Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.bldgs.c9001697
EISBN: 978-1-62708-219-8
... waters is regulated by the Occupational Safety and Health Administration, the U.S. Environmental Protection Agency, the U.S. Public Health Service and other related federal and state agencies. The sole purpose of these regulations is to safeguard the health and safety of the general population. Some...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.conag.c9001680
EISBN: 978-1-62708-221-1
... (Other, miscellaneous, or unspecified) wear Fatigue fracture Introduction Experimental Procedure Results Discussion Conclusions References References 1. Code of U.S. Federal Regulations . Title 30—Mineral Resources; Chapter 1—Mine Safety and Health Administration, Department...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.bldgs.c0091378
EISBN: 978-1-62708-219-8
... brass (UNS C68700) are less susceptible to corrosion. Suitability for use in potable water systems is the prime consideration in this case, however. This points out that not only are the degrading effects of selective leaching on the function of the component important, but also the effects...
Series: ASM Handbook
Volume: 11A
Publisher: ASM International
Published: 30 August 2021
DOI: 10.31399/asm.hb.v11A.a0006800
EISBN: 978-1-62708-329-4
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003501
EISBN: 978-1-62708-180-1
... reasons, the process of conceptual design may also address the possibility of eliminating a part or combining functions, because one complex part may be less expensive overall than two or more simpler parts. This step may involve consideration of materials and manufacturing costs and economics...
Series: ASM Handbook
Volume: 11A
Publisher: ASM International
Published: 30 August 2021
DOI: 10.31399/asm.hb.v11A.a0006832
EISBN: 978-1-62708-329-4
..., and deposition and trial testimonies. engineering design product liability product litigation Product Liability Litigation and the Expert Witness Admissibility of Expert Opinions Considerations of How to Evaluate Data Factual Evidence—Testimony, Witness Statements, and Accident Reports...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.chem.c9001458
EISBN: 978-1-62708-220-4
.... These aspects are dealt with by the “Brussels Treaty Organisation—Industrial, Safety and Health Committee” in their “Recommendations on the Construction and Use of Centrifuges” which are contained in Form 719 issued by the Ministry of Labour, H.M. Factory Inspectorate. This publication is similar to B.S. 767...
Series: ASM Handbook
Volume: 11A
Publisher: ASM International
Published: 30 August 2021
DOI: 10.31399/asm.hb.v11A.a0006811
EISBN: 978-1-62708-329-4
... of the Economic Downturn on Total Joint Replacement Demand in the United States: Updated Projections to 2021 , J. Bone Joint Surg. Am. , Vol 96 , 2014 , p 624 – 630 8. Cheng M. , Medical Device Regulations: Global Overview and Guiding Principles , World Health Organization , 2003 , p 3 9...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003500
EISBN: 978-1-62708-180-1
... the preliminary stages of an investigation should be factual rather than judgmental. It is important to recognize that some of the terminology used in a failure analysis can be judgmental, and consideration must be given to the implications associated with the use of such terminology. For example, when examining...
Series: ASM Handbook
Volume: 11
Publisher: ASM International
Published: 15 January 2021
DOI: 10.31399/asm.hb.v11.a0006753
EISBN: 978-1-62708-295-2
... analysis can be judgmental, and consideration must be given to the implications associated with the use of such terminology. For example, when examining both a failed and an unfailed component returned from service, references to the unfailed sample as “good” and the failed sample as “bad” should...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.power.c9001536
EISBN: 978-1-62708-229-7
...Abstract Abstract Argonne National Laboratory has conducted analyses of failed components from nuclear power-generating stations since 1974. The considerations involved in working with and analyzing radioactive components are reviewed here, and the decontamination of these components...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003515
EISBN: 978-1-62708-180-1
... part. Requires properly trained personnel with considerable application experience Magnetic particle A magnet or electrical current creates magnetic fields in a specimen. Magnetic particles applied to the surface indicate the location of a field leakage, signaling a discontinuity. Used on metal...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003526
EISBN: 978-1-62708-180-1
... to produce a certain amount of power; an off-road vehicle needs to carry 20% more cargo; a railroad bridge must span a river; a replacement knee joint or a handheld computer are needed. Inherent in any design are other limitations and considerations such as cost, ease of fabrication, weight, size, safety...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.marine.c9001720
EISBN: 978-1-62708-227-3
... anaerobic conditions that occur under accumulated biofoul layers. Specific concerns regarding extended deterioration of the submerged hull include 1) the U.S.S. Arizona is a war memorial in which over 900 men are entombed 2) fuel oil is still trapped at depth and is an environmental concern 3) health...
Series: ASM Handbook
Volume: 11
Publisher: ASM International
Published: 15 January 2021
DOI: 10.31399/asm.hb.v11.a0006773
EISBN: 978-1-62708-295-2
...Abstract Abstract When complex designs, transient loadings, and nonlinear material behavior must be evaluated, computer-based techniques are used. This is where the finite-element analysis (FEA) is most applicable and provides considerable assistance in design analysis as well as failure...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003532
EISBN: 978-1-62708-180-1
... of a roll made from AISI O1 tool steel that cracked during quenching. The quench cracks were located adjacent to deep stamp marks, and the microstructure contained considerable retained austenite. No residual carbide, normally present in this grade when properly heat treated, was present. Consequently...
Series: ASM Handbook
Volume: 11
Publisher: ASM International
Published: 15 January 2021
DOI: 10.31399/asm.hb.v11.a0006772
EISBN: 978-1-62708-295-2
..., codes, and standards. The knowledge of codes and standards is necessary to all types of reconstruction. Examples of codes and standards commonly referenced by personnel involved with reconstruction are: Occupational Safety and Health Administration (OSHA) standards for construction and industrial...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003523
EISBN: 978-1-62708-180-1
... of reconstruction. The following are examples of codes and standards commonly referenced by personnel involved with reconstruction: Occupational Safety and Health Administration (OSHA) standards for construction and industrial accidents American National Standards Institute (ANSI) standards for products...
Series: ASM Handbook
Volume: 11
Publisher: ASM International
Published: 15 January 2021
DOI: 10.31399/asm.hb.v11.9781627082952
EISBN: 978-1-62708-295-2
Series: ASM Handbook
Volume: 11
Publisher: ASM International
Published: 15 January 2021
DOI: 10.31399/asm.hb.v11.a0006793
EISBN: 978-1-62708-295-2
... concern. Potential impact wear problems are also found in dental implants and heart valves, where health and well-being are at stake. In this article, some generic features of impact wear are described and two particular examples are examined in detail. Impact Wear Modes Impact Wear of Metals...