h) Excellent (h) (e) Monel None Good (h) Excellent (h) Excellent (h) (e) A-286 Passivated Good (h) Excellent (h) Excellent (h) (e) Blind bolts (b) A-286 Passivated Excellent (h...
Series: ASM Handbook
Volume: 11B
Publisher: ASM International
Published: 15 May 2022
DOI: 10.31399/asm.hb.v11B.a0006931
EISBN: 978-1-62708-395-9
... >465 273 525 690 1275 … … 29.5 PVC <80 <175 >180 >355 >180 >355 450 840 21 9.0 38 Polyvinylidene chloride –17 1 195 385 >220 >430 535 995 11 4.7 60 PTFE 126 260 >327 >620 400 750 560 1040 4 1.7 95 Aramid honeycomb core...
Series: ASM Handbook
Volume: 11B
Publisher: ASM International
Published: 15 May 2022
DOI: 10.31399/asm.hb.v11B.a0006936
EISBN: 978-1-62708-395-9
..., and complex robotics may be required when this method is used on larger parts. The through-transmission technique is also extremely useful for detecting disbonds, core damage, and moisture intrusion in sandwich structures (parts with a honeycomb or foam core surrounded by laminate face sheets). Pulse-echo...
Series: ASM Handbook
Volume: 11A
Publisher: ASM International
Published: 30 August 2021
DOI: 10.31399/asm.hb.v11A.a0006805
EISBN: 978-1-62708-329-4
... composites Fastener type Fastener material Surface coating Suggested application Epoxy/graphite composite Kevlar (DuPont) Fiberglass Honeycomb Blind rivets (a) 5056 aluminum None Not recommended (b) Excellent (b) Excellent (b) (c) Monel None Good (b...
Series: ASM Handbook
Volume: 11
Publisher: ASM International
Published: 15 January 2021
DOI: 10.31399/asm.hb.v11.a0006775
EISBN: 978-1-62708-295-2
.... Important work from the period of the 1950s and 1960s can be found in the literature ( Ref 10 – 13 ). A discussion of identifying what is meant by cleavage in metallic materials can be found in Ref 14 . Honeycombe ( Ref 4 ) summarized models and experimental evidence for brittle fracture together...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003537
EISBN: 978-1-62708-180-1
.... It was then realized that cleavage fracture in crystalline materials could not be based simply on a normal stress criterion (e.g., see Honeycombe ( Ref 2 ). Many new tools and techniques for studying fracture surfaces have become available and made possible a more complete understanding of fracture processes...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003538
EISBN: 978-1-62708-180-1
Series: ASM Handbook
Volume: 11B
Publisher: ASM International
Published: 15 May 2022
DOI: 10.31399/asm.hb.v11B.a0006923
EISBN: 978-1-62708-395-9
... Polyvinyl chloride <80 <175 >180 >355 >180 >355 450 840 21 9.0 38 Polyvinylidene chloride −17 1 195 385 >220 >430 532 995 11 4.7 60 Polytetrafluoroethylene 126 260 >327 >620 400 750 560 1040 4 1.7 95 Aramid honeycomb core 275 525 375...