Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.power.c9001473
EISBN: 978-1-62708-229-7
... years. The gearbox casing was a grey iron casting and the main gear wheel, the remains of which can be seen in Figure 1 , consisted of a cast iron, double-spoked wheel, on to the periphery of which was shrunk two steel rims in which the teeth were hobbed. The pinion was machined from the solid and its...
Series: ASM Failure Analysis Case Histories
Volume: 2
Publisher: ASM International
Published: 01 December 1993
DOI: 10.31399/asm.fach.v02.c9001269
EISBN: 978-1-62708-215-0
... 0.254 0.010 863 66 0.254 0.010 842 65 Carbide-deficient region 766 62 749 61 755 61 759 61 Carbide-rich region 795 63 842 65 885 67 945 69 Chemical analysis of high speed steel hob<xref rid="c9001269-tn1" ref-type="table-fn">(a)</xref> Table 2...