1-20 of 131 Search Results for

galvanized steel

Sort by
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.design.c0046079
EISBN: 978-1-62708-233-4
... Abstract After only a short time in service, oil-fired orchard heaters made of galvanized low-carbon steel pipe, 0.5 mm (0.020 in.) in thickness, became sensitive to impact, particularly during handling and storage. Most failures occurred in an area of the heater shell that normally reached...
Series: ASM Failure Analysis Case Histories
Volume: 1
Publisher: ASM International
Published: 01 December 1992
DOI: 10.31399/asm.fach.v01.c9001100
EISBN: 978-1-62708-214-3
... Abstract Galvanized A36 steel unsleeved shear-type anchor bolts failed during installation. The galvanized steel bolts were approximately 18 mm (0.7 in.) in diameter with a 90 deg bend between the long and short legs. As-fractured, sawcut, and unfractured specimens were examined. Failure...
Image
Published: 01 June 2019
Fig. 1 Orchard heater of galvanized low-carbon steel that broke in a brittle manner because of an iron-zinc intermetallic compound along the grain boundaries. Dimensions given in inches. View A-A: micrograph of an etched section that shows the microstructure of the steel sheet. 400x More
Image
Published: 01 December 2019
Fig. 25 Macroscopic views of the galvanized carbon-steel stiffeners showing ( a , b ) cracks at the outside of the bend, and ( c ) fracture surface partially covered by a film of zinc More
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.mech.c0006900
EISBN: 978-1-62708-225-9
... Abstract Several type 301 half-hard stainless steel clamps used to hold cylindrical galvanized steel covers to galvanized cast iron bases failed in flooded manholes after one to six months of service. Before service, they were treated with antiseize compound containing MoS2. Based...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.process.c9001215
EISBN: 978-1-62708-235-8
... Abstract The surface of a hook did not possess the smooth and shiny zinc bloom surface normally observed on hot galvanized steel parts but was matte and rough. Large cracks were observed in the zinc layer. The hook was made of silicon-killed alloy steel 41Cr4. A silicon content of 0.27...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.marine.c0046911
EISBN: 978-1-62708-227-3
... Abstract A steel galvanizing vat measuring 3 x 1.2 x 1.2 m (10 x 4 x 4 ft) and made of 19 mm thick carbon steel plate (ASTM A285, grade B)) at a shipbuilding and ship-repair facility failed after only three months of service. To verify suspected failure cause, two T joints were made in 12.5 mm...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.power.c0046874
EISBN: 978-1-62708-229-7
... atmosphere. Recommendations included replacing all safety valves in the system with new open-top valves that had shot-peened and galvanized steel springs. Alternatively, the valve springs could be made from a corrosion-resistant metal-for example, a 300 series austenitic stainless steel or a nickel-base...
Series: ASM Failure Analysis Case Histories
Volume: 3
Publisher: ASM International
Published: 01 December 2019
DOI: 10.31399/asm.fach.v03.c9001832
EISBN: 978-1-62708-241-9
... with a purge ventilation system designed to continuously remove hydrogen gas and vapors without letting radionuclides escape. Several intergranular cracks were discovered in the vent pipe of one such system. The pipe, made of galvanized steel sheet, connects to an exhaust fan downstream of high-efficiency...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.homegoods.c0006897
EISBN: 978-1-62708-222-8
... Abstract The small cable (drop wire) providing service for individual subscribers from the aerial plant is held in place by a clamp made of a tin-coated brass body (attached to the cable) and a copper tail wire loop (attached to a galvanized steel hook or to a porcelain insulator). The tail...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.bldgs.c9001219
EISBN: 978-1-62708-219-8
... Galvanized steels Suspension bridges Wire products Galvanized steel Surface treatment related failures Hydrogen damage and embrittlement During construction of a river bridge with 80 twisted cables, one or more fractures were found in each of 21 wires of 18 cables before assembly, All were located...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.process.c9001178
EISBN: 978-1-62708-235-8
... Abstract Eight cylinderhead screws cracked after a short running time in motors. They were made of Fe-0.45C-1Cr steel, had rolled threads, were heat treated to 110 kg/sq mm tensile strength, and were electrolytically galvanized. All fractured at the root of the thread. The surfaces of fracture...
Series: ASM Failure Analysis Case Histories
Volume: 1
Publisher: ASM International
Published: 01 December 1992
DOI: 10.31399/asm.fach.v01.c9001125
EISBN: 978-1-62708-214-3
... Abstract An 1100 aluminum alloy connector of a high-tension aluminum conductor steel-reinforced (ACSR) transmission cable failed after more than 20 years in service, in a region of consider able industrial pollution. The steel core was spliced with a galvanized 1020 carbon steel sheath. Visual...
Series: ASM Failure Analysis Case Histories
Volume: 2
Publisher: ASM International
Published: 01 December 1993
DOI: 10.31399/asm.fach.v02.c9001336
EISBN: 978-1-62708-215-0
... assemblies to eliminate the forming operation, and removal of the source of chlorine were recommended. Food processing Pitting (corrosion) 304L UNS S30403 Galvanic corrosion Pitting corrosion Background Catastrophic pitting corrosion occurred in type 304L stainless steel pipe flange...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.modes.c0046535
EISBN: 978-1-62708-234-1
... Abstract One of five underground drain lines intended to carry a highly acidic effluent from a chemical-processing plant to distant holding tanks failed in just a few months. Each line was made of 304L stainless steel pipe 73 mm (2 in.) in diam with a 5 mm (0.203 in.) wall thickness. Lengths...
Image
Published: 01 January 2002
Fig. 2 Breaks in mill scale (Fe 3 O 4 ) leading to galvanic corrosion of steel More
Image
Published: 15 January 2021
Fig. 2 Breaks in mill scale (Fe 3 O 4 ) leading to galvanic corrosion of steel More
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.auto.c9001678
EISBN: 978-1-62708-218-1
... Abstract Six galvanized high-tensile steel bolts were used to hold the wheels of a four-wheel drive vehicle. The right hand rear wheel of this vehicle detached causing the vehicle to roll and resulting in considerable damage to the body. The wheel was detached by shearing of four of the bolts...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.matlhand.c9001246
EISBN: 978-1-62708-224-2
... be concluded from the investigation that the temperature did not exceed the Ac3 point of the wire material, which should be about 750 deg C, and that the heating lasted a fairly long time. Cables Cracking (fracturing) Galvanized steels Overheating Wire Cold-drawn steel (Other, general...
Book Chapter

Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003548
EISBN: 978-1-62708-180-1
... through a conducting medium or electrolyte to the other more cathodic metal (liberating hydrogen and/or causing a “reduction” of oxides). This action is seen in Fig. 2 where a couple is made up of steel and mill scale. Fig. 2 Breaks in mill scale (Fe 3 O 4 ) leading to galvanic corrosion of steel...