1-9 of 9 Search Results for

galvanizing post treatment

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Series: ASM Failure Analysis Case Histories
Volume: 3
Publisher: ASM International
Published: 01 December 2019
DOI: 10.31399/asm.fach.v03.c9001812
EISBN: 978-1-62708-241-9
... metal environments in industry Coatings, e.g., Cd, Zn on steels, inadvertently exposed to high temperatures Solders, Brazes, and Galvanizing baths (if applied/residual stresses are high) Liquid–metal coolants for nuclear reactors, nuclear fission products, and neutron spallation targets...
Series: ASM Failure Analysis Case Histories
Volume: 3
Publisher: ASM International
Published: 01 December 2019
DOI: 10.31399/asm.fach.v03.c9001768
EISBN: 978-1-62708-241-9
... the hot-rolling. The plate angles were directly hot-rolled with special rolls and roll gap adjustments were done with suitable roll pass design to give the shape of an angle. No post-working heat treatment was applied. Therefore, higher hardness near the edge was not due to this work hardening effect...
Series: ASM Failure Analysis Case Histories
Volume: 3
Publisher: ASM International
Published: 01 December 2019
DOI: 10.31399/asm.fach.v03.c9001817
EISBN: 978-1-62708-241-9
...). The desired microstructure and mechanical properties are controlled and adjusted by carbon content of the steel and subsequent heat treatment. The heat treatment that produces the starting microstructure for wire production is termed patenting. It consists of heating to austenite region and isothermal holding...
Series: ASM Handbook
Volume: 11
Publisher: ASM International
Published: 15 January 2021
DOI: 10.31399/asm.hb.v11.a0006783
EISBN: 978-1-62708-295-2
... in ASTM G 82 ( Ref 3 ). To prepare a valid galvanic series for a given set of materials and environment of interest, all the factors affecting the potential must be addressed. This includes material composition, heat treatment, surface preparation (mill scale, coatings, surface finish, etc...
Book Chapter

Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003548
EISBN: 978-1-62708-180-1
... Abstract This article addresses the forms of corrosion that contribute directly to the failure of metal parts or that render them susceptible to failure by some other mechanism. It describes the mechanisms of corrosive attack for specific forms of corrosion such as galvanic corrosion, uniform...
Series: ASM Handbook
Volume: 11
Publisher: ASM International
Published: 15 January 2021
DOI: 10.31399/asm.hb.v11.a0006782
EISBN: 978-1-62708-295-2
... evaluation. Care must be taken when evaluating laboratory data to be certain that conclusions drawn result in an accurate assessment of the operating environment. ASTM International G 16 ( Ref 9 ) provides a guide for handling data. It refers to ASTM International E 178 ( Ref 10 ) for the treatment...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003556
EISBN: 978-1-62708-180-1
... effects are of significant concern in failure analysis and prevention. Microbially induced corrosion problems afflict water-handling operations and manufacturing processes in oil and gas production, pipelining, refining, petrochemical synthesis, power production, fermentation, waste water treatment...
Series: ASM Handbook
Volume: 11
Publisher: ASM International
Published: 15 January 2021
DOI: 10.31399/asm.hb.v11.a0006788
EISBN: 978-1-62708-295-2
... corrosion by: Direct involvement in the electrochemical corrosion cell Generation of corrosive metabolites Alteration of chemical conditions at the metal surface Disruption of passivating layers Degradation of coatings, cathodic protection, and treatment chemicals Microorganisms can...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003500
EISBN: 978-1-62708-180-1
... hardening method Design for installation Unsatisfactory piping support Improper piping flexibility Undersized piping Inadequate foundation Unsatisfactory soil data Liquid ingestion Inadequate liquid drain Design error Material of construction Flaw or defect Improper material Improper treatment Design...