Series: ASM Failure Analysis Case Histories
Volume: 3
Publisher: ASM International
Published: 01 December 2019
DOI: 10.31399/asm.fach.v03.c9001783
EISBN: 978-1-62708-241-9
... Abstract An aluminum bronze bushing that serves as a guide in a crimping machine began to fail after 50,000 cycles or approximately two weeks of operation. Until then, typical run times had been on the order of months. Although the bushings are replaceable and relatively inexpensive, the cost...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0001808
EISBN: 978-1-62708-180-1
... Abstract This article discusses failures in shafts such as connecting rods, which translate rotary motion to linear motion, and in piston rods, which translate the action of fluid power to linear motion. It describes the process of examining a failed shaft to guide the direction of failure...
Series: ASM Handbook
Volume: 11A
Publisher: ASM International
Published: 30 August 2021
DOI: 10.31399/asm.hb.v11A.a0006810
EISBN: 978-1-62708-329-4
..., manufacturing procedures, and service history. Detailed knowledge of these factors can often be helpful in guiding the direction of failure investigation and corrective action. Design Parameters The failure analyst should have copies of the detail and assembly drawings as well as the material and testing...
Series: ASM Handbook
Volume: 11B
Publisher: ASM International
Published: 15 May 2022
DOI: 10.31399/asm.hb.v11B.a0006922
EISBN: 978-1-62708-395-9
... Study: Plastic Bushing General use: The part is a plastic bushing used between a metal rod and a roller ( Fig. 5 ). Fig. 5 Plastic bushing General dimensions: 30 mm long, 35 mm in diameter, 2.5 mm nominal thickness. Requirements : 15 MPa (2175.57 psi) tensile/compressive...
Series: ASM Handbook
Volume: 11B
Publisher: ASM International
Published: 15 May 2022
DOI: 10.31399/asm.hb.v11B.a0006864
EISBN: 978-1-62708-395-9
... are extruded above their melting temperature ( T m ); amorphous thermoplastics are extruded above their glass transition temperature ( T g ). The selection of processing temperature can be guided by material data sheets. If a material data sheet is not available, the selection of processing temperature...
Series: ASM Handbook
Volume: 11
Publisher: ASM International
Published: 15 January 2021
DOI: 10.31399/asm.hb.v11.a0006789
EISBN: 978-1-62708-295-2
... and relevant tribosystems Table 1 Wear processes and relevant tribosystems Wear process Examples of relevant tribosystems Sliding wear Sliding bearings; cam and tappets; guides; seals; piston rings; disc-pad braking system; forming dies; cutting tools Fretting wear Riveted joints...
Series: ASM Handbook
Volume: 11A
Publisher: ASM International
Published: 30 August 2021
DOI: 10.31399/asm.hb.v11A.a0006834
EISBN: 978-1-62708-329-4
... subcomponents of a rolling-element bearing. Source: Ref 1 , 2 To separate and guide the rolling elements but also to reduce the overall useless frictional losses (and especially the friction between the rolling elements themselves due to the detrimental effect of opposite contacting sliding speed...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003553
EISBN: 978-1-62708-180-1
Series: ASM Handbook
Volume: 11B
Publisher: ASM International
Published: 15 May 2022
DOI: 10.31399/asm.hb.v11B.9781627083959
EISBN: 978-1-62708-395-9
Series: ASM Handbook
Volume: 11B
Publisher: ASM International
Published: 15 May 2022
DOI: 10.31399/asm.hb.v11B.a0006925
EISBN: 978-1-62708-395-9
.... Chief among the factors to consider are production volume and information about the size, shape, and complexity of the part. With the process-first approach, the designer begins by selecting the manufacturing process, guided by the same factors. Then, materials consistent with the selected process...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003524
EISBN: 978-1-62708-180-1
... accurate color rendition is required, the subject should be photographed with a color chart, which should be sent to the photographic studio for use as a guide in developing and printing. Some indication of size, such as a scale, coin, hand, and so forth, should be included in the photograph. Samples...
Series: ASM Handbook
Volume: 11B
Publisher: ASM International
Published: 15 May 2022
DOI: 10.31399/asm.hb.v11B.a0006923
EISBN: 978-1-62708-395-9
Series: ASM Handbook
Volume: 11A
Publisher: ASM International
Published: 30 August 2021
DOI: 10.31399/asm.hb.v11A.9781627083294
EISBN: 978-1-62708-329-4
Series: ASM Handbook
Volume: 11A
Publisher: ASM International
Published: 30 August 2021
DOI: 10.31399/asm.hb.v11A.a0006831
EISBN: 978-1-62708-329-4